Abstract

Abstract Lowering the thermal energy and increasing the kinetic energy of sprayed particles by newly developed HVAF systems can significantly reduce material decarburization, and increases sliding wear and corrosion resistance of hard metal coatings, making HVAF coatings attractive both economically and environmentally over its HVOFs predecessors. Two agglomerated and sintered feedstock powder chemistries, respectively WC-Co (88/12) and WC-CoCr (86/10/4), with increasing primary carbides grain size from 0.2 to 4.0 microns, have been deposited by the latest HVAF-M3 process onto carbon steel substrates. Respective dry sliding wear behaviours and friction coefficients were evaluated at room temperature via Ball-on-disk (ASTM G99-90) wear tests against Al2O3 counterparts, and via Pin-on-disk (ASTM G77-05) wear tests against modified martensitic steel counterparts in both dry and lubricated conditions. Sliding wear mechanisms, with formation of wavy surface morphology and brittle cracking, are discussed regarding the distribution and size of primary carbides. Corrosion behaviours were evaluated via standard Neutral Salt Spray (NSS), Acetic Acid Salt Spray (AASS), accelerated corrosion test and electrochemical polarization test at room temperature. Optimization of coating tribological properties are discussed regarding the suitable selection of primary carbide size for different working load applications.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · High-Temperature Coating Behaviors · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. M. Bielewski, Replacing Cadmium and Chromium, Research and Technology Organization and NATO, RTO-AG-AVT-140, 2011, Chp.23, pp. 1-22
2. L.-M. Berger, P. Vuoristo, T. Mäntylä, W. Kunert, W. Lengauer, and P. Ettmayer, Practical Solutions to Engineering Problems, C.C. Berndt, Ed., ASM International, Materials Park, OH, 1996, p 97-106
3. G. Bolelli, R. Giovanardi, L. Lusvarghi, and T. Manfredini, Corrosion Resistance of HVOF-Sprayed Coatings for Hard Chrome Replacement, Corros. Sci., 2006, 48, p 3375-339710.1016/j.corsci.2006.03.001 ↗
4. A. Wank, B. Wielage, H. Pokhmurska, E. Friesen, and G. Reisel, Comparison of Hardmetal and Hard Chromium Coatings Under Different Tribological Conditions, Surf. Coat. Technol., 2006, 201, p 1975-198010.1016/j.surfcoat.2006.04.058 ↗
5. G. Bolelli, L.M. Berger, M. Bonetti, and L. Lusvarghi, Comparative Study of the Dry Sliding Wear Behaviour of HVOF-Sprayed WC-(W, Cr)2C-Ni and WC-CoCr Hardmetal Coatings, Wear, 2014, 309, p 96-11110.1016/j.wear.2013.11.001 ↗
6. G. Bolelli, L.-M. Berger, T. Börner, H. Koivuluoto, L. Lusvarghi, C. Lyphout, N. Markocsan, V. Matikainen, P. Nylén, P. Sassatelli, R. Trache, and P. Vuoristo, Tribology of HVOF- and HVAF-Sprayed WC-CoCr Hardmetal Coatings: A Comparative Assessment, Surf. Coat. Technol., 2015, 265, p 125-14410.1016/j.surfcoat.2015.01.048 ↗
7. Q. Wang, S. Zhang, Y. Cheng, J. Xiang, X. Zhao, and G. Yang, Wear and Corrosion Performances of WC-10Co4Cr Coatings Deposited by Different HVOF and HVAF Spraying Processes, Surf. Coat. Technol., 2013, 218, p 127-13610.1016/j.surfcoat.2012.12.041 ↗
8. M. Barletta, G. Bolelli, B. Bonferroni, and L. Lusvarghi, Wear and Corrosion Behaviour of HVOF-Sprayed WC-CoCr Coatings on Al Alloys, J. Therm. Spray Technol., 2010, 19(1-2), p 358-36710.1007/s11666-009-9387-1 ↗
9. ASTM G99-05, Standard Test Method for Wear Testing with a Pin-on-Disk Apparatus, ASTM International, West Conshohocken, PA, 2010. www.astm.org
10. ASTM G77-, Standard Test Method for Wear Testing with a Ball-on-Disk Apparatus, ASTM International
11. S. Luyckx and A. Love, The Dependence of the Contiguity of WC on Co Content and Its Independence from WC Grain Size in WC-Co Alloys, Int. J. Refract. Metals Hard Mat., 2005, V24, p 75-79
12. C. Lyphout, J. Kitamura, K. Sato, J. Yamada, and S. Dizdar, Tungsten Carbide Deposition Processes for Hard Chrome Alternative: Preliminary Study of HVAF vs. HVOF Thermal Spray Processes, Proceedings ITSC 2013, Busan, South Korea, 201310.31399/asm.cp.itsc2013p0506 ↗
