Apparent Interfacial Toughness of Undoped and Photoluminescent Eu3+-Doped Yttria-Stabilized Zirconia Thermal Barrier Coatings
Source abstract
Abstract
Most photoluminescence methods for the diagnostic of thermal barrier coatings (TBC) rely on the functionalization of yttria-stabilized zirconia (YSZ) with trivalent lanthanide ions. It consists in determining temperature and detecting preventively damages within the volume of the TBC prior to ceramic topcoat spallation. The latter depends on the interfacial toughness, which is an important factor to address thermal barrier coating’s performance and durability. In this paper, the influence of the addition of rare earth elements (Eu3+) on the interfacial toughness of TBC deposited by atmospheric plasma spray is investigated. Two types of coatings are deposited and investigated: (1) Type I: coating deposited using Eu3+-doped YSZ powder (2 mol.%), (2) Type II: coating deposited using undoped YSZ powder. Both types of coatings are heat-treated at 1100 °C under isothermal conditions using different oxidation exposure times: 100, 300 and 800 h. The morphology of the interface between the topcoat (TBC) and the bond coat is analyzed by scanning electron microscopy. The apparent interfacial toughness is investigated using indentation. It is shown that the interfacial apparent toughness decreases as the oxidation exposure time increases. Concomitantly, the thickness of the thermally grown oxide (TGO) layer between the bond coat and the topcoat increases. Results show as well that the partial substitution of Y3+ ions by a low amount of Eu3+ ions (2 mol.%) does not have influence on the microstructure and the interfacial toughness of the YSZ coatings. In addition, energy dispersive spectrometry reveals that there is no diffusion of Eu3+ into the TGO layer. It is therefore concluded that the use of Eu3+ for damage diagnostic based on photoluminescence methods will not induce any kind of degradation of the properties of TBCs.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. N. Padture, M. Gell, and E.H. Jordan, Thermal Barrier Coatings for Gas-Turbine Engine Applications, Science, 2002, 296, p 280-28410.1126/science.1068609 ↗
2. B. Goswami, K.R. Ashok, and S.K. Sahay, Thermal Barrier Coating System for Gas Turbine Application—A Review, High Temp. Mater. Process., 2004, 23, p 73-9210.1515/HTMP.2004.23.2.73 ↗
3. W.R. Chen, X. Wu, and D. Dudzinski, Influence of Thermal Cycle Frequency on the TGO Growth and Cracking Behaviors of an APS-TBC, J. Therm. Spray Technol., 2012, 21(6), p 1294-129910.1007/s11666-012-9824-4 ↗
4. M. Gupta, K. Skogsberg, and P. Nylén, Influence of Topcoat-Bondcoat Interface Roughness on Stresses and Lifetime in Thermal Barrier Coatings, J. Therm. Spray Technol., 2014, 23(1-2), p 170-18110.1007/s11666-013-0022-9 ↗
5. W.R. Chen, R. Archer, X. Huang et al., TGO Growth and Crack Propagation in a Thermal Barrier Coating, J. Therm. Spray Technol., 2008, 17(5-6), p 858-86410.1007/s11666-008-9251-8 ↗
6. L. Pin, V. Vidal, F. Blas, F. Ansart, S. Duluard, J.P. Bonino, Y. Le Maoult, and P. Lours, Optimized Sol-Gel Thermal Barrier Coatings for Long-Term Cyclic Oxidation Life, J. Eur. Ceram. Soc., 2014, 34, p 961-97410.1016/j.jeurceramsoc.2013.10.013 ↗
