journal article·2019-10

Characterization and Accelerated Erosion Testing of WC-Co-Cr- and CoNiCrAlY-Coated CA6NM Turbine Steel

Deepak Kumar Goyal, Harpreet Singh, Harmesh Kumar

Publisher page

Abstract

In the present study, in-depth characterization of the high-velocity oxy-fuel (HVOF)-spray WC-Co-Cr and CoNiCrAlY coatings deposited on CA6NM turbine steel was done using scanning electron microscope (SEM), x-ray diffraction (XRD), roughness tester, microhardness tester, and optical image analyzer. Further, these coatings were tested under accelerated slurry erosion conditions using a high-speed erosion test rig. The effects of three different parameters related to actual operating conditions, namely erodent velocity relative to target surface, average erodent particle size, and slurry concentration on erosion behavior of these coatings, were investigated. SEM images on the specimen surface taken before and after erosion tests were carefully examined to understand the possible erosion mechanism. The study revealed that HVOF-sprayed WC-Co-Cr coating was found to impart higher erosion resistance in comparison with CoNiCrAlY coating under all the slurry erosion conditions. The reason for this behavior may be attributed to the higher hardness of HVOF-sprayed WC-10Co-4Cr coating in comparison with CoNiCrAlY coating.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Erosion and Abrasive Machining · High-Temperature Coating Behaviors · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. B.S.K. Naidu, Developing Silt Consciousness in the Minds of Hydropower Engineers, in Proceedings of 1st International Conference on Silting Problems in Hydropower Plants, CBIP, 13–15 Oct. 1999 (New Delhi), p 1–36
2. D.P. Sharma and S. Singh, Operational Problems of Water Turbine in U.P.—With Special Reference to Tiloth Power Station, in Proceedings of All India Seminar on Metallurgical Problems in Power Projects, 30–31 Oct. 1987 (Lucknow), p 18–35
3. B. Bhushan and B.K. Gupta, Handbook of Tribology: Materials, Coatings, and Surface Treatment, McGraw Hill, New York, 1997, p 629
4. J.H. Gummer, Combating Silt Erosion in Hydraulic Turbines, Hydro Rev. Wordwide, 2009, 17, p 28-34
5. F.J. Hermanek, Thermal Spray Terminology and Company Origins, ASM International, Materials Park, OH, USA, 2001
6. L. Gil and M.H. Staia, Microstructure and Properties of HVOF Thermal Sprayed NiWCrBSi Coatings, Surf. Coat. Technol., 1999, 120–121, p 423-42910.1016/S0257-8972(99)00494-6 ↗
7. J. Postlethwaite and S. Nesic, Erosion in Disturbed Liquid/Particle Pipe Flow: Effects of Flow Geometry and Particle Surface Roughness, Corrosion, 1993, 49(10), p 850-85710.5006/1.3316009 ↗
8. M.M. Salama, An Alternative to API, 14E Erosional Velocity Limits for Sand Laden Fluids, J. Energy Resour. Technol., 2000, 122(2), p 71-7710.1115/1.483167 ↗
9. T. Manisekaran, M. Kamaraj, S.M. Sharrif, and S.V. Joshi, Slurry Erosion Studies on Surface Modified 13Cr-4Ni Steels: Effect of Angle of Impingement and Particle Size, J. Mater. Eng. Perform., 2007, 16(5), p 567-57210.1007/s11665-007-9068-5 ↗
10. R. Gupta, S.N. Singh, and V. Sehadri, Prediction of Uneven Wear in a Slurry Pipeline on the Basis of Measurements in a Pot Tester, Wear, 1995, 184(2), p 169-17810.1016/0043-1648(94)06566-7 ↗
