Abstract

KCl-induced high-temperature corrosion behavior of four HVAF-sprayed Ni-based coatings (Ni21Cr, Ni5Al, Ni21Cr7Al1Y and Ni21Cr9Mo) under KCl deposit has been investigated in ambient air at 600 °C up to 168 h. The coatings were deposited onto 16Mo3 steel—a widely used boiler tube material. Uncoated substrate, 304L and Sanicro 25 were used as reference materials in the test environment. SEM/EDS and XRD techniques were utilized to characterize the as-sprayed and exposed samples. The results showed that the small addition of KCl significantly accelerated degradation to the coatings. All coatings provided better corrosion resistance compared to the reference materials. The alumina-forming Ni5Al coating under KCl deposit was capable of forming a more protective oxide scale compared to the chromia-forming coatings as penetration of Cl through diffusion paths was hindered. Both active corrosion and chromate formation mechanisms were found to be responsible for the corrosion damages. The corrosion resistance of the coatings based on the microstructure analysis and kinetics had the following ranking (from the best to worst): Ni5Al > Ni21Cr > Ni21Cr7Al1Y > Ni21Cr9Mo.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · Thermochemical Biomass Conversion Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. R. Saidur, E.A.A. Abdelaziz, A. Demirbas, M.S.S. Hossain, and S. Mekhilef, A Review on Biomass as a Fuel for Boilers, Renew. Sustain. Energy Rev., 2011, 15(5), p 2262-228910.1016/j.rser.2011.02.015 ↗
2. N. Otsuka, A Thermodynamic Approach on Vapor-Condensation of Corrosive Salts from Flue Gas on Boiler Tubes in Waste Incinerators, Corros. Sci., 2008, 50(6), p 1627-163610.1016/j.corsci.2008.02.004 ↗
3. M. Montgomery, S.A. Jensen, U. Borg, O. Biede, and T. Vilhelmsen, Experiences with High Temperature Corrosion at Straw-Firing Power Plants in Denmark, Mater. Corros., 2011, 62(7), p 593-60510.1002/maco.201005856 ↗
4. H.J. Grabke, E. Reese, and M. Spiegel, The Effects of Chlorides, Hydrogen Chloride, and Sulfur Dioxide in the Oxidation of Steels Below Deposits, Corros. Sci., 1995, 37(7), p 1023-104310.1016/0010-938X(95)00011-8 ↗
5. A. Zahs, M. Spiegel, and H.J.J. Grabke, Chloridation and Oxidation of Iron, Chromium, Nickel and Their Alloys in Chloridizing and Oxidizing Atmospheres at 400-700 °C, Corros. Sci., 2000, 42(6), p 1093-112210.1016/S0010-938X(99)00142-0 ↗
6. H.P. Nielsen, F.J. Frandsen, K. Dam-Johansen, and L.L. Baxter, Implications of Chlorine-Associated Corrosion on the Operation Of Biomass-Fired Boilers, Prog. Energy Combust. Sci., 2000, 26(3), p 283-29810.1016/S0360-1285(00)00003-4 ↗
7. T. Blomberg, Which are the Right Test Conditions for the Simulation of High Temperature Alkali Corrosion in Biomass Combustion?, Mater. Corros., 2006, 57(2), p 170-17510.1002/maco.200503905 ↗
8. M. Spiegel, A. Zahs, and H.J. Grabke, Fundamental Aspects of Chlorine Induced Corrosion, Mater. High Temp., 2003, 20(2), p 153-15910.1179/mht.2003.018 ↗
9. T. Jonsson, J. Froitzheim, J. Pettersson, J.E. Svensson, L.G. Johansson, and M. Halvarsson, The Influence of KCl on the Corrosion of an Austenitic Stainless Steel (304L) in Oxidizing Humid Conditions at 600 °C: A Microstructural Study, Oxid. Met., 2009, 72(3-4), p 213-23910.1007/s11085-009-9156-z ↗
10. C. Pettersson, J. Pettersson, H. Asteman, J.E. Svensson, and L.G. Johansson, KCl-Induced High Temperature Corrosion of the Austenitic Fe-Cr-Ni Alloys 304L and Sanicro 28 at 600 °C, Corros. Sci., 2006, 48(6), p 1368-137810.1016/j.corsci.2005.05.018 ↗
