High-Velocity Suspension Flame Sprayed (HVSFS) Hydroxyapatite Coatings for Biomedical Applications
Source abstract
Abstract
In this study, hydroxyapatite (HAp) coatings were deposited on Ti plates by the high-velocity suspension flame spraying (HVSFS) technique. The process characteristic, the microstructure and phase composition of the coatings are significantly influenced by the solvent and by the design of the combustion chamber (CC) of the HVSFS torch. Water-based suspensions always lead to fairly low surface temperatures (≈350 °C), deposition efficiencies <40%, and produce coatings with low amount of crystalline HAp, which tend to dissolve very rapidly in simulated body fluid (SBF) solutions. DEG-based suspensions, when sprayed with properly-designed CCs, produce deposition efficiencies of 45-55% and high surface temperatures (550-600 °C). In these coatings, the degree of crystallinity increases from the bottom layer to the top layer, probably because the increasingly large surface temperature can eventually favour re-crystallisation of individual lamellae during cooling. These coatings are much more stable in SBF solutions.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Bone Tissue Engineering Materials · Advanced materials and composites · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. S. Kurtz, E. Lau, M. Halpern, and K. Ong, Trend Shows Growing Orthopedic Surgery Case Load, Mater. Manag. Health Care, 2006, 15(7), p 61-62
2. E. Wintermantel and H. Suk-Woo, Medizintechnik mit biokompatiblen Werkstoffen und Verfahren, 3rd ed., Springer, New York, 2002, p 216-228, ISBN 3-540-41261-1 (in German)
3. C.L. Tisdel, V.M. Goldberg, J.A. Parr, J.S. Bensusan, L.S. Staikoff, and S. Stevenson, The Influence of a Hydroxyapatite and Tricalcium-Phosphate Coating on Bone Growth into Titanium Fiber-Metal Implants, J. Bone Jt. Surg. Am., 1994, 76, p 159-17110.2106/00004623-199402000-00001 ↗
4. J. Dumbleton and M.T. Manley, Hydroxyapatite-Coated Prostheses in Total Hip and Knee Arthroplasty, J. Bone Jt. Surg. Am., 2004, 86, p 2526-254010.2106/00004623-200411000-00028 ↗
5. R. Petit, The Use of Hydroxyapatite in Orthopaedic Surgery: A Ten-Year Review, Eur. J. Orthop. Surg. Traumatol., 1999, 9, p 71-7410.1007/BF01695730 ↗
6. L. Sun, C.C. Berndt, K.A. Gross, and A. Kucuk, Materials Fundamentals and Clinical Performance of Plasma-Sprayed Hydroxyapatite Coatings: A Review, J. Biomed. Mater. Res., 2001, 58, p 570-59210.1002/jbm.1056 ↗
7. K.A. Khor, P. Cheang, and Y. Wang, The Thermal Spray Processing of HA Powders and Coatings, JOM, 1997, 49(2), p 51-5710.1007/BF02915482 ↗
8. K.A. Khor, H. Li, and P. Cheang, Significance of Melt-Fraction in HVOF Sprayed Hydroxyapatite Particles, Splats and Coatings, Biomaterials, 2004, 25(7), p 1177-118610.1016/j.biomaterials.2003.08.008 ↗
9. K. Gross and C. Berndt, Thermal Processing of HA for Coating Production, J. Biomed. Mater. Res. B, 1998, 39(4), p 580-58710.1002/(SICI)1097-4636(19980315)39:4<580::AID-JBM12>3.0.CO;2-B ↗
10. R.B. Heimann, Recent Trends Towards Improved Plasma-Sprayed Advanced Bioceramic Coatings on Ti6Al4V Implants, Mat.-wiss. u. Werkstofftech., 1999, 30, p 775-78210.1002/(SICI)1521-4052(199912)30:12<775::AID-MAWE775>3.0.CO;2-W ↗
11. S. Dyshlovenko, C. Pierlot, L. Pawlowski, R. Tomaszek, and P. Chagnon, Experimental Design of Plasma Spraying and Laser Treatment of Hydroxyapatite Coatings, Surf. Coat. Technol., 2006, 201, p 2054-206010.1016/j.surfcoat.2006.04.055 ↗
