journal article·2024-06

Trade-Off Among Cavitation Erosion Resistance, Corrosion Resistance, and Antifouling Properties of HVOF-Sprayed WC-CoCr Coating via Adding Stainless Steel and Copper

Zhe Guo, Xiaomei Liu, Ye Tian, Ping Zhou, Miao Yu, Jin Liu, Xu Yin, Rui Yang, Hua Li

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced materials and composites · High-Temperature Coating Behaviors · Erosion and Abrasive Machining

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. R. Pecha and B. Gompf, Microimplosions: Cavitation Collapse and Shock Wave Emission on a Nanosecond Time Scale, Phys. Rev. Lett., 2000, 84(6), p 1328-1330. https://doi.org/10.1103/PhysRevLett.84.132810.1103/PhysRevLett.84.1328 ↗
2. L. Ye, X. Zhu, Y. He, and X. Wei, Ultrasonic Cavitation Damage Characteristics of Materials and a Prediction Model of Cavitation Impact Load Based on Size Effect, Ultrason. Sonochem., 2020, 66, 105115. https://doi.org/10.1016/j.ultsonch.2020.10511510.1016/j.ultsonch.2020.105115 ↗
3. Z.B. Zheng, J. Long, S. Wang, H. Li, J. Wang, and K.H. Zheng, Cavitation Erosion-Corrosion Behaviour of Fe-10Cr Martensitic Steel Microalloyed with Zr in 3.5% NaCl Solution, Corros. Sci., 2021, 184, 109382. https://doi.org/10.1016/j.corsci.2021.10938210.1016/j.corsci.2021.109382 ↗
4. I. Richardson, Guide to Nickel Aluminium Bronze for Engineers, ed. by C. Powell, Copper Development Association, (2016)
5. K.S. Park and S. Kim, Corrosion and Corrosion Fatigue Characteristics of Cast NAB Coated with NAB by HVOF Thermal Spray, J. Electrochem. Soc., 2011, 158(10), p C335-C340. https://doi.org/10.1149/1.362234310.1149/1.3622343 ↗
6. L. Zhao, B. Du, J. Yao, H. Chen, R. Ding, and K. Li, Microstructure and Mechanical Properties of Nickel-Aluminum Bronze Coating on 17-4PH Stainless Steel by Laser Cladding, Chin. J. Mech. Eng., 2022, 35(6), p 140.10.1186/s10033-022-00807-z ↗
7. E. Feldshtein, O. Devojno, S. Wojciechowski, M. Kardapolava, I. Kasyakova, and A. Balduyeva, Tribologic Behavior and Surface Integrity of NAB Bronze Coatings Reinforced with WC and Cr3C2 Carbides Using Ytterbium Fiber Laser, Tribol. Int., 2023, 188, 108784. https://doi.org/10.1016/j.triboint.2023.10878410.1016/j.triboint.2023.108784 ↗
8. J. Basumatary, M. Nie, and R.J.K. Wood, The Synergistic Effects of Cavitation Erosion–Corrosion in Ship Propeller Materials, J. Bio- Tribo-Corros., 2015, 1, p 12. https://doi.org/10.1007/s40735-015-0012-110.1007/s40735-015-0012-1 ↗
9. J. Basumatary and R.J.K. Wood, Different Methods of Measuring Synergy Between Cavitation Erosion and Corrosion for Nickel Aluminium Bronze in 3.5% NaCl Solution, Tribol. Int., 2017, 147, 104843. https://doi.org/10.1016/j.triboint.2017.08.00610.1016/j.triboint.2017.08.006 ↗
10. J. Basumatary and R.J.K. Wood, Synergistic Effects of Cavitation Erosion and Corrosion for Nickel Aluminium Bronze with Oxide Film in 3.5% NaCl Solution, Wear, 2017, 376–377, p 1286-1297. https://doi.org/10.1016/j.wear.2017.01.04710.1016/j.wear.2017.01.047 ↗
