Environmentally Resistant Mo-Si-B-Based Coatings
Source abstract
Abstract
High-temperature applications have demonstrated aluminide-coated nickel-base superalloys to be remarkably effective, but are reaching their service limit. Alternate materials such as refractory (e.g., W, Mo) silicide alloys and SiC composites are being considered to extend high temperature capability, but the silica surfaces on these materials require coatings for enhanced environmental resistance. This can be accomplished with a Mo-Si-B-based coating that is deposited by a spray deposition of Mo followed by a chemical vapor deposition of Si and B by pack cementation to develop an aluminoborosilica surface. Oxidation of the as-deposited (Si + B)-pack coatings proceeds with partial consumption of the initial MoSi2 forming amorphous silica. This Si depletion leads to formation of a B-saturated Mo5Si3 (T1) phase. Reactions between the Mo and the B rich phases develop an underlying Mo5SiB2 (T2) layer. The T1 phase saturated with B has robust oxidation resistance, and the Si depletion is prevented by the underlying diffusion barrier (T2). Further, due to the natural phase transformation characteristics of the Mo-Si-B system, cracks or scratches to the outer silica and T1 layers can be repaired from the Si and B reservoirs of T2 + MoB layer to yield a self-healing characteristic. Mo-Si-B-based coatings demonstrate robust performance up to at least 1700 °C not only to the rigors of elevated temperature oxidation, but also to CMAS attack, hot corrosion attack, water vapor and thermal cycling.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Advanced ceramic materials synthesis · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. D.M. Dimiduk and J.H. Perepezko, Mo-Si-B Alloys: Developing a Revolutionary Turbine-Engine Material, MRS Bull., 2003, 28(9), p 639-64510.1557/mrs2003.191 ↗
2. J.H. Perepezko, The Hotter The Engine, The Better, Science, 2009, 326, p 1068-106910.1126/science.1179327 ↗
3. J.A. Lemberg and R.O. Ritchie, Mo-Si-B Alloys for Ultrahigh-Temperature Structural Applications, Adv. Mater., 2012, 24(26), p 1-3610.1002/adma.201200764 ↗
4. J.H. Perepezko and R. Sakidja, Oxidation Resistant Coatings for Ultra-High Temperature Refractory Mo-Base Alloys, Adv. Eng. Mater., 2009, 11, p 892-89710.1002/adem.200900118 ↗
5. J.H. Perepezko and R. Sakidja, Extended Functionality of Environmentally-Resistant Mo-Si-B-Based Coatings, JOM, 2013, 65, p 307-31710.1007/s11837-012-0520-0 ↗
6. E.J. Opila, N.S. Jacobson, D.L. Myers, and E.H. Copland, Predicting Oxide Stability in High-Temperature Water Vapor, JOM, 2006, 58(1), p 22-2810.1007/s11837-006-0063-3 ↗
7. J.H. Perepezko, Surface Engineering of Mo-Base Alloys for Elevated Temperature Environmental Resistance, Annu. Rev. Mater. Res., 2015, 45, p 519-54210.1146/annurev-matsci-070214-020959 ↗
8. I. Spitsberg and J. Steibel, Thermal and Environmental Barrier Coatings for SiC/SiC CMCs in Aircraft Engine Applications, Int. J. Appl. Ceram. Technol., 2004, 1(4), p 291-30110.1111/j.1744-7402.2004.tb00181.x ↗
9. P. Ritt, O.J. Lu-Steffes, R. Sakidja, J.H. Perepezko, W. Lenling, D. Crawmer, and J. Beske, Application of Plasma Spraying as a Precursor in the Synthesis of Oxidation-Resistant Coatings, J. Thermal Spray Tech., 2013, 22(6), p 992-100110.1007/s11666-013-9947-2 ↗