11. J. Pettersson, H. Asteman, J.E. Svensson, and L.G. Johansson, KCl Induced Corrosion of a 304-Type Austenitic Stainless Steel at 600 °C; the Role of Potassium, Oxid. Met., 2005, 64(1-2), p 23-4110.1007/s11085-005-5704-3 ↗
12. C. Berlanga and J.A. Ruiz, Study of Corrosion in a Biomass Boiler, J. Chem., 2013, 2013, p 1-810.1155/2013/272090 ↗
13. Y. Kawahara, Application of High Temperature Corrosion-Resistant Materials and Coatings Under Severe Corrosive Environment in Waste-to-Energy Boilers, J. Therm. Spray Technol., 2007, 16(2), p 202-21310.1007/s11666-006-9012-5 ↗
14. R. Bender and M. Schütze, The Role of Alloying Elements in Commercial Alloys for Corrosion Resistance in Oxidizing–Chloridizing Atmospheres Part I: Literature Evaluation and Thermodynamic Calculations on Phase Stabilities, Mater. Corros., 2003, 54(8), p 567-58610.1002/maco.200390129 ↗
15. E.O. Ezugwu, Z.M. Wang, and A.R. Machado, The Machinability of Nickel-Based Alloys: A Review, J. Mater. Process. Technol., 1999, 86(1-3), p 1-1610.1016/S0924-0136(98)00314-8 ↗
16. L. Pawlowski, The Science and Engineering of Thermal Spray Coatings, John Wiley & Sons, 200810.1002/9780470754085 ↗
17. M. Oksa, J. Metsäjoki, and J. Kärki, Thermal Spray Coatings for High-Temperature Corrosion Protection in Biomass Co-Fired Boilers, J. Therm. Spray Technol., 2014, 24(1-2), p 194-205
18. S. Tuurna, T. Varis, K. Penttilä, K. Ruusuvuori, S. Holmström, and S. Yli-Olli, Optimised Selection of New Protective Coatings for Biofuel Boiler Applications, Mater. Corros., 2011, 62(7), p 642-64910.1002/maco.201005898 ↗
19. T. Varis et al., High Temperature Corrosion of Thermally Sprayed NiCr and FeCr Coatings Covered with a KCl-K2SO4 Salt Mixture, Surf. Coat. Technol., 2015, 265, p 235-24310.1016/j.surfcoat.2014.11.012 ↗
20. T. Hussain, T. Dudziak, N.J. Simms, and J.R. Nicholls, Fireside Corrosion Behavior of HVOF and Plasma-Sprayed Coatings in Advanced Coal/Biomass Co-fired Power Plants, J. Therm. Spray Technol., 2013, 22(5), p 797-80710.1007/s11666-013-9887-x ↗
21. M.A. Uusitalo, P.M.J. Vuoristo, and T.A. Mäntylä, High Temperature Corrosion of Coatings and Boiler Steels Below Chlorine-Containing Salt Deposits, Corros. Sci., 2004, 46(6), p 1311-133110.1016/j.corsci.2003.09.026 ↗
22. M. Uusitalo, P.M. Vuoristo, and T. Mäntylä, High Temperature Corrosion of Coatings and Boiler Steels in Oxidizing Chlorine-Containing Atmosphere, Mater. Sci. Eng. A, 2003, 346(1-2), p 168-17710.1016/S0921-5093(02)00537-3 ↗
23. G. Bolelli et al., Tribological Behavior of HVOF- and HVAF-Sprayed Composite Coatings Based on Fe-Alloy + WC-12% Co, Surf. Coat. Technol., 2014, 248, p 104-11210.1016/j.surfcoat.2014.03.037 ↗
24. A.P. Wang, T. Zhang, and J.Q. Wang, Formation and Properties of Ni-Based Amorphous Metallic Coating Produced by HVAF Thermal Spraying, Mater. Trans., 2005, 46(5), p 1010-101510.2320/matertrans.46.1010 ↗
25. A. Verstak and V. Baranovski, Activated Combustion HVAF Coatings for Protection against Wear and High Temperature Corrosion, Therm. Spray 2003 Adv. Sci. Appl. Technol., 2003, p 535-54110.31399/asm.cp.itsc2003p0535 ↗
26. E. Sadeghimeresht, N. Markocsan, P. Nylén, and S. Björklund, Corrosion Performance of Bi-Layer Ni/Cr2C3-NiCr HVAF Thermal Spray Coating, Appl. Surf. Sci., 2016, 369, p 470-48110.1016/j.apsusc.2016.02.002 ↗
27. A. Verstak, High Velocity Air-Fuel Spraying and Its Applications in Oil and Gas Industry, California, 2012.10.31399/asm.cp.itsc2012p0529 ↗
28. C. Lyphout et al., Tribological Properties of Hard Metal Coatings Sprayed by High-Velocity Air Fuel Process, J. Therm. Spray Technol., 2016, 25(1-2), p 331-34510.1007/s11666-015-0285-4 ↗