11. Y. Tian, H. Zhao, R. Yang, H.J. Zhang, M. Yu, P. Zhou, H. Li, and X.Y. Chen, Behavior of the Hard Phases of Copper Alloys Subjected to Cavitation Erosion Investigated by SEM Observation, Tribol. Int., 2022, 174, 107771. https://doi.org/10.1016/j.triboint.2022.10777110.1016/j.triboint.2022.107771 ↗
12. H.B. Li, C.T. Yang, E.Z. Zhou, C.G. Yang, H. Feng, Z.H. Jiang, D.K. Xu, T.Y. Gu, and K. Yang, Microbiologically Influenced Corrosion Behavior of S32654 Super Austenitic Stainless Steel in the Presence of Marine Pseudomonas aeruginosa Biofilm, J. Mater. Sci. Technol., 2017, 33(12), p 1596-1603. https://doi.org/10.1016/j.jmst.2017.03.00210.1016/j.jmst.2017.03.002 ↗
13. D.K. Xu, J. Xia, E.Z. Zhou, D.W. Zhang, H.B. Li, C.G. Yang, Q. Li, H. Lin, X.G. Li, and K. Yang, Accelerated Corrosion of 2205 Duplex Stainless Steel Caused by Marine Aerobic Pseudomonas aeruginosa Biofilm, Bioelectrochemistry, 2017, 113, p 1-8. https://doi.org/10.1016/j.bioelechem.2016.08.00110.1016/j.bioelechem.2016.08.001 ↗
14. M. Moradi, Z.L. Song, L.J. Yang, J.J. Jiang, and J. He, Effect of Marine Pseudoalteromonas sp. on the Microstructure and Corrosion Behaviour of 2205 Duplex Stainless Steel, Corros. Sci., 2014, 84, p 103-112. https://doi.org/10.1016/j.corsci.2014.03.01810.1016/j.corsci.2014.03.018 ↗
15. L.Y. Huang, W.W. Chang, D.W. Zhang, Y. Huang, Z.Y. Li, Y.T. Lou, H.C. Qian, C.Y. Jiang, X.G. Li, and A. Mol, Acceleration of Corrosion of 304 Stainless Steel by Outward Extracellular Electron Transfer of Pseudomonas aeruginosa Biofilm, Corros. Sci., 2022, 199, 110159. https://doi.org/10.1016/j.corsci.2022.11015910.1016/j.corsci.2022.110159 ↗
16. M. Yu, H.J. Zhang, Y. Tian, R. Yang, H. Li, and X.Y. Chen, Role of Marine Bacillus subtilis and Pseudomonas aeruginosa in Cavitation Erosion Behaviour of 316L Stainless Steel, Wear, 2023, 514–515, 204593. https://doi.org/10.1016/j.wear.2022.20459310.1016/j.wear.2022.204593 ↗
17. K. Morshed-Behbahani, D.P. Bishop, and A. Nasiri, A Review of the Corrosion Behavior of Conventional and Additively Manufactured Nickel-Aluminum Bronze (NAB) Alloys: Current Status and Future Challenges, Mater. Horizons, 2023, 10, p 5391–5435. https://doi.org/10.1039/d3mh00951c10.1039/d3mh00951c ↗
18. T. Murray, S. Thomas, Y.X. Wu, W. Neil, and C. Hutchinson, Selective Laser Melting of Nickel Aluminium Bronze, Addit. Manuf., 2020, 33, 101122. https://doi.org/10.1016/j.addma.2020.10112210.1016/j.addma.2020.101122 ↗
19. G. Ghiara, R. Spotorno, S. Delsante, F. Formicola, A. Franzetti, and P. Cristiani, Opposite Corrosion Behaviour of Aluminum Bronze Induced by Pseudomonas fluorescens and Its Metabolites, Corros. Sci., 2022, 208, 110656. https://doi.org/10.1016/j.corsci.2022.11065610.1016/j.corsci.2022.110656 ↗
20. Y. Tian, H. Zhao, R. Yang, X. Liu, H. Li, and X. Chen, Effects of Bacillus sp. Adhesion on Cavitation Erosion Behaviour of Nickel Aluminium Bronze in Artificial Seawater, Wear, 2022, 498–499, 204344. https://doi.org/10.1016/j.wear.2022.20434410.1016/j.wear.2022.204344 ↗