7. J. Sniezewski, V. Vidal, P. Lours, and Y. Le Maoult, Thermal Barrier Coatings Adherence and Spallation: Interfacial Indentation Resistance and Cyclic Oxidation Behavior Under Thermal Gradient, Surf. Coat. Technol., 2009, 204, p 807-81110.1016/j.surfcoat.2009.09.062 ↗
8. Y.K. Liu, Y.H. Liu, P. Lours et al., Influence of Isothermal Aging Conditions on APS TBC’s Interfacial Fracture Toughness, Surf. Coat. Technol., 2017, 313, p 417-42410.1016/j.surfcoat.2017.01.008 ↗
9. J.I. Eldridge and T.J. Bencic, Monitoring Delamination of Plasma-Sprayed Thermal Barrier Coatings by Reflectance-Enhanced Luminescence, Surf. Coat. Technol., 2006, 201, p 3926-393010.1016/j.surfcoat.2006.08.008 ↗
10. J.I. Eldridge, T.J. Bencic, C.M. Spuckler, J. Singh, and D.E. Wolfe, Delamination-Indicating Thermal Barrier Coatings Using YSZ: Eu Sublayers, J. Am. Ceram. Soc., 2006, 89, p 3246-325110.1111/j.1551-2916.2006.01211.x ↗
11. C. Pilgrim, S. Berthier, J. Feist et al., Photoluminescence for Quantitative Non-destructive Evaluation of Thermal Barrier Coating Erosion, Surf. Coat. Technol., 2012, 209(9), p 44-5110.1016/j.surfcoat.2012.08.025 ↗
12. M.M. Gentleman and D.R. Clarke, Concepts for Luminescence Sensing of Thermal Barrier Coatings, Surf. Coat. Technol., 2004, 188, p 93-10010.1016/j.surfcoat.2004.08.005 ↗
13. R.J.L. Steenbakker, J.P. Feist, R.G. Wellman, and J.R. Nicholls, Sensor Thermal Barrier Coatings: Remote In Situ Condition Monitoring of EB-PVD Coatings at Elevated Temperatures, J. Eng. Gas Turbines Power Trans., 2009, 131, p 04130110.1115/1.3077662 ↗
14. G. Portu, L. Micele, Y. Sekiguchi et al., Measurement of Residual Stress Distributions in Al2O3/3Y-TZP Multilayered Composites by Fluorescence and Raman Microprobe Piezo-Spectroscopy, Acta Mater., 2005, 53(5), p 1511-152010.1016/j.actamat.2004.12.003 ↗
15. Y. Zhao, C. Ma, F. Huang et al., Residual Stress Inspection by Eu3+ Photoluminescence Piezo-Spectroscopy: An Application in Thermal Barrier Coatings, J. Appl. Phys., 2013, 114(7), p 502
16. L.L. Sun, H.B. Guo, H. Peng et al., Phase Stability and Thermal Conductivity of Ytterbia and Yttria Co-doped Zirconia, Prog. Nat. Sci. Mater. Int., 2013, 23(4), p 440-44510.1016/j.pnsc.2013.06.013 ↗
17. J.R. Nicholls, K.J. Lawson, A. Johnstone, and D.S. Rickerby, Methods to Reduce the Thermal Conductivity of EB-PVD TBCs, Surf. Coat. Technol., 2002, 151, p 383-39110.1016/S0257-8972(01)01651-6 ↗
18. D.S. Rickerby, P. Morrell, and Y.A. Tamarin, Metallic Article Having a Thermal Barrier Coating and a Method of Application Thereof, brevet US6025078 (A), 2000
19. M.J. Maloney, Thermal Barrier Coating Systems and Materials, brevet US6177200 (B1), 2001
20. U. Schulz, K. Fritscher, C. Leyens, M. Peters, and W.A. Kaysser, Thermocyclic Behavior of Differently Stabilized and Structured EB-PVD Thermal Barrier Coatings, Mater. Werkst., 1997, 28, p 370-37610.1002/mawe.19970280811 ↗
21. U. Schulz, P. Moretto, B. Saint-Ramond, A. Vanlieshout, O. Lavigne, and A. Börger, Low Thermal Conductivity Ceramics for Turbine Blade Thermal Barrier Coating Application. In: E. Lara-Curzio, M.J. Readey (eds.) 28th International Conference on Advanced Ceramics and Composites B Engineering Science Proceedings. Wiley, 2004, p 375-38010.1002/9780470291191.ch57 ↗