11. D.A. Stewart, P.H. Shipway, and D.G. McCartney, Microstructural Evolution in Thermally Sprayed WC-Co Coatings: Comparison Between Nanocomposite and Conventional Starting Powders, Acta Mater., 2000, 48, p 1593-160410.1016/S1359-6454(99)00440-1 ↗
12. T. Sudaprasert, P.H. Shipway, and D.G. McCartney, Sliding Wear Behaviour of HVOF Sprayed WC-Co Coatings Deposited with Both Gas-Fuelled and Liquid-Fuelled Systems, Wear, 2003, 255, p 943-94910.1016/S0043-1648(03)00293-X ↗
13. S.B. Mishra, K. Chandra, and S. Prakash, Erosion-Corrosion Performance of NiCrAlY Coating Produced by Plasma Spray Process in a Coal-Fired Thermal Power Plant, Surf. Coat. Technol., 2013, 216, p 23-3410.1016/j.surfcoat.2012.09.044 ↗
14. S.B. Mishra, K. Chandra, and S. Prakash, Characterisation and Erosion Behaviour of Plasma Sprayed NiCrAlY and Ni-20Cr Coatings on a Fe-Based Superalloy, J. Tribol., 2006, 128(3), p 469-47510.1115/1.2197843 ↗
15. E. Lugscheider, J. Zwick, M. Hertter, and D. Sporer, Control of Coating Properties of Abradable Seals by On-Line Process Diagnostics, in Proceedings of International Thermal Spray Conference, 2–4 May, 2005, Basel, Switzerland10.31399/asm.cp.itsc2005p0610 ↗
16. F.J. Belzunce, V. Higuera, and S. Poveda, High Temperature Oxidation of HFPD Thermal-Sprayed MCrAlY Coatings, Mater. Sci. Eng. A, 2001, 297(1–2), p 162-16710.1016/S0921-5093(00)01239-9 ↗
17. V. Higuera, F.J. Belzunce, and J. Riba, High Temperature Oxidation of Plasma and HVOF Thermal Sprayed CoNiCrAlY Coatings in Simulated Gas Turbine and Furnace Environments, Surf. Eng., 2009, 25, p 319-32510.1179/026708408X375271 ↗
18. D.K. Goyal, H. Singh, H. Kumar, and V. Sahni, Erosive Wear Study of HVOF Spray Cr3C2-NiCr Coated CA6NM Turbine Steel, Journal of Tribology, 2014, 136, p 041602-1-041602-11
19. D.K. Goyal, H. Singh, H. Kumar, and V. Sahni, Slurry Erosive Wear Evaluation of HVOF-Spray Cr2O3 Coating on Some Turbine Steels, J. Therm. Spray Technol., 2012, 21(5), p 838-85110.1007/s11666-012-9795-5 ↗
20. D.K. Goyal, H. Singh, H. Kumar, and V. Sahni, Slurry Erosion Behaviour of HVOF Sprayed WC–10Co–4Cr and Al2O3 +13TiO2 Coatings on a Turbine Steel, Wear, 2012, 289, p 46-5710.1016/j.wear.2012.04.016 ↗
21. B.K. Prasad, A.K. Jha, O.P. Modi, and A.H. Yegneswaran, Effect of Sand Concentration in the Medium and Travel Distance and Speed on the Slurry Wear Response of a Zinc-Based Alloy Alumina Particle Composite, Tribol. Lett., 2004, 17(2), p 301-30910.1023/B:TRIL.0000032468.27468.2c ↗
22. A.V. Levy and P. Chik, The Effects of Erodent Composition and Shape on the Erosion of Steel, Wear, 1983, 89(2), p 151-16210.1016/0043-1648(83)90240-5 ↗
23. M. Liebhard and A. Levy, The Effect of Erodent Particle Characteristics on the Erosion of Metals, Wear, 1991, 151(2), p 381-39010.1016/0043-1648(91)90263-T ↗
24. J. Subrahmanyam, M.P. Srivastava, and R. Sivakumar, Characterization of Plasma-Sprayed WC-Co Coatings, Mater. Sci. Eng., 1986, 84, p 209-21410.1016/0025-5416(86)90240-5 ↗
25. W. Coulson and S.J. Harris, The Microstructure of WC-Co Coatings Produced by HVOF Spraying with Liquid Fuel, Trans. Inst. Met. Finish., 1997, 75, p 108-11210.1080/00202967.1997.11871153 ↗
26. A. Kumar, A. Sharma, and S.K. Goel, Erosion Behaviour of WC-10Co-4Cr Coating on 23-8-N Nitronic Steel by HVOF Thermal Spraying, Appl. Surf. Sci., 2016, 370, p 418-42610.1016/j.apsusc.2016.02.163 ↗