21. Z. Song, S.W. Yang, P. Li, J.X. Sun, D.Y. Xing, W.C. Peng, and F.Y. Sun, Roles of Initial Bacterial Attachment and Growth in the Biofouling Development on the Microfiltration Membrane: From Viewpoints of Individual Cell and Interfacial Interaction Energy, J. Membr. Sci., 2021, 638, 119723. https://doi.org/10.1016/j.memsci.2021.11972310.1016/j.memsci.2021.119723 ↗
22. H.J. Kim, J.S. Park, T.K. Lee, D. Kang, J.H. Kang, K. Shin, and S.W. Jung, Dynamics of Marine Bacterial Biofouling Communities After Initial Alteromonas genovensis Biofilm Attachment to Anti-fouling Paint Substrates, Mar. Pollut. Bull., 2021, 172, 112895. https://doi.org/10.1016/j.marpolbul.2021.11289510.1016/j.marpolbul.2021.112895 ↗
23. S. Hong, Y. Wu, J. Zhang, Y. Zheng, Y. Qin, and J. Lin, Ultrasonic Cavitation Erosion of High-Velocity Oxygen-Fuel (HVOF) Sprayed Near-Nanostructured WC-10Co-4Cr Coating in NaCl Solution, Ultrason. Sonochem., 2015, 26, p 87–92. https://doi.org/10.1016/j.ultsonch.2015.01.01210.1016/j.ultsonch.2015.01.012 ↗
24. S. Hong, Y. Wu, J. Zhang, Y. Zheng, Y. Qin, and J. Lin, Effect of Ultrasonic Cavitation Erosion On Corrosion Behavior of High-Velocity Oxygen-Fuel (HVOF) Sprayed Near-Nanostructured WC-10Co-4Cr Coating, Ultrason. Sonochem., 2015, 27, p 374–378. https://doi.org/10.1016/j.ultsonch.2015.06.00610.1016/j.ultsonch.2015.06.006 ↗
25. Z. Ding, W. Chen, and Q. Wang, Resistance of Cavitation Erosion Of Multimodal WC-12Co Coatings Sprayed by HVOF, Trans. Nonferrous Met. Soc. China, 2011, 21(10), p 2231-2236. https://doi.org/10.1016/s1003-6326(11)61000-510.1016/s1003-6326(11)61000-5 ↗
26. X. Ding, X.D. Cheng, X. Yu, C. Li, C.Q. Yuan, and Z.X. Ding, Structure and Cavitation Erosion Behavior of HVOF Sprayed Multi-Dimensional WC-10Co4Cr Coating, Trans. Nonferrous Met. Soc. China, 2018, 28(3), p 487-494. https://doi.org/10.1016/s1003-6326(18)64681-310.1016/s1003-6326(18)64681-3 ↗
27. X. Ding, Y. Huang, C. Yuan, and Z. Ding, Deposition and Cavitation Erosion Behavior of Multimodal WC-10Co4Cr Coatings Sprayed by HVOF, Surf. Coat. Technol., 2020, 392, 125757. https://doi.org/10.1016/j.surfcoat.2020.12575710.1016/j.surfcoat.2020.125757 ↗
28. X. Ding, X.D. Cheng, C.Q. Yuan, J. Shi, and Z.X. Ding, Structure of Micro-Nano WC-10Co4Cr Coating and Cavitation Erosion Resistance in NaCl Solution, Chin. J. Mech. Eng., 2017, 30(5), p 1239-1247. https://doi.org/10.1007/s10033-017-0162-910.1007/s10033-017-0162-9 ↗
29. X. Ding, D. Ke, C.Q. Yuan, Z.X. Ding, and X.D. Cheng, Microstructure and Cavitation Erosion Resistance of HVOF Deposited WC-Co Coatings with Different Sized WC, Coatings, 2018, 8(9), p 307. https://doi.org/10.3390/coatings809030710.3390/coatings8090307 ↗
30. M.M. Lima, C. Godoy, P.J. Modenesi, J.C. Avelar-Batista, A. Davison, and A. Matthews, Coating Fracture Toughness Determined by Vickers Indentation: An Important Parameter in Cavitation Erosion Resistance of WC-Co Thermally Sprayed Coatings, Surf. Coat. Technol., 2004, 177–178, p 489–496. https://doi.org/10.1016/s0257-8972(03)00917-410.1016/s0257-8972(03)00917-4 ↗
31. M.S. Lamana, A.G.M. Pukasiewicz, and S. Sampath, Influence of Cobalt Content and HVOF Deposition Process on the Cavitation Erosion Resistance of WC-Co Coatings, Wear, 2018, 398–399, p 209–219. https://doi.org/10.1016/j.wear.2017.12.00910.1016/j.wear.2017.12.009 ↗