10. J.L. Sabourin and R.A. Yetter, High-Temperature Heterogeneous Reaction Kinetics of Tungsten Oxidation by CO(2), CO, and O(2), J. Propuls. Power, 2009, 25(2), p 490-49810.2514/1.38123 ↗
11. J.H. Perepezko and R. Sakidja, Oxidation-Resistant Coatings for Ultra-High-Temperature Refractory Mo-Based Alloys, JOM, 2010, 62(10), p 13-1910.1007/s11837-010-0148-x ↗
12. P. Ritt, R. Sakidja, and J.H. Perepezko, Mo-Si-B Based Coating for Oxidation Protection of SiC-C Composites, Surf. Coat. Technol., 2012, 206(19-20), p 4166-417210.1016/j.surfcoat.2012.04.016 ↗
13. V.A. Ravi, S.D. Cramer, and B.S. Covino, Jr., Pack cementation coatings, ASM Handbook, Volume 13A: Corrosion: Fundamentals, Testing, and Protection, S.D. Cramer, and B.S. Covino, Jr., Eds., ASM International, Materials Park, 2003, p 763-77110.31399/asm.hb.v13a.a0003686 ↗
14. R. Sakidja, F. Rioult, J. Werner, and J.H. Perepezko, Aluminum Pack Cementation of Mo-Si-B Alloys, Scr. Mater., 2006, 55, p 90310.1016/j.scriptamat.2006.07.044 ↗
15. M. Akinc, M.K. Meyer, M.J. Kramer, A.J. Thom, J.J. Huebsch, and B. Cook, Mater. Sci. Eng., 1999, 261, p 1610.1016/S0921-5093(98)01045-4 ↗
16. M.K. Meyer, A.J. Thom, and M. Akinc, Oxide Scale Formation and Isothermal Oxidation Behavior of Mo-Si-B Intermetallics at 600-1000 °C, Intermetallics, 1999, 7, p 15310.1016/S0966-9795(98)00058-2 ↗
17. N.S. Jacobson, D.L. Myers, E.J. Opila, and E.H. Copland, Interactions of Water Vapor with Oxides at Elevated Temperatures, J. Phys. Chem. Solids, 2005, 66, p 471-47810.1016/j.jpcs.2004.06.044 ↗
18. E.J. Opila, Oxidation and Volatilization of Silica Formers in Water Vapor, J. Am. Ceram. Soc., 2003, 86, p 1238-124810.1111/j.1151-2916.2003.tb03459.x ↗
19. E.J. Opila, Paralinear Oxidation of CVD SiC in Water Vapor, J. Am. Ceram. Soc., 1997, 80, p 197-20510.1111/j.1151-2916.1997.tb02810.x ↗
20. E.J. Opila, Paralinear Oxidation of Silicon Nitride in a Water-Vapor/Oxygen Environment, J. Am. Ceram. Soc., 2003, 86, p 1256-126110.1111/j.1151-2916.2003.tb03461.x ↗
21. F. Rebillat, X. Martin, E. Garitte, and A. Guette, Design, Development, and Applications of Engineering Ceramics and Composites, Am. Ceram. Soc., 2010, 215, p 151-166
22. K. Gente, F. Rebillat, and F. Langlais, High Temperature Corrosion and Materials Chemistry III: Proceedings of the International Symposium, Pennington NJ Electrochemical Society, 2003, pp. 545-556.
23. P. Mandal, A.J. Thom, M.J. Kramer, V. Behrani, and M. Akinc, Mater. Sci. Eng. A, 2004, 371, p 335-34210.1016/j.msea.2003.12.025 ↗
24. F.A. Rioult, S.D. Imhoff, R. Sakidja, and J.H. Perepezko, Transient Oxidation of Mo-Si-B Alloys: Effect of the Microstructure Size Scale, Acta Mater., 2009, 57, p 4600-461310.1016/j.actamat.2009.06.036 ↗
25. J.M. Drexler, K. Shinoda, A.L. Ortiz, D.S. Li, A.L. Vasiliev, A.D. Gledhill, S. Sampath, and N.P. Padture, Air-Plasma-Sprayed Thermal Barrier Coatings that are Resistant to High-Temperature Attack by Glassy Deposits, Acta Mater., 2010, 58, p 6835-684410.1016/j.actamat.2010.09.013 ↗
26. T.A. Jackson, D.R. Eklund, and A.J. Fink, High Speed Propulsion: Performance Advantage of Advanced Materials, J. Mater. Sci., 2004, 39, p 590510.1023/B:JMSC.0000041687.37448.06 ↗