12. E. Bouyer, F. Gitzhofer, and M.I. Boulos, Suspension Plasma Spraying for Hydroxyapatite Powder Preparation by R.F. Plasma, J. Mater. Sci. Lett., 1997, 49(2), p 58-62
13. C. Renghini, E. Girardin, A.S. Fomin, A. Manescu, A. Sabbioni, S.M. Barinov, V.S. Komlev, G. Albertini, and F. Fiori, Plasma Sprayed Hydroxyapatite Coatings from Nanostructured Granules, Mater. Sci. Eng. B, 2008, 152(1-3), p 86-9010.1016/j.mseb.2008.06.016 ↗
14. R.S. Lima, K.A. Khor, H. Li, P. Cheang, and B.R. Marple, HVOF Spraying of Nanostructured Hydroxyapatite for Biomedical Applications, Mater. Sci. Eng. A, 2005, 396, p 181-18710.1016/j.msea.2005.01.037 ↗
15. H. Li and K.A. Khor, Characteristics of the Nanostructures in Thermal Sprayed Hydroxyapatite Coatings and Their Influence on Coating Properties, Surf. Coat. Technol., 2006, 201(6), p 2147-215410.1016/j.surfcoat.2006.03.024 ↗
16. H. Li, B.S. Ng, K.A. Khor, P. Cheang, and T.W. Clyne, Raman Spectroscopy Determination of Phases Within Thermal Sprayed Hydroxyapatite Splats and Subsequent In Vitro Dissolution Examination, Acta Mater., 2004, 52, p 445-45310.1016/j.actamat.2003.09.046 ↗
17. K.A. Khor, H. Li, and P. Cheang, Significance of Melt-Fraction in HVOF Sprayed Hydroxyapatite Particles, Splats and Coatings, Biomaterials, 2004, 25, p 1177-118610.1016/j.biomaterials.2003.08.008 ↗
18. K.A. Gross, S. Saber-Samandari, and K.S. Heemann, Evaluation of Commercial Implants with Nanoindentation Defines Future Development Needs for Hydroxyapatite Coatings, J. Biomed. Mater. Res. B, 2010, 93(1), p 1-810.1002/jbm.b.31537 ↗
19. N. Cao, J. Dong, Q. Wang, Q. Ma, C. Xue, and M. Li, An Experimental Bone Defect Healing with Hydroxyapatite Coating Plasma Sprayed on Carbon/Carbon Composite Implants, Surf. Coat. Technol., 2010, 205(4), p 1150-115610.1016/j.surfcoat.2010.05.008 ↗
20. R.W. Trice and K.T. Faber, Role of Lamellae Morphology on the Microstructural Development and Mechanical Properties of Small-Particle Plasma-Sprayed Alumina, J. Am. Ceram. Soc., 2000, 83(4), p 889-89610.1111/j.1151-2916.2000.tb01290.x ↗
21. C. Monterrubio-Badillo, H. Ageorges, T. Chartier, J.F. Coudert, and P. Fauchais, Preparation of LaMnO3 Perovskite Thin Films by Suspension Plasma Spraying for SOFC Cathodes, Surf. Coat. Technol., 2006, 200, p 3743-375610.1016/j.surfcoat.2005.01.002 ↗
22. F.-L. Toma, G. Bertrand, D. Klein, C. Coddet, and C. Meunier, Nanostructured Photocatalytic Titania Coatings Formed by Suspension Plasma Spraying, J. Therm. Spray Technol., 2006, 15(4), p 587-59210.1361/105996306X147234 ↗
23. F.-L. Toma, G. Bertrand, S. Begin, C. Meunier, O. Barres, D. Klein, and C. Coddet, Microstructure and Environmental Functionalities of TiO2-Supported Catalysts Obtained by Suspension Plasma Spraying, Appl. Catal. B, 2006, 68, p 74-8410.1016/j.apcatb.2006.07.009 ↗
24. A. Killinger, M. Kuhn, and R. Gadow, High-Velocity Suspension Flame Spraying (HVSFS), a New Approach for Spraying Nanoparticles with Hypersonic Speed, Surf. Coat. Technol., 2006, 201(5), p 1922-192910.1016/j.surfcoat.2006.04.034 ↗
25. X.Q. Ma, J. Roth, D.W. Gandy, and G.J. Frederick, A New High-Velocity Oxygen Fuel Process for Making Finely Structured and Highly Bonded Inconel Alloy Layers from Liquid Feedstock, J. Therm. Spray Technol., 2006, 15, p 670-67510.1361/105996306X147090 ↗