32. X. Liu, J. Kang, W. Yue, G. Ma, Z. Fu, L. Zhu, D. She, J. Liang, W. Weng, H. Wang, and C. Wang, Cavitation Erosion Behavior of HVOF Sprayed WC-10Co4Cr Cermet Coatings in Simulated Sea Water, Ocean Eng., 2019, 190, 106449. https://doi.org/10.1016/j.oceaneng.2019.10644910.1016/j.oceaneng.2019.106449 ↗
33. H.J. Zhang, Y.F. Gong, X.Y. Chen, A. McDonald, and H. Li, A comparative Study of Cavitation Erosion Resistance of Several HVOF-Sprayed Coatings in Deionized Water and Artificial Seawater, J. Therm. Spray Technol., 2019, 28(5), p 1060–1071. https://doi.org/10.1007/s11666-019-00869-x10.1007/s11666-019-00869-x ↗
34. J. Lin, S. Hong, Y. Zheng, W. Sun, M. Kang, and X. Fu, Cavitation Erosion Resistance in NaCl Medium of HVOF Sprayed WC-Based Cermet Coatings at Various Flow Velocities: A Comparative Study on the Effect of Ni and CoCr Binder Phases, Int. J. Refract. Met. Hard Mater., 2021, 94, 105407. https://doi.org/10.1016/j.ijrmhm.2020.10540710.1016/j.ijrmhm.2020.105407 ↗
35. R. Piola, A.S.M. Ang, M. Leigh, and S.A. Wade, A Comparison of the Antifouling Performance of Air Plasma Spray (APS) Ceramic and High Velocity Oxygen Fuel (HVOF) Coatings for Use in Marine Hydraulic Applications, Biofouling, 2018, 34(5), p 479–491. https://doi.org/10.1080/08927014.2018.146505210.1080/08927014.2018.1465052 ↗
36. A. Jasu and R.R. Ray, Biofilm Mediated Strategies to Mitigate Heavy Metal Pollution: A Critical Review in Metal Bioremediation, Biocatal. Agric. Biotechnol., 2021, 37, 102183. https://doi.org/10.1016/j.bcab.2021.10218310.1016/j.bcab.2021.102183 ↗
37. P.D. Rodrigues, R.G. Ferrari, L.S. Kato, R.A. Hauser-Davis, and C.A. Conte, A Systematic Review on Metal Dynamics and Marine Toxicity Risk Assessment Using Crustaceans as Bioindicators, Biol. Trace Elem. Res., 2022, 200(2), p 881–903. https://doi.org/10.1007/s12011-021-02685-310.1007/s12011-021-02685-3 ↗
38. D.H. Kim, A.B. Alayande, J.M. Lee, J.H. Jang, S.M. Jo, M.R. Jae, E.T. Yang, and K.J. Chae, Emerging Marine Environmental Pollution and Ecosystem Disturbance in Ship Hull Cleaning for Biofouling Removal, Sci. Total. Environ., 2024, 906, 167459. https://doi.org/10.1016/j.scitotenv.2023.16745910.1016/j.scitotenv.2023.167459 ↗
39. ASTM E2109-01, Standard Test Methods for Determining Area Percentage Porosity in Thermal Sprayed Coatings. American Society for Testing and Materials International 2021 (2021)
40. C.B. Ponton and R.D. Rawlings, Vickers Indentation Fracture Toughness Test Part 1 Review of Literature and Formulation of Standardised Indentation Toughness Equations, Mater. Sci. Technol., 1989, 5(9), p 865–872. https://doi.org/10.1179/mst.1989.5.9.86510.1179/mst.1989.5.9.865 ↗
41. A.G. Evans and T.R. Wilshaw, Quasi-Static Solid Particle Damage in Brittle Solids — I. Observations Analysis and Implications, Acta Metall., 1976, 24(10), p 939–956. https://doi.org/10.1016/0001-6160(76)90042-010.1016/0001-6160(76)90042-0 ↗
