Ti-6Al-4V (Ti64) coating with a thickness of about 9 mm was deposited on commercial Ti64 substrate via a high-pressure cold spray process. The microstructure, hardness, and wear and corrosion resistance of the Ti64 coating were systematically investigated. The hardness of the Ti64 coating was higher than that of the Ti64 substrate due to the cold-worked microstructure of the coating. The tribological results showed that there was no significant difference in the surface wear rates of the Ti64 coating measured on its different layers while the surface wear resistance of the Ti64 coating was lower than its cross-sectional wear resistance. The corrosion results showed that the Ti64 coating did not effectively prevent its underlying Ti64 substrate from corrosion due to the occurrence of pores in the coating microstructure. It could be concluded that the hardness and wear resistance of the Ti64 coating were comparable to those of the commercial Ti64 substrate.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metal Alloys Wear and Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. C. Leyens and M. Peters, Titanium and titanium alloys: fundamentals and applications, Wiley, Weinheim, 2006
2. R. Boyer, E.W. Collings, and G. Welsch, Materials properties: titanium alloys, ASM International, Russell Township, 1994
3. F.M. Kustas and M.S. Misra, Friction and Wear of Titanium Alloys, in Lubrication, and wear technology, ASM Handbook, vol 18, P.J. Blau, Ed., ASM International, 1992, p. 778-784
4. R.W. Schutz, Corrosion of Titanium and Titanium Alloys, in Corrosion: Materials, ASM Handbook, vol 13B, S.D. Cramer and B.S. Covino, Jr., Ed., ASM International, 2005, p. 252-29910.31399/asm.hb.v13b.a0003822 ↗
5. R. Walker and B. Barnes, High-Velocity Oxygen Fuel Spray Coatings for Reclamation, Mater. Des., 1994, 15(6), p 323-32910.1016/0261-3069(94)90026-4 ↗
6. M. Froning, P. Ruggiero, J. Tsiao, J. Marnix, C. Alford, and G. Shubert, Transition of a World Class HVOF Thermal Spray Capability into a US Engine Overhaul Facility, in Thermal spray solutions, Advances in Technology and Application: Proceedings of the International Thermal Spray Conference 2004 (Osaka, JP), DVS, Düsseldorf, Germany10.31399/asm.cp.itsc2004p0011 ↗
7. A. Kumar, J. Boy, R. Zatorski, and L.D. Stephenson, Thermal Spray and Weld Repair Alloys for the Repair of Cavitation Damage in Turbines and Pumps: A Technical Note, J. Therm. Spray Technol., 2005, 14(2), p 177-18210.1361/10599630523737 ↗
8. J.C. Tan, L. Looney, and M.S.J. Hashmi, Component Repair Using HVOF Thermal Spraying, J. Mater. Process. Technol., 1999, 92–93, p 203-20810.1016/S0924-0136(99)00113-2 ↗
9. N. Bala, H. Singh, J. Karthikeyan, and S. Prakash, Cold Spray Coating Process for Corrosion Protection: A Review, Surf. Eng., 2014, 30(6), p 414-42110.1179/1743294413Y.0000000148 ↗
10. H. Singh, T.S. Sidhu, and S.B.S. Kalsi, Cold Spray Technology: Future of Coating Deposition Processes, Frattura ed Integrita Strutturale, 2012, 22, p 69-8410.3221/IGF-ESIS.22.08 ↗
11. H. Assadi, T. Schmidt, H. Richter, J.O. Kliemann, K. Binder, F. Gartner, T. Klassen, and H. Kreye, On Parameter Selection in Cold Spraying, J. Therm. Spray Technol., 2011, 20(6), p 1161-117610.1007/s11666-011-9662-9 ↗
12. N.W. Khun, A.W.Y. Tan, and E. Liu, Mechanical and Tribological Properties of Cold Sprayed Ti Coatings on Ti-6Al-4V Substrates, J. Therm. Spray Technol., 2016, 25(4), p 715-72410.1007/s11666-016-0396-6 ↗
