Ablative Property and Mechanism of ZrC-TaC/ZrC-SiC Coatings on C/C Composites under Different Heat Fluxes
Source abstract
Abstract
In high-temperature aerobic environment, carbon materials have to be protected to delay the oxidation process. In this work, ZrC-TaC coatings were deposited by supersonic atmospheric plasma spraying on ZrC-SiC-coated C/C composites and ablation tests were conducted by oxyacetylene torch under different heat fluxes. When subjected to 4.2 WM/m2 for 20 s, the mass and linear ablation rates of the ZrC-TaC/ZrC-SiC coating system were 0.0076 g/s and 0.0005 mm/s, respectively. In the ablation process, the infiltration of the oxygen and liquid Ta2O5 into the inner layer resulted in significant oxidation of the ZrC-SiC inner layer. Due to the oxidation and microstructure evolution of the ZrC-TaC and ZrC-SiC layers, the porous Zr-Ta-O oxide layer, oxidized ZrC-TaC, and ZrC-SiC layers formed a better chemical combination and showed higher resistance to ablation. However, for a heat flux of 3.2 WM/m2, the molten Zr-Ta-O oxides that have good self-healing ability, were mainly formed on the ablative surface; liquid Ta2O5 together with trace oxygen could penetrate into the inner layers, resulting in the lack of chemical combination between the layers. As a result, the molten oxides were easy to denudate during the ablation and cooling process and showed lower resistance to ablation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · High-Temperature Coating Behaviors · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. H.M. Gajiwala, U.K. Vaidya, S.A. Sodah and S. Jeelani, Hybridized Resin Matrix Approach Applied for Development of Carbon/Carbon Composites-I, Carbon, 1998, 36, p 903–912.10.1016/S0008-6223(97)00204-2 ↗
2. X. Yang, Q. Huang, Z. Su et al., A Double Layer Nanostructure SiC Coating for Anti-Oxidation Protection of Carbon/Carbon Composites Prepared by Chemical Vapor Reaction and Chemical Vapor Deposition, Ceram. Int., 2013, 39, p 5053–5062.10.1016/j.ceramint.2012.11.104 ↗
3. C. Fang, X. Yang, K. He et al., Microstructure and Ablation Properties of La2O3 Modified C/C-SiC Composites Prepared Via Precursor Infiltration Pyrolysis, J. Eur. Ceram. Soc., 2019, 39, p 762–772.10.1016/j.jeurceramsoc.2018.11.041 ↗
4. VZh. Shemet, A.P. Pomytkin and V.S. Neshpor, High-Temperature Oxidation Behavior of Carbon Materials in Air, Carbon, 1993, 31, p 1–6.10.1016/0008-6223(93)90148-4 ↗
5. Y. Zhang, H. Wang, T. Li et al., Ultra-High Temperature Ceramic Coating for Carbon/Carbon Composites Against Ablation above 2000 K, Ceram. Int., 2018, 44, p 3056–3063.10.1016/j.ceramint.2017.11.066 ↗
6. F. Smeacetto, M. Salvo and M. Ferraris, Oxidation Protective Multilayer Coatings for Carbon-Carbon Composites, Carbon, 2002, 40, p 583–587.10.1016/S0008-6223(01)00151-8 ↗
7. D. Huang, M. Zhang, Q. Huang et al., Preparation of a Double Layer SiC Coating and its Oxidation Resistance at 1773 K, Corros. Sci., 2014, 87, p 134–140.10.1016/j.corsci.2014.06.024 ↗
8. X. Yang, Q. Huang, Z. Su et al., Resistance to Oxidation and Ablation of SiC Coating on Graphite Prepared by Chemical Vapor Reaction, Corros. Sci., 2013, 75, p 16–27.10.1016/j.corsci.2013.05.009 ↗
9. Y. Chu, H. Li, Q. Fu et al., Oxidation Protection of C/C Composites with a Multilayer Coating of SiC and Si + SiC + SiC Nanowires, Carbon, 2012, 50, p 1280–1288.10.1016/j.carbon.2011.10.048 ↗
10. Y. Liu, J. Wan, X. Zuo et al., Oxidation Behavior of 2D C/SiC Composites Coated with Multi-Layer SiC/Si-B-C/SiC Coatings under Wet Oxygen Atmosphere, Appl. Surf. Sci., 2015, 353, p 214–223.10.1016/j.apsusc.2015.06.153 ↗
11. C. Hu, X.L. Ge, Y.R. Niu et al., Influence of Oxidation Behavior of Feedstock on Microstructure and Ablation Resistance of Plasma-Sprayed Zirconium Carbide, J. Therm. Spray Technol., 2015, 24, p 1302–1311.10.1007/s11666-015-0307-2 ↗
12. K. Wang, L. Cao, J. Huang and J. Fei, A Mullite/SiC Oxidation Protective Coating for Carbon/Carbon Composites, J. Eur. Ceram. Soc., 2013, 33, p 191–198.10.1016/j.jeurceramsoc.2012.08.009 ↗
13. Q. Fu, H. Li, X. Shi et al., Silicon Carbide Coating to Protect Carbon/Carbon Composites Against Oxidation, Scripta. Mater., 2005, 52, p 923–927.10.1016/j.scriptamat.2004.12.029 ↗
14. X. Yang, Y. Zou, Q. Huang et al., Influence of Preparation Technology on the Structure and Phase Composition of MoSi2-Mo5Si3/SiC Multi-Coating for Carbon/Carbon Composites, J. Mate. Sci. Technol., 2010, 26, p 106–112.10.1016/S1005-0302(10)60017-5 ↗