42. ASTM D1141-98, Standard Practice for the Preparation of Substitute Ocean Water. American Society for Testing and Materials International 2013 (2013)
43. ASTM B117-19, Standard Practice for Operating Salt Spray (fog) Apparatus. American Society for Testing and Materials International 2019 (2019)
44. ASTM G32-16(2021)e1, Standard Test Method for Cavitation Erosion Using Vibratory Apparatus. American Society for Testing and Materials International 2021 (2021)
45. J. Wang, R. Yang, Y. Tian, P. Zhou, J. Huang, H. Li, and X. Chen, Effect of Annealing on the Cavitation Erosion Resistance of HVOF-Sprayed Fe-Based Amorphous Composite Coatings, J. Therm. Spray Technol., 2023, 32(6), p 1758–1771. https://doi.org/10.1007/s11666-023-01606-110.1007/s11666-023-01606-1 ↗
46. M. de Nicolás-Morillas, L. Llanes, and E. Gordo, High-Temperature Wettability in Hard Materials: Comparison of Systems with Different Binder/Carbide Phases and Evaluation of C Addition, Int. J. Refract. Met. Hard Mater., 2023, 111, 106081. https://doi.org/10.1016/j.ijrmhm.2022.10608110.1016/j.ijrmhm.2022.106081 ↗
47. G.A. Yasinskaya, The Wetting of Refractory Carbides, Borides, and Nitrides by Molten Metals, Sov. Powder Metall. Met. Ceram., 1966, 5(7), p 557–559. https://doi.org/10.1007/BF0078011610.1007/BF00780116 ↗
48. Q.L. Lin, Z.B. Ma, and R. Sui, Wetting and Pressureless Infiltration Behavior of Cu/316L System at 1100°C, Surf. Interfaces, 2023, 42, 103462. https://doi.org/10.1016/j.surfin.2023.10346210.1016/j.surfin.2023.103462 ↗
49. Q.S. Liu, X.B. Liu, G. Wang, Y.F. Liu, Y. Meng, and S.H. Zhang, Effect of Cu Content on Microstructure Evolution and Tribological Behaviors of Ni60 Composite Coatings on 45# Steel by Laser Cladding, Opt. Laser Technol., 2022, 156, 108549. https://doi.org/10.1016/j.optlastec.2022.10854910.1016/j.optlastec.2022.108549 ↗
50. J. Yang, Z.B. Wang, Y.X. Qiao, and Y.G. Zheng, Synergistic Effects of Deposits and Sulfate Reducing Bacteria on the Corrosion of Carbon Steel, Corros. Sci., 2022, 199, 110210. https://doi.org/10.1016/j.corsci.2022.11021010.1016/j.corsci.2022.110210 ↗
51. H. Wang, J.H. Xu, X.S. Du, H.B. Wang, X. Cheng, and Z.L. Du, Stretchable and Self-Healing Polyurethane Coating with Synergistic Anticorrosion Effect for the Corrosion Protection of Stainless Steels, Prog. Org. Coat., 2022, 164, 106672. https://doi.org/10.1016/j.porgcoat.2021.10667210.1016/j.porgcoat.2021.106672 ↗
52. J.M. Perry, A. Neville, and T. Hodgkiess, A Comparison of the Corrosion Behavior of WC-Co-Cr and WC-Co HVOF Thermally Sprayed Coatings by In Situ Atomic Force Microscopy (AFM), J. Therm. Spray Technol., 2002, 11(4), p 536–541. https://doi.org/10.1361/10599630277034867310.1361/105996302770348673 ↗
53. G. Bolelli, R. Giovanardi, L. Lusvarghi, and T. Manfredini, Corrosion Resistance of HVOF-Sprayed Coatings for Hard Chrome Replacement, Corros. Sci., 2006, 48(11), p 3375–3397. https://doi.org/10.1016/j.corsci.2006.03.00110.1016/j.corsci.2006.03.001 ↗
54. J. Liu, T. Chen, C. Yuan, and X. Bai, Performance Analysis of Cavitation Erosion Resistance and Corrosion Behavior of HVOF-Sprayed WC-10Co-4Cr, WC-12Co, and Cr3C2-NiCr Coatings, J. Therm. Spray Technol., 2020, 29(4), p 798–810. https://doi.org/10.1007/s11666-020-00994-y10.1007/s11666-020-00994-y ↗