13. N.W. Khun, A.W.Y. Tan, and E. Liu, Effect of Working Pressure on Wear and Corrosion Resistance of Cold Sprayed Ti-6Al-4V Coatings, Surf. Coat. Technol., 2016, 302, p 1-1210.1016/j.surfcoat.2016.05.052 ↗
14. N.W. Khun, A.W.Y. Tan, W. Sun, and E. Liu, Effect of Heat Treatment Temperature on Microstructure, and Mechanical and Tribological Properties of Cold Sprayed Ti-6Al-4V Coatings, Tribol. Trans., 2016, doi: 10.1080/10402004.2016.1244584)10.1080/10402004.2016.1244584) ↗
15. S.V. Klinkov, V.F. Kosarev, and M. Rein, Cold Spray Deposition: Significance of Particle Impact Phenomena, Aerosp. Sci. Technol., 2005, 9, p 582-59110.1016/j.ast.2005.03.005 ↗
16. K.G. Budinski, Tribological Properties of Titanium Alloys, Wear, 1991, 151(2), p 203-21710.1016/0043-1648(91)90249-T ↗
17. Q. Niu, X. Zheng, M. Chen, and W. Ming, Study on the Tribological Properties of Titanium Alloys Sliding Against WC-CO During the Dry Friction, Ind. Lubr. Tribol., 2014, 66(2), p 202-20810.1108/ILT-11-2011-0099 ↗
18. S.B. Pitchuka, B. Boesl, C. Zhang, D. Lahiri, A. Nieto, G. Sundararajan, and A. Agarwal, Dry Sliding Wear Behavior of Cold Sprayed Aluminum Amorphous/Nanocrystalline Alloy Coatings, Surf. Coat. Technol., 2014, 238, p 118-12510.1016/j.surfcoat.2013.10.055 ↗
19. N.W. Khun, R.T. Li, K. Loke, and K.A. Khor, Effects of Al-Cr-Fe Quasicrystal Content on Tribological Properties of Cold Sprayed Titanium Composite Coatings, Tribol. Trans., 2015, 58(4), p 616-62410.1080/10402004.2014.991860 ↗
20. K. Ishikawa, T. Suzuki, Y. Kitamura, and S. Tobe, Corrosion Resistance of Thermal Sprayed Titanium Coatings in Chloride Solution, J. Therm. Spray Technol., 1999, 8(2), p 273-27810.1361/105996399770350494 ↗
21. T. Hussian, D.G. MaCartney, P.H. Shipway, and T. Marrocco, Corrosion Behaviour of Cold Sprayed Titanium Coatings and Free Standing Deposits, J. Therm. Spray Technol., 2011, 20(1–2), p 260-27410.1007/s11666-010-9540-x ↗
22. H.R. Wang, W.Y. Li, J. Wang, and Q. Wang, Corrosion Behaviour of Cold Sprayed Titanium Protective Coating on 1Cr13 Substrate in Seawater, Surf. Coat. Technol., 2007, 201(9–11), p 5203-520610.1016/j.surfcoat.2006.07.104 ↗
23. H. Assadi, F. Gartner, T. Stoltenhoff, and H. Kreye, Bonding mechanism in cold gas spraying, Acta Mater., 2003, 51, p 4379-439410.1016/S1359-6454(03)00274-X ↗
24. R. Huang, M. Sone, W. Ma, and H. Fukanuma, The Effect of Heat Treatment on the Mechanical Properties of Cold Sprayed Coatings, Surf. Coat. Technol., 2015, 261, p 278-28810.1016/j.surfcoat.2014.11.017 ↗
25. N.W. Khun, R.T. Li, and K.A. Khor, Mechanical and Tribological Properties of Spark Plasma Sintered Titanium Composites Filled with Different Al-Cr-Fe Quasicrystal Content, Tribol. Trans., 2015, 58(5), p 859-86610.1080/10402004.2015.1023411 ↗
26. N.W. Khun, G.S. Frankel, and M. Sumption, Effects of Normal Load, Sliding Speed and Surface Roughness on Tribological Properties of Niobium Under Dry and Wet Conditions, Tribol. Trans., 2014, 57(5), p 944-95410.1080/10402004.2014.927546 ↗
27. N.W. Khun, E. Liu, A.W.Y. Tan, D. Senthilkumar, B. Albert, and D.M. Lal, Effects of Deep Cryogenic Treatment on Mechanical and Tribological Properties of AISI, D3 Tool Steel, Friction, 2015, 3(3), p 234-24210.1007/s40544-015-0089-z ↗
28. J.H.W. Siu and L.K.Y. Li, An Investigation of the Effect of Surface Roughness and Coating Thickness on the Friction and Wear Behaviour of a Commercial MoS2-Metal Coating on AISI, 400C Steel, Wear, 2000, 237(2), p 283-28710.1016/S0043-1648(99)00349-X ↗