27. W.G. Fahrenholtz and G.E. Hilmas, Oxidation of Ultra-High Temperature Transition Metal Diboride Ceramics, Int. Mater. Rev., 2012, 57, p 6110.1179/1743280411Y.0000000012 ↗
28. M.M. Opeka, I.G. Talmy, and J.A. Zaykoski, Oxidation-Based Materials Selection for 2000 C+ Hypersonic Aerosurfaces: Theoretical Considerations and Historical Experience, J. Mater. Sci., 2004, 39, p 588710.1023/B:JMSC.0000041686.21788.77 ↗
29. E. Eakins, D.D. Jayaseelan, and W.E. Lee, Toward Oxidation-Resistant ZrB2-SiC Ultra High Temperature Ceramics, Metall. Mater. Trans. A, 2011, 42A, p 87810.1007/s11661-010-0540-8 ↗
30. P.J. Ritt, P.A. Williams, S.C. Splinter, and J.H. Perepezko, Arc Jet Testing and Evaluation of Mo-Si-B Coated Mo and SiC-ZrB2 Ceramics, J. Eur. Ceram. Soc., 2013, 34(15), p 3521-353310.1016/j.jeurceramsoc.2014.06.011 ↗
31. N.P. Padture, M. Gell, and E.H. Jordan, Thermal Barrier Coatings for Gas-Turbine Engine Applications, Science, 2002, 296, p 280-28410.1126/science.1068609 ↗
32. R.C. Reed, Superalloys and Coatings for High-Temperature Applications, JOM, 2006, 58, p 3610.1007/s11837-006-0065-1 ↗
33. X. Chen, Calcium-Magnesium-Alumina-Silicate (CMAS) Delamination Mechanisms in EB-PVD Thermal Barrier Coatings, Surf. Coat. Technol., 2006, 200, p 3418-342710.1016/j.surfcoat.2004.12.029 ↗
34. S. Kramer, J. Yang, C.G. Levi, and C.A. Johnson, Thermochemical Interaction of Thermal Barrier Coatings with Molten CaO-MgO-Al2O3-SiO2 (CMAS) Deposits, J. Am. Ceram. Soc., 2006, 89, p 3167-317510.1111/j.1551-2916.2006.01209.x ↗
35. B.J. Harder, J. Ramirez-Rico, J.D. Almer, K.N. Lee, and K.T. Faber, Chemical and Mechanical Consequences of Environmental Barrier Coating Exposure to Calcium-Magnesium-Aluminosilicate, J. Am. Ceram. Soc., 2011, 94, p S178-S18510.1111/j.1551-2916.2011.04448.x ↗
36. A.G. Evans and J.W. Hutchinson, The Mechanics of Coating Delamination in Thermal Gradients, Surf. Coat. Technol., 2007, 201, p 7905-791610.1016/j.surfcoat.2007.03.029 ↗
37. S. Kramer, S. Faulhaber, M. Chambers, D.R. Clarke, C.G. Levi, J.W. Hutchinson, and A.G. Evans, Mechanisms of Cracking and Delamination Within Thick Thermal Barrier Systems in Aero-Engines Subject to Calcium-Magnesium-Alumino-Silicate (CMAS) Penetration, Mater. Sci. Eng. A, 2008, 490, p 26-3510.1016/j.msea.2008.01.006 ↗
38. I.P. Downs, J.H. Perepezko, R. Sakidja, and S.R. Choi, Suppressing CMAS Attack with a MoSiB-Based Coating, Surf. Coat. Technol., 2014, 239, p 138-14610.1016/j.surfcoat.2013.11.032 ↗
39. R.A. Rapp, Hot Corrosion of Materials: A Fluxing Mechanism?, Corros. Sci., 2002, 44(2), p 209-22110.1016/S0010-938X(01)00057-9 ↗
40. N. Eliaz, G. Shemesh, and R.M. Latanision, Hot Corrosion in Gas Turbine Components, Eng. Fail. Anal., 2002, 9(1), p 31-4310.1016/S1350-6307(00)00035-2 ↗
41. M.G. Lawson, H.R. Kim, F.S. Pettit, and J.R. Blachere, Hot Corrosion of Silica, J. Am. Ceram. Soc., 1990, 73(4), p 989-99510.1111/j.1151-2916.1990.tb05147.x ↗
42. A. Lange, M. Heilmaier, T. Sossamann, and J.H. Perepezko, Oxidation Behavior of Pack-Cemented Si-B Oxidation Protection Coatings for Mo-Si-B Alloys at 1300 °C, Surf. Coat. Technol., 2015, 266, p 57-6310.1016/j.surfcoat.2015.02.015 ↗