15. Z. Yan, X. Xiong, P. Xiao et al., A Multilayer Coating of Dense SiC Alternated with Porous Si-Mo for the Oxidation Protection of Carbon/Carbon Silicon Carbide Composites, Carbon, 2008, 46, p 149–153.10.1016/j.carbon.2008.01.027 ↗
16. L. Cheng, Y. Xu, L. Zhang and X. Yin, Preparation of an Oxidation Protection Coating for C/C Composites by Low Pressure Chemical Vapor Deposition, Carbon, 2000, 38, p 1493–1498.10.1016/S0008-6223(00)00086-5 ↗
17. X. Jin, X. Fan, C. Lu and T. Wang, Advances in Oxidation and Ablation Resistance of High and Ultra-High Temperature Ceramics Modified or Coated Carbon/Carbon Composites, J. Eur. Ceram. Soc., 2018, 38, p 1–28.10.1016/j.jeurceramsoc.2017.08.013 ↗
18. Y.R. Niu, H.Y. Wang, L.P. Huang et al., Oxidation and Ablation Resistance of Low Pressure Plasma-Sprayed ZrB2-Si Composite Coating, J. Therm. Spray Technol., 2014, 23, p 470–476.10.1007/s11666-013-0020-y ↗
19. Y. Zeng, D. Wang, X. Xiong et al., Ultra-High-Temperature Ablation Behavior of SiC-ZrC-TiC Modified Carbon/Carbon Composites Fabricated Via Reactive Melt Infiltration, J. Eur. Ceram. Soc., 2020, 40, p 651–659.10.1016/j.jeurceramsoc.2019.10.027 ↗
20. G. Li, M. Wu, X. Xiong et al., Preparation and Ablation Properties of ZrC-TaC Co-Deposition Coating for Carbon-Carbon Composites, Ceram. Trans., 2014, 248, p 569–578.10.1002/9781118932995.ch65 ↗
21. X. Ren, H. Li, Q. Fu et al., TaB2-SiC-Si Multiphase Oxidation Protective Coating for SiC-Coated Carbon/Carbon Composites, J. Eur. Ceram. Soc., 2013, 33, p 2953–2959.10.1016/j.jeurceramsoc.2013.06.028 ↗
22. G. Feng, H. Li, X. Yao et al., Ablation Resistance of TaC-Modified HfC Coating Prepared by Supersonic Plasma Spraying for SiC-Coated Carbon/Carbon Composites, Ceram. Int., 2019, 45, p 17936–17945.10.1016/j.ceramint.2019.06.011 ↗
23. Y. Yang, K. Li, Z. Zhao and G. Liu, HfC-ZrC-SiC Multiphase Protective Coating for SiC-Coated C/C Composites Prepared by Supersonic Atmospheric Plasma Spraying, Ceram. Int., 2017, 43, p 1495–1503.10.1016/j.ceramint.2016.10.120 ↗
24. J. Ren, Y. Zhang, Y. Fu et al., Effects of the Second Phase on the Microstructure and Ablation Resistance of HfC Coating on C/C Composites, Surf. Coat. Technol., 2018, 344, p 250–258.10.1016/j.surfcoat.2018.03.023 ↗
25. X. Xiong, Y. Wang, G. Li et al., HfC/ZrC Ablation Protective Coating for Carbon/Carbon Composites, Corros. Sci., 2013, 77, p 25–30.10.1016/j.corsci.2013.06.042 ↗
26. Y. Yang, K. Li, G. Liu and Z. Zhao, Ablation-Resistant Composite Coating of HfC-TaC-SiC for C/C Composites Deposited by Supersonic Atmospheric Plasma Spraying, J. Ceram. Sci. Technol., 2016, 7, p 379–385.
27. J. Ren, E. Feng, Y. Zhang et al., Microstructure and Anti-Ablation Performance of HfC-TaC and HfC-ZrC Coatings Synthesized by CVD on C/C Composites, Ceram. Int., 2020, 46, p 10147–10158.10.1016/j.ceramint.2020.01.006 ↗
28. T. Liu, Y. Niu, C. Li et al., Ablation Resistance of ZrC-MoSi2/ZrC-SiC Double-Layered Coating in a Plasma Flame, Corros. Sci., 2018, 145, p 239–248.10.1016/j.corsci.2018.10.006 ↗
29. Y. Xu, W. Sun, X. Xiong et al., Ablation Characteristics of Mosaic Structure ZrC-SiC Coatings on Low-Density, Porous C/C Composites, J. Mater. Sci. Technol., 2019, 35, p 2785–2798.10.1016/j.jmst.2019.08.004 ↗
30. A. Shi, X. Yang, C. Fang et al., Effect of CNTs Addition on Microstructure, Ablation Property and Mechanism of ZrC-SiC Coating for C/C-ZrC-SiC Composites, Vacuum, 2020, 172, p 109099.10.1016/j.vacuum.2019.109099 ↗
31. Measurement Standard of Ablation Properties of Materials, GJB323A-96, National Standard Committee of China, Beijing, 1996.
32. X. Yang, Z. Su, Q. Huang et al., Microstructure and Mechanical Properties of C/C-ZrC-SiC Composites Fabricated by Reactive Melt Infiltration with Zr, Si Mixed Powders, J. Mate. Sci. Technol., 2013, 29, p 702–710.10.1016/j.jmst.2013.05.005 ↗
33. S. Tang and C. Hu, Design, Preparation and Properties of Carbon Fiber Reinforced Ultra-High Temperature Ceramic Composites for Aerospace Applications: A Review, J. Mate. Sci. Technol., 2017, 33, p 117–130.10.1016/j.jmst.2016.08.004 ↗
34. X. Pan, Y. Niu, X. Xu et al., Long Time Ablation Behaviors of Designed ZrC-SiC-TiC Ternary Coatings for Environments Above 2000 °C, Corros. Sci., 2020, 170, p 108654.10.1016/j.corsci.2020.108654 ↗