29. P.J. Blau, Friction science and technology, Marcel Dekker, New York, 1996
30. K. Kato, Wear in Relation to Friction: Review, Wear, 2005, 241, p 151-15710.1016/S0043-1648(00)00382-3 ↗
31. C.M. Mate, Tribology on the Small Scale: a Bottom Up Approach to Friction, Lubrication and Wear, 1st ed., Oxford University Press, Oxford, 2008
32. H. Ronkainen, A. Laukkanen, and K. Holmberg, Friction in a Coated Surface Deformed by a Sliding Sphere, Wear, 2007, 263(7–12), p 1315-132310.1016/j.wear.2007.01.103 ↗
33. B. Bhushan, Tribology and Mechanics of Magnetic Storage Device, 2nd ed., Springer, New York, 199610.1007/978-1-4612-2364-1 ↗
34. S. Stewart and R. Ahmed, Rolling Contact Fatigue of Surface Coatings: Reveiw, Wear, 2002, 253, p 1132-114410.1016/S0043-1648(02)00234-X ↗
35. S.H. Teoh, Fatigue of Biomaterials: a Review, Int. J. Fatigue, 2000, 22, p 825-83710.1016/S0142-1123(00)00052-9 ↗
36. E.S.M. Sherif, A.A. Almajid, K.A. Khalil, H. Junaedi, and F.H. Latief, Electrochemical Studies on the Corrosion Behaviour of API, X65 Pipeline Steel in Chloride Solutions, Int. J. Electrochem. Sci., 2013, 8, p 9360-937010.1016/S1452-3981(23)12975-0 ↗
37. R.M.A. Shahba, W.A. Ghannem, A.E.S. El-Shenawy, A.S.I. Ahemd, and S.M. Tantawy, Corrosion and Inhibition of Ti-6Al-4V Alloy in NaCl Solution, Int. J. Electrochem. Sci., 2011, 6, p 5499-550910.1016/S1452-3981(23)18423-9 ↗
38. H.J. Song, M.K. Kim, G.C. Jung, M.S. Vang, and Y.J. Park, The Effect of Spark Anodizing Treatment of Pure Titanium Metals and Titanium Alloys on Corrosion Characteristics, Surf. Coat. Technol., 2007, 201(21), p 8738-874510.1016/j.surfcoat.2006.11.022 ↗
39. N.W. Khun and G.S. Frankel, Effect of Hexafluorozirconic Acid Pretreatment on Cathodic Delamination of Epoxy Coatings from Steel Substrates, Corrosion, 2015, 71(3), p 277-28410.5006/1407 ↗
40. N.W. Khun and G.S. Frankel, Composition and Corrosion Protection of Hexafluorozirconic Acid Treatment on Steel, Mater. Corros., 2015, 66(11), p 1215-122210.1002/maco.201508255 ↗
41. A. Zeng, E. Liu, I.F. Annergren, S.N. Tan, S. Zhang, P. Hing, and J. Gao, EIS capacitance Diagnosis of Nanoporosity Effect on the Corrosion Protection of DLC Films, Diam. Relat. Mater., 2002, 11, p 160-16810.1016/S0925-9635(01)00568-4 ↗
42. S.M. Bhola and B. Mishra, Effect of pH on the Electrochemical Properties of Oxides Formed over α-Ti-15Mo and Mixed Ti-6Al-4V Alloys, Int. J. Electrochem. Sci., 2013, 8, p 7075-708710.1016/S1452-3981(23)14830-9 ↗
43. C. Moreno, S. Hernández, J.J. Santana, J. González-Guzmán, R.M. Souto, and S. González, Characterization of Water Uptake by Organic Coatings Used for the Corrosion Protection of Steel as Determined from Capacitance Measurements, Int. J. Electrochem. Sci., 2012, 7, p 8444-845710.1016/S1452-3981(23)18006-0 ↗
44. N.W. Khun, E. Liu, and X.T. Zeng, Corrosion Behaviour of Nitrogen Doped Diamond-Like Carbon Thin Films in NaCl Solution, Corros. Sci., 2009, 51(9), p 2158-216410.1016/j.corsci.2009.05.050 ↗
45. E.M. Fayyad, M.A. Almaadeed, A. Jones, and A.M. Abdullah, Evaluation Techniques for the Corrosion Resistance of Self-Healing Coatings, Int. J. Electrochem. Sci., 2014, 9, p 4989-501110.1016/S1452-3981(23)08147-6 ↗
46. S. Kuroda, J. Kawakita, T. Fukushima, and S. Tobe, Importance of the Adhesion of HVOF Sprayed Coatings for Aqueous Corrosion Resistance, Mater. Trans., 2003, 44(3), p 381-38810.2320/matertrans.44.381 ↗