29. A. Milanti, V. Matikainen, H. Koivuluoto, G. Bolelli, L. Lusvarghi, and P. Vuoristo, Effect of Spraying Parameters on the Microstructural and Corrosion Properties of HVAF-Sprayed Fe-Cr-Ni-B-C Coatings, Surf. Coat. Technol., 2015, 277, p 81-9010.1016/j.surfcoat.2015.07.018 ↗
30. E. Sadeghimeresht, H. Hooshyar, N. Markocsan, S. Joshi, and P. Nylén, Oxidation Behavior of HVAF-Sprayed NiCoCrAlY Coating in H2–H2O Environment, Oxid. Met., 2016, 86(3-4), p 299-31410.1007/s11085-016-9637-9 ↗
31. G. Wang, Z. Huang, P. Xiao, and X. Zhu, Spraying of Fe-Based Amorphous Coating with High Corrosion Resistance by HVAF, J. Manuf. Process., 2016, 22, p 34-3810.1016/j.jmapro.2016.01.009 ↗
32. E. Sadeghimeresht, N. Markocsan, M. Huhtakangas, and S. Joshi, Isothermal Oxidation of HVAF-Sprayed Ni-Based Chromia, Alumina and Mixed-Oxide Scale Forming Coatings in Ambient Air, Surf. Coat. Technol., 2017, 316, p 10-2110.1016/j.surfcoat.2017.03.017 ↗
33. R. Bender and M. Schütze, The Role of Alloying Elements in Commercial Alloys for Corrosion Resistance in Oxidizing–Chloridizing Atmospheres. Part II: Experimental Investigations, Mater. Corros., 2003, 54(9), p 652-68610.1002/maco.200303673 ↗
34. N. Bala, H. Singh, S. Prakash, and J. Karthikeyan, Investigations on the Behavior of HVOF and Cold Sprayed Ni-20Cr Coating on T22 Boiler Steel in Actual Boiler Environment, J. Therm. Spray Technol., 2012, 21(1), p 144-15810.1007/s11666-011-9698-x ↗
35. M.H. Enayati, F. Karimzadeh, M. Tavoosi, B. Movahedi, and A. Tahvilian, Nanocrystalline NiAl Coating Prepared by HVOF Thermal Spraying, J. Therm. Spray Technol., 2011, 20(3), p 440-44610.1007/s11666-010-9588-7 ↗
36. Y.S. Li, Y. Niu, and M. Spiegel, High Temperature Interaction of Al/Si-Modified Fe-Cr Alloys with KCl, Corros. Sci., 2007, 49(4), p 1799-181510.1016/j.corsci.2006.10.019 ↗
37. K.N. Strafford, P.K. Datta, and G. Forster, High-Temperature Chloridation of Binary FeCr Alloys at 1000 °C, Mater. Sci. Eng. A, 1989, 120-121(PART 1), p 61-6810.1016/0921-5093(89)90719-3 ↗
38. T.S. Sidhu, A. Malik, S. Prakash, and R.D. Agrawal, Cyclic Oxidation Behavior of Ni- and Fe-Based Superalloys in Air and Na 2 SO 4-25% NaCl Molten Salt Environment at 800 °C, Int. J. Phys. Sci., 2006, 1(September), p 27-33
39. T. Jonsson, A. Slomian, T.N. Lomholt, S. Kiamehr, and K.V. Dahl, Microstructural Investigations of Pure Nickel Exposed to KCl Induced High Temperature Corrosion, Mater. High Temp., 2015, 32(1-2), p 44-4910.1179/0960340914Z.00000000060 ↗
40. T.J. Pan, Y.S. Li, Q. Yang, R.F. Feng, and A. Hirose, Internal Oxidation and Phase Transformations of Multi-phase Fe-Ni-Al and Fe-Ni-Al-Cr Alloys Induced by KCl Corrosion, Corros. Sci., 2011, 53(6), p 2115-212110.1016/j.corsci.2011.02.034 ↗
41. Y.S. Li and M. Spiegel, Models Describing the Degradation of FeAl and NiAl Alloys Induced by ZnCl2KCl Melt at 400-450 °C, Corros. Sci., 2004, 46(8), p 2009-202310.1016/j.corsci.2003.10.019 ↗
42. C.J. Wang and C.C. Li, Corrosion Behaviors of AISI, 1025 Steels with Electroless Nickel/Aluminized Coatings in NaCl-Induced Hot Corrosion, Surf. Coat. Technol., 2004, 177-178, p 37-4310.1016/j.surfcoat.2003.06.004 ↗
43. F.H. Yuan, Z.X. Chen, Z.W. Huang, Z.G. Wang, and S.J. Zhu, Oxidation Behavior of Thermal Barrier Coatings with HVOF and Detonation-Sprayed NiCrAlY Bondcoats, Corros. Sci., 2008, 50(6), p 1608-161710.1016/j.corsci.2008.02.002 ↗
44. B. Wang, J. Gong, A.Y. Wang, C. Sun, R.F. Huang, and L.S. Wen, Oxidation Behaviour of NiCrAlY Coatings on Ni-Based Superalloy, Surf. Coat. Technol., 2002, 149(1), p 70-7510.1016/S0257-8972(01)01427-X ↗