26. R. Rampon, F.-L. Toma, G. Bertrand, and C. Coddet, Liquid Plasma Sprayed Coatings of Yttria-Stabilized Zirconia for SOFC Electrolytes, J. Therm. Spray Technol., 2006, 15(4), p 682-68810.1361/105996306X146712 ↗
27. P. Fauchais, R. Etchart-Salas, V. Rat, J.F. Coudert, N. Caron, and K. Wittmann-Ténèze, Parameters Controlling Liquid Plasma Spraying: Solutions, Sols, or Suspensions, J. Therm. Spray Technol., 2008, 17(1), p 31-5910.1007/s11666-007-9152-2 ↗
28. R. Gadow, A. Killinger, M. Kuhn, and D. López, Hochgeschwindigkeitssuspensionsflammspritzen, Deutsche Patentanmeldung Nr. DE 10 2005 038 453 A1 (in German)
29. Thermal Spray 2009: Expanding Thermal Spray Performance to New Markets and Applications, B.R. Marple, M.M. Hyland, Y.-C. Lau, C.-J. Li, R.S. Lima, and G. Montavon, Eds., 4-7 May 2009(Las Vegas, NV), ASM International, 2009, p 150-155
30. T. Kokubo and H. Takadama, How Useful is SBF in Predicting In Vivo Bone Bioactivity?, Biomaterials, 2006, 27, p 2907-291510.1016/j.biomaterials.2006.01.017 ↗
31. A. Killinger, M. Kuhn, and R. Gadow, High-Velocity Suspension Flame Spraying (HVSFS), a New Approach for Spraying Nanoparticles with Hypersonic Speed, Surf. Coat. Technol., 2006, 201, p 1922-192910.1016/j.surfcoat.2006.04.034 ↗
32. R. Lietzow, “Herstellung von Nanosuspensionen mittels Entspannung überkritischer Fluide”, Ph.D. Thesis, Universität Karlsruhe, Cuvillier-Verlag, 2006, ISBN 978-3-86727-080-9 (in German)
33. C. Synowietz and K. Schäfer, Chemiker-Kalender, 3rd ed., C. Synowietz and K. Schäfer, Eds., 1984, Springer, 1984, ISBN 3-540-12652-x10.1007/978-3-642-61734-8 ↗
34. L. Pawlowski, Finely Grained Nanometric and Submicrometric Coatings by Thermal Spraying: A Review, Surf. Coat. Technol., 2008, 202(18), p 4318-432810.1016/j.surfcoat.2008.04.004 ↗
35. R. Gadow, A. Killinger, and N. Stiegler, Hydroxyapatite Coatings for Biomedical Applications Deposited by Different Thermal Spray Techniques, Surf. Coat. Technol., 2010, 205, p 1157-116410.1016/j.surfcoat.2010.03.059 ↗
36. K. VanEvery, M.J.M. Krane, R.W. Trice, H. Wang, W. Porter, M. Besser, D. Sordelet, J. Ilavsky, and J. Almer, Column Formation in Suspension Plasma-Sprayed Coatings and Resultant Thermal Properties, J. Therm. Spray Technol., 2011, 20, p 817-82810.1007/s11666-011-9632-2 ↗
37. G. Bolelli, V. Cannillo, R. Gadow, A. Killinger, L. Lusvarghi, J. Rauch, and M. Romagnoli, Effect of the Suspension Composition on the Microstructural Properties of High Velocity Suspension Flame Sprayed (HVSFS) Al2O3 Coatings, Surf. Coat. Technol., 2010, 204(8), p 1163-117910.1016/j.surfcoat.2009.10.045 ↗
38. E. Dongmo, A. Killinger, M. Wenzelburger, and R. Gadow, Numerical Approach and Optimization of the Combustion and Gas Dynamics in High Velocity Suspension Flame Spraying (HVSFS), Surf. Coat. Technol., 2009, 203(15), p 2139-214510.1016/j.surfcoat.2008.12.006 ↗
39. U. Posset, E. Löcklin, R. Thull, and W. Kiefer, Vibrational Spectroscopic Study of Tetracalcium Phosphate in Pure Polycrystalline Form and as a Constituent of Self-Setting Bone Cement, J. Biomed. Mater. Res., 1998, 40, p 640-64510.1002/(SICI)1097-4636(19980615)40:4<640::AID-JBM16>3.0.CO;2-J ↗
40. R. Cuscò, F. Guitián, S. de Aza, and L. Artús, Differentiation Between Hydroxyapatite and Beta-Tricalcium Phosphate by Means of Micro-Raman Spectroscopy, J. Eur. Ceram. Soc., 1998, 18(9), p 1301-130510.1016/S0955-2219(98)00057-0 ↗