13. C. Lyphout, S. Björklund, M. Karlsson, M. Runte, G. Reisel, and P. Boccaccio, Screening Design of Supersonic Air Fuel Processing for hard Metal Coatings, J. Therm. Spray Technol., 2014, 23(8), p 1323-133210.1007/s11666-014-0139-5 ↗
14. C. Lyphout and K. Sato, Screening Design of Hard Metal Feedstock Powders for Supersonic Air Fuel Processing, Surf. Coat. Technol., 2014, 258(2014), p 447-45710.1016/j.surfcoat.2014.08.055 ↗
15. J.C.P. Zuñega, M.G. Gee, R.J.K. Wood, and J. Walker, Scratch Testing of WC/Co Hardmetals, Tribol. Int., 2012, 54, p 77-8610.1016/j.triboint.2012.02.027 ↗
16. G. Bolelli, A. Candeli, H. Koivuluoto, L. Lusvarghi, T. Manfredini, and P. Vuoristo, Microstructure-Based Thermo-Mechanical Modelling of Thermal Spray Coatings, J. Therm. Spray Technol., 2015, 73(15), p 20-34
17. W.A. Glaeser, Wear Debris Classification, Modern Tribology Handbook—Volume One—Macrotribology, B. Bhushan, F.E. Kennedy, and A.Z. Szeri, Ed., CRC Press, Boca Raton, Florida (USA), 2001, p 301-315
18. J.V. Gabrusenoks, P.D. Cikmach, A.R. Lusis, J.J. Kepleris, and G.M. Ramans, Electrochromic Colour Centres in Amorphous Tungsten Trioxide Thin Films, Solid State Ionics, 1984, 14, p 25-3010.1016/0167-2738(84)90006-7 ↗
19. M.F. Daniel, B. Desbat, J.C. Lassegues, B. Gerand, and M. Figlarz, Infrared and Raman Study of WO3 Tungsten Trioxides and WO3 xH2O Tungsten Trioxide Hydrates, J. Solid State Chem., 1987, 67, p 235-24710.1016/0022-4596(87)90359-8 ↗
20. S. Usmani, S. Sampath, D.L. Houck, and D. Lee, Effect of Carbide Grain Size on the Sliding and Abrasive Wear Behavior of Thermally Sprayed WC-Co Coatings, Tribol. Trans., 1997, 40(3), p 470-47810.1080/10402009708983682 ↗
21. T. Sudaprasert, P.H. Shipway, and D.G. McCartney, Sliding Wear Behaviour of HVOF Sprayed WC-Co Coatings Deposited With Both Gas-Fuelled and Liquid-Fuelled Systems, Wear, 2003, 255, p 943-94910.1016/S0043-1648(03)00293-X ↗
22. Q. Yang, T. Senda, and A. Ohmori, Effect of Carbide Grain Size on Microstructure and Sliding Wear Behavior of HVOF Sprayed WC-12% Co Coatings, Wear, 2003, 254(1-2), p 23-3410.1016/S0043-1648(02)00294-6 ↗
23. Q. Yang, T. Senda, and A. Hirose, Sliding Wear Behavior of WC-12% Co Coatings at Elevated Temperatures, Surf. Coat. Technol., 2006, 200(14-15), p 4208-421210.1016/j.surfcoat.2004.12.032 ↗
24. C. Verdon, A. Karimi, and J.-L. Martin, A Study of High Velocity Oxy-Fuel Thermally Sprayed Tungsten Carbide Based Coatings. Part 1: Microstructures, Mater. Sci. Eng. A, 1998, 246(1-2), p 11-2410.1016/S0921-5093(97)00759-4 ↗
25. L.-M. Berger, R. Puschmann, J. Spatzier, and S. Matthews, Potential of HVAF Spray Process, Therm. Spray Bull., 2013, 6(1), p 16-20
26. G.W. Stachowiak and A.W. Batchelor, Engineering Tribology, 2nd ed., Butterworth-Heinemann, Woburn, MA, 2001, p 483-531
27. I. Konyashin, Cemented Carbides for Mining, Construction and Wear Parts, Comprehensive Hard Materials—Volume I: Hardmetals, V.K. Sarin, D. Mari, L. Llanes, and C.E. Nebel, Ed., Elsevier, Amsterdam, The Netherlands, 2014, p 425-45110.1016/B978-0-08-096527-7.00015-5 ↗
28. G.W. Stachowiak and A.W. Batchelor, Engineering Tribology, 2nd ed., Butterworth-Heinemann, Woburn, MA, USA, 2001, p 560-569
29. J.R. Davis, Ed., ASM Specialty Handbook: Nickel, Cobalt, and Their Alloys, ASM International, Materials Park, OH, USA, 2000, p 382-383
30. A.S. Kurlov and A.I. Gusev, Tungsten Carbides—Structure, Properties and Application in Hardmetals, Springer Series in Materials Science, Vol 184, R. Hull, C. Jagadish, R.M. Osgood, J. Parisi, and Z.M. Wang, Ed., Springer, Cham, 2013, p 34-36
31. A.M. Human and H.E. Exner, The Relationship Between Electrochemical Behaviour and In-service Corrosion of WC Based Cemented Carbides, Int. J. Refract. Met. Hard Mater., 1997, 15, p 65-7110.1016/S0263-4368(96)00014-5 ↗
32. A.M. Human and H.E. Exner, Electrochemical Behaviour of Tungsten-Carbide Hardmetals, Mater. Sci. Eng. A, 1996, 209, p 180-19110.1016/0921-5093(95)10137-3 ↗