55. P. Dhaiveegan, N. Elangovan, T. Nishimura, and N. Rajendran, Corrosion Behavior of 316L and 304 Stainless Steels Exposed to Industrial-Marine-Urban Environment: Field Study, RSC Adv., 2016, 6(53), p 47314–47324. https://doi.org/10.1039/c6ra04015b10.1039/c6ra04015b ↗
56. Z.P. Wang, Y. Wang, B.W. Zhang, Z. Zhang, K. Xiao, J.S. Wu, Q. Yao, G.J. Ma, and G. Sun, Passivation Behavior of 316L Stainless Steel in Artificial Seawater: Effects of pH and Dissolved Oxygen, Anti-Corros. Methods Mater., 2021, 68(2), p 122–129. https://doi.org/10.1108/acmm-09-2020-236710.1108/acmm-09-2020-2367 ↗
57. M. Seo, G. Hultquist, C. Leygraf, and N. Sato, The Influence of Minor Alloying Elements (Nb, Ti and Cu) on the Corrosion Resistivity of Ferritic Stainless-Steel in Sulfuric-Acid-Solution, Corros. Sci., 1986, 26(11), p 949–955. https://doi.org/10.1016/0010-938x(86)90085-510.1016/0010-938x(86)90085-5 ↗
58. J.W. Wu, F.P. Wang, Y.X. Guo, X.J. Shang, J. Zhang, and Q.B. Liu, Cu Assisted Improvement of Wear and Corrosion Resistance in FeCoNiAl High-Entropy Intermetallic Coating by Laser Cladding, J. Mater. Res. Technol., 2023, 23, p 1105–1119. https://doi.org/10.1016/j.jmrt.2023.01.00310.1016/j.jmrt.2023.01.003 ↗
59. S. Hong, Y.P. Wu, J.F. Zhang, Y.G. Zheng, Y.J. Qin, W.W. Gao, and G.Y. Li, Cavitation Erosion Behavior and Mechanism of HVOF Sprayed WC-10Co-4Cr Coating in 3.5 wt% NaCl Solution, Trans. Indian Inst. Met., 2015, 68(1), p 151–159. https://doi.org/10.1007/s12666-014-0440-510.1007/s12666-014-0440-5 ↗
60. Y. Korobov, H. Alwan, N. Soboleva, A. Makarov, N. Lezhnin, V. Shumyakov, M. Antonov, and M. Deviatiarov, Cavitation Resistance of WC-10Co4Cr and WC-20CrC-7Ni HVAF Coatings, J. Therm. Spray Technol., 2022, 31, p 234–246. https://doi.org/10.1007/s11666-021-01242-710.1007/s11666-021-01242-7 ↗
61. Y.G. Wang, H.Y. Li, X.Y. Yuan, Y.B. Jiang, Z.A. Xiao, and Z. Li, Review of Copper and Copper Alloys as Immune and Antibacterial Element, Trans. Nonferrous Met. Soc. China, 2022, 32(10), p 3163–3181. https://doi.org/10.1016/s1003-6326(22)66011-410.1016/s1003-6326(22)66011-4 ↗
62. X.Y. Zhang, J. Wu, X. Tao, Z.Q. Huang, J.M. Wang, A. Zammit, C.B. Tang, and J. Chen, Designing Cu Chemical Distribution in Ti(AlCu)N Coatings for Enhanced Erosion-Corrosion and Antibacterial Performance, Appl. Surf. Sci., 2024, 648, 159053. https://doi.org/10.1016/j.apsusc.2023.15905310.1016/j.apsusc.2023.159053 ↗
63. Z. Liu, J.W. Ye, A. Rauf, S.Q. Zhang, G.Y. Wang, S.Q. Shi, and G.L. Ning, A Flexible Fibrous Membrane Based on Copper(II) Metal-Organic Framework/Poly(Lactic Acid) Composites with Superior Antibacterial Performance, Biomater. Sci., 2021, 9(10), p 3851–3859. https://doi.org/10.1039/d1bm00164g10.1039/d1bm00164g ↗
64. M. Vincent, R.E. Duval, P. Hartemann, and M. Engels-Deutsch, Contact Killing and Antimicrobial Properties of Copper, J. Appl. Microbiol., 2018, 124(5), p 1032–1046. https://doi.org/10.1111/jam.1368110.1111/jam.13681 ↗