27. D. Al-Anazi, M.S.J. Hashmi, and B.S. Yilbas, High-Velocity Oxy-Fuel Thermally Sprayed CoNiCrAlY Coatings on Ti-6Al-4V Alloy: High Cycle Fatigue Properties of Coating, J. Eng. Manuf., 2007, 221, p 647-65410.1243/09544054JEM772 ↗
28. D. Naumenko, V. Shemet, L. Singheiser, and W.J. Quadakkers, Failure Mechanisms of Thermal Barrier Coatings on MCrAlY-Type Bondcoats Associated with the Formation of the Thermally Grown Oxide, J. Mater. Sci., 2009, 44, p 1687-170310.1007/s10853-009-3284-3 ↗
29. T. Peat, A. Galloway, A. Toumpis, D. Harvey, and W.H. Yang, Performance Evaluation of HVOF Deposited Cermet Coatings Under Dry and Slurry Erosion, Surf. Coat. Technol., 2016, 300, p 118-12710.1016/j.surfcoat.2016.05.039 ↗
30. R.C. Tucker Jr., Ch. 11: Handbook of Deposition Technologies for Films & Coatings (1994), p 591
31. A. Elkholy, Prediction of Abrasion Wear for Slurry Pump Materials, Wear, 1983, 84, p 39-4910.1016/0043-1648(83)90117-5 ↗
32. A.V. Levy and G. Hickey, Liquid-Solid Particle Slurry Erosion of Steels, Wear, 1987, 117, p 129-14610.1016/0043-1648(87)90251-1 ↗
33. T. Alam, M.A. Islam, and Z.N. Farhat, Slurry Erosion of Pipeline Steel: Effect of Velocity and Microstructure, J. Tribol., 2016, 138(2), p 21604-2161410.1115/1.4031599 ↗
34. G.F. Truscott, A Literature Survey on Wear on Pipelines, BHRA Fluid Engineering, Cranfield Publ, Cranfield, UK, TN, 1975, p 1295
35. I. Finnie, Some Observations on the Erosion of Ductile Metals, Wear, 1972, 19, p 81-8910.1016/0043-1648(72)90444-9 ↗
36. H.M. Clark and K.K. Wong, Impact Angle, Particle Energy and Mass Loss in Erosion by Dilute Slurries, Wear, 1995, 186–187, p 454-46410.1016/0043-1648(95)07120-2 ↗
37. Z. Feng and A. Ball, The Erosion of Four Materials Using Seven Erodents—Towards an Understanding, Wear, 1999, 233–235, p 674-68410.1016/S0043-1648(99)00176-3 ↗
38. B.K. Gandhi, S.N. Singh, and V. Seshadri, Study of the Parametric Dependence of Erosion Wear for the Parallel Flow of Solid-Liquid Mixtures, Tribol. Int., 1999, 32, p 275-28210.1016/S0301-679X(99)00047-X ↗
39. B.K. Gandhi and S.V. Borse, Effects of Particle Size and Size Distribution on Estimating Erosion Wear of Cast Iron in Sand-Water Slurries, Indian J. Eng. Mater. Sci., 2002, 9, p 480-486
40. B.K. Gandhi and S.V. Borse, Nominal Particle Size of Multi-sized Particulate Slurries for Evaluation of Erosion Wear and Effect of Fine Particles, Wear, 2004, 257, p 73-7910.1016/j.wear.2003.10.013 ↗
41. I.M. Hutchings, A Model for the Erosion of Metals by Spherical Particles at Normal Incidence, Wear, 1981, 70, p 269-28110.1016/0043-1648(81)90347-1 ↗
42. M.K. Padhy and R.P. Saini, Effect of Size and Concentration of Silt Particles on the Erosion of Pelton Turbine Buckets, Energy, 2009, 34, p 1477-148310.1016/j.energy.2009.06.015 ↗
43. D.K. Goyal, H. Singh, and H. Kumar, An Overview of Slurry Erosion Control by the Application of High Velocity Oxy Fuel Sprayed Coatings, J. Eng. Tribol., 2011, 225, p 1092-1105
44. G.W. Stachowiak and A.W. Batchelor, Engineering Tribology, Elsevier, Amsterdam, New York, 1993, p 511
45. D.W. Wheeler and R.J.K. Wood, Erosion of Hard Surface Coatings for Use in Offshore Gate Valves, Wear, 2005, 258, p 526-53610.1016/j.wear.2004.03.035 ↗
46. D.J. O’Flynn, M.S. Bingley, M.S.A. Bradley, and A.J. Burnett, A Model to Predict the Solid Particle Erosion Rate of Metals and its Assessment Using Heat-Treated Steels, Wear, 2001, 248(1–2), p 162-17710.1016/S0043-1648(00)00554-8 ↗