41. R.B. Heimann, Thermal Spraying of Biomaterials, Surf. Coat. Technol., 2006, 201(5), p 2012-201910.1016/j.surfcoat.2006.04.052 ↗
42. S. Dyshlovenko, L. Pawlowski, B. Pateyron, I. Smurov, and J.H. Harding, Modelling of Plasma Particle Interactions and Coating Growth for Plasma Spraying of Hydroxyapatite, Surf. Coat. Technol., 2006, 200, p 3757-376910.1016/j.surfcoat.2005.04.002 ↗
43. R. Jaworski, C. Pierlot, L. Pawlowski, M. Bigan, and M. Quivrin, Synthesis and Preliminary Tests of Suspension Plasma Spraying of Fine Hydroxyapatite Powder, J. Therm. Spray Technol., 2008, 17(5-6), p 679-68410.1007/s11666-008-9220-2 ↗
44. P. Fauchais, M. Fukumoto, A. Vardelle, and M. Vardelle, Knowledge Concerning Splat Formation: An Invited Review, J. Therm. Spray Technol., 2004, 13(3), p 337-36010.1361/10599630419670 ↗
45. C. Chang, J. Huang, J. Xia, and C. Ding, Study on Crystallization Kinetics of Plasma Sprayed Hydroxyapatite Coating, Ceram. Int., 1999, 25, p 479-48310.1016/S0272-8842(98)00063-7 ↗
46. C.T. Crowe, T.R. Troutt, and J.N. Chung, Numerical Models for Two-Phase Turbulent Flows, Annu. Rev. Fluid Mech., 1996, 28, p 11-4310.1146/annurev.fl.28.010196.000303 ↗
47. P.C. Huang, J. Heberlein, and E. Pfender, Particle Behavior in a Two-Fluid Turbulent Plasma Jet, Surf. Coat. Technol., 1995, 73, p 142-15110.1016/0257-8972(94)02382-4 ↗
48. M. Ivosevic, R.A. Cairncross, and R. Knight, 3D Predictions of Thermally Sprayed Polymer Splats: Modeling Particle Acceleration, Heating and Deformation on Impact with a Flat Substrate, Int. J. Heat Mass Transf., 2006, 49, p 3285-329710.1016/j.ijheatmasstransfer.2006.03.028 ↗
49. V.R. Srivatsan and A. Dolatabadi, Simulation of Particle-Shock Interaction in a High Velocity Oxygen Fuel Process, J. Therm. Spray Technol., 2006, 15(4), p 481-48710.1361/105996306X147126 ↗
50. J. Oberste Berghaus, J.-G. Legoux, C. Moreau, F. Tarasi, and T. Chráska, Mechanical and Thermal Transport Properties of Suspension Thermal-Sprayed Alumina-Zirconia Composite Coatings, J. Therm. Spray Technol., 2008, 17(1), p 91-10410.1007/s11666-007-9146-0 ↗
51. S.W.K. Kweh, K.A. Khor, and P. Cheang, Plasma-Sprayed Hydroxyapatite (HA) Coatings with Flame-Spheroidized Feedstock: Microstructure and Mechanical Properties, Biomaterials, 2000, 21(12), p 1223-123410.1016/S0142-9612(99)00275-6 ↗
52. H.C. Gledhill, I.G. Turner, and C. Doyle, In Vitro Dissolution Behaviour of Two Morphologically Different Thermally Sprayed Hydroxyapatite Coatings, Biomaterials, 2001, 22(7), p 695-70010.1016/S0142-9612(00)00232-5 ↗
53. S.-W. Ha, R. Reber, K.-L. Eckert, M. Petitmermet, J. Mayer, E. Wintermantel, C. Baerlocher, and H. Gruner, Chemical and Morphological Changes of Vacuum-Plasma-Sprayed Hydroxyapatite Coatings During Immersion in Simulated Physiological Solutions, J. Am. Ceram. Soc., 1998, 81, p 81-8810.1111/j.1151-2916.1998.tb02298.x ↗
54. D. Lahiri, A.P. Benaduce, F. Rouzaud, J. Solomon, A.K. Keshri, L. Kos, and A. Agarwal, Wear Behavior and In Vitro Cytotoxicity of Wear Debris Generated from Hydroxyapatite-Carbon Nanotube Composite Coating, J. Biomed. Mater. Res. A, 2011, 96(1), p 1-1210.1002/jbm.a.32952 ↗
55. M. Bohner and J. Lemaitre, Can Bioactivity be Tested In Vitro with SBF Solution?, Biomaterials, 2009, 30, p 2175-217910.1016/j.biomaterials.2009.01.008 ↗