22. M.H. Habibi, L. Wang, J.D. Liang et al., An Investigation on Hot Corrosion Behavior of YSZ-Ta2O5 in Na2SO4 + V2O5 Salt at 1100 °C, Corros. Sci., 2013, 75, p 409-41410.1016/j.corsci.2013.06.025 ↗
23. C.C. Pilgrim, S. Berthier, J.P. Feist, R.G. Wellman, and A.L. Heyes, Photoluminescence for Quantitative Non-destructive Evaluation of Thermal Barrier Coating Erosion, Surf. Coat. Technol., 2012, 209, p 44-5110.1016/j.surfcoat.2012.08.025 ↗
24. R.J.L. Steenbakker, R.G. Wellman, and J.R. Nicholls, Erosion of Gadolinia Doped EBPVD TBCs, Surf. Coat. Technol., 2006, 201, p 2140-214610.1016/j.surfcoat.2006.03.022 ↗
25. S. Jiang, X. Huang, Z. He et al., Phase Transformation and Lattice Parameter Changes of Non-trivalent Rare Earth-Doped YSZ as a Function of Temperature, J. Mater. Eng. Perform., 2018, 27(5), p 2263-227010.1007/s11665-018-3159-3 ↗
26. E. Copin, T. Sentenac, Y. Le Maoult, F. Blas, F. Ansart, V. Vidal, and P. Lours, Feasibility of Luminescent Multilayer Sol–Gel Thermal Barrier Coating Manufacturing for Future Applications in Through-Thickness Temperature Gradient Sensing, Surf. Coat. Technol., 2014, 260, p 90-9610.1016/j.surfcoat.2014.08.077 ↗
27. J.I. Eldridge, T.J. Bencic, S.W. Allison, and D.L. Beshears, Depth-Penetrating Temperature Measurements of Thermal Barrier Coatings Incorporating Thermographic Phosphors, J. Therm. Spray Technol., 2004, 13, p 44-5010.1007/s11666-004-0048-0 ↗
28. M.D. Chambers, D.R. Clarke, Doped Oxides for High-Temperature Luminescence and Lifetime Thermometry. In: Annual Review of Materials Research, Palo Alto, 2009, p 325-35910.1146/annurev-matsci-112408-125237 ↗
29. M.M. Gentleman, J.I. Eldridge, D.M. Zhu, K.S. Murphy, and D.R. Clarke, Non-contact Sensing of TBC/BC Interface Temperature in a Thermal Gradient, Surf. Coat. Technol., 2006, 201, p 3937-394110.1016/j.surfcoat.2006.08.102 ↗
30. H.M. Tawancy, N. Sridhar, and N.M. Abbas, Failure Mechanism of a Thermal Barrier Coating System on a Nickel-Base Superalloy, J. Materi. Sci., 1998, 33, p 681-68610.1023/A:1004333627312 ↗
31. J.L. Vasinonta and A. Beuth, Measurement of Interfacial Toughness in Thermal Barrier Coating Systems by Indentation, Eng. Fract. Mech., 2001, 68, p S843-S86010.1016/S0013-7944(00)00130-2 ↗
32. W.G. Mao, J. Wan, C.Y. Dai et al., Evaluation of Microhardness, Fracture Toughness and Residual Stress in a Thermal Barrier Coating System: A Modified Vickers Indentation Technique, Surf. Coat. Technol., 2012, 206, p 4455-446110.1016/j.surfcoat.2012.02.060 ↗
33. D. Chicot, P. Démarécaux, and J. Lesage, Apparent Interface Toughness of Substrate and Coating Couples from Indentation Tests, Thin Solid Films, 1996, 283, p 151-15710.1016/0040-6090(96)08763-9 ↗
34. Y. Liu, V. Vidal, S. Le Roux, F. Blas, F. Ansart, and P. Lours, Influence of Isothermal and Cyclic Oxidation on the Apparent Interfacial Toughness in Thermal Barrier Coating Systems, J. Eur. Ceram. Soc., 2015, 35, p 4269-427510.1016/j.jeurceramsoc.2015.07.018 ↗
35. L.T. Wu, R.T. Wu, X. Zhao, and P. Xiao, Microstructure Parameters Affecting Interfacial Adhesion of Thermal Barrier Coatings by the EB-PVD Method, Mater. Sci. Eng. A, 2014, 594, p 193-20210.1016/j.msea.2013.11.054 ↗
36. P. Planques, V. Vidal, P. Lours et al., Mechanical and Thermo-physical Properties of Plasma-Sprayed Thermal Barrier Coatings: A Literature Survey, Oxid. Met., 2017, 88, p 133-14310.1007/s11085-016-9693-1 ↗