Observation of Residual Stress and Fatigue Behavior of Structurally Integrated Thermally Sprayed Nickel Coatings
Source abstract
Abstract
Fatigue behavior is strongly correlated with the residual stress state within thermal spray coatings, with neutral or compressive residual stresses being favorable for fatigue-sensitive applications. However, determination of the coating’s residual stress state is predominately made prior to subjection of the coating to cyclic loading and does not give insight into possible changes to the residual stress state once in service. In this work, high-velocity, oxy-fuel nickel coatings were subjected to a partial fatigue loading regime, via both rotating bend fatigue and cantilever fatigue, targeting 99% of the total system fatigue life. Neutron diffraction was used to measure changes between the initial compressive residual stresses and after partial fatigue loading and was compared with the residual stress measurements made via beam curvature techniques during deposition. Results indicate that the fatigue credit typically associated with compressive residual stress coatings was partially dependent on the mode of loading and that there was a change in the residual stress magnitude due to changes during fatigue cycling. Additionally, metallographic assessment of the fracture surface was used to determine final fatigue failure within the substrate and crack propagation within the coating crossing through the substrate interface into the substrate.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Metal Alloys Wear and Properties · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. T.W. Clyne and S.C. Gill, Residual Stresses in Thermal Spray Coatings and Their Effect on Interfacial Adhesion: A Review of Recent Work, J. Therm. Spray Technol., 1996, 5(4), p 401-41810.1007/BF02645271 ↗
2. M. Gui, R. Eybel, B. Asselin, S. Radhakrishnan, and J. Cerps, Influence of Processing Parameters on Residual Stress of High Velocity Oxy-Fuel Thermally Sprayed WC-Co-Cr, Coating, 2012, 21(10), p 2090-2098
3. S. Sampath, X.Y. Jiang, J. Matejicek, L. Prchlik, A. Kulkarni, and A. Vaidya, Role of Thermal Spray Processing Method on the Microstructure, Residual Stress and Properties of Coatings: An Integrated Study for Ni–5 wt%Al Bond Coats, Mater. Sci. Eng. A, 2004, 364(1), p 216-23110.1016/j.msea.2003.08.023 ↗
4. S. Sampath, V. Srinivasan, A. Valarezo, A. Vaidya, and T. Streibl, Sensing, Control, and in Situ Measurement of Coating Properties: An Integrated Approach Toward Establishing Process-Property Correlations, J. Therm. Spray Technol., 2009, 18(2), p 243-25510.1007/s11666-009-9314-5 ↗
5. J. Schijve, Ed., Residual Stress, Fatigue of Structures and Materialsed, Springer, Dordrecht, 2009, p 89-104
6. S. Kuroda, T. Dendo, and S. Kitahara, Quenching Stress in Plasma Sprayed Coatings and Its Correlation with the Deposit Microstructure, J. Therm. Spray Technol., 1995, 4(1), p 75-8410.1007/BF02648531 ↗
7. S. Kuroda, Y. Tashiro, H. Yumoto, S. Taira, H. Fukanuma, and S. Tobe, Peening Action and Residual Stresses in High-Velocity Oxygen Fuel Thermal Spraying of 316l Stainless Steel, J. Therm. Spray Technol., 2001, 10(2), p 367-37410.1361/105996301770349457 ↗
8. T.S. Sidhu, S. Prakash, and R.D. Agrawal, State of the Art of HVOF Coating Investigations—A Review, Mar. Technol. Soc. J., 2005, 39(2), p 53-6410.4031/002533205787443908 ↗
9. T. Suhonen, T. Varis, S. Dosta, M. Torrell, and J.M. Guilemany, Residual Stress Development in Cold Sprayed Al, Cu and Ti Coatings, Acta Mater., 2013, 61(17), p 6329-633710.1016/j.actamat.2013.06.033 ↗
10. A. Valarezo, W.B. Choi, W. Chi, A. Gouldstone, and S. Sampath, Process Control and Characterization of NiCr Coatings by HVOF-DJ2700 System: A Process Map Approach, J. Therm. Spray Technol., 2010, 19(5), p 852-86510.1007/s11666-010-9492-1 ↗
11. D.E. Wolfe, T.J. Eden, J.K. Potter, and A.P. Jaroh, Investigation and Characterization of Cr3C2-Based Wear-Resistant Coatings Applied by the Cold Spray Process, J. Therm. Spray Technol., 2006, 15(3), p 400-41210.1361/105996306X124400 ↗
12. J. Kawakita, H. Katanoda, M. Watanabe, K. Yokoyama, and S. Kuroda, Warm Spraying: An Improved Spray Process to Deposit Novel Coatings, Surf. Coat. Technol., 2008, 202(18), p 4369-437310.1016/j.surfcoat.2008.04.011 ↗
13. R.K. Kumar, M. Kamaraj, S. Seetharamu, T. Pramod, and P. Sampathkumaran, Effect of Spray Particle Velocity on Cavitation Erosion Resistance Characteristics of HVOF and HVAF Processed 86WC-10Co4Cr Hydro Turbine Coatings, J. Therm. Spray Technol., 2016, 25(6), p 1217-123010.1007/s11666-016-0427-3 ↗
14. J.A. Browning, Viewing the Future of High-Velocity Oxyfuel (HVOF) and High-Velocity Air Fuel (HVAF) Thermal Spraying, J. Therm. Spray Technol., 1999, 8(3), p 351-356
15. S. Kuroda, M. Watanabe, K. Kim, and H. Katanoda, Current Status and Future Prospects of Warm Spray Technology, J. Therm. Spray Technol., 2011, 20(4), p 653-67610.1007/s11666-011-9648-7 ↗
16. J.M. Guilemany, N. Espallargas, P.H. Suegama, and A.V. Benedetti, Comparative Study of Cr3C2–NiCr Coatings Obtained by HVOF and Hard Chromium Coatings, Corr. Sci., 2006, 48(10), p 2998-301310.1016/j.corsci.2005.10.016 ↗
17. A. Ibrahim and C.C. Berndt, Fatigue and Deformation of Hvof Sprayed WC–Co Coatings and Hard Chrome Plating, Mater. Sci. Eng. A, 2007, 456(1), p 114-11910.1016/j.msea.2006.12.030 ↗
18. B.D. Sartwell, K. Legg, P. Bretz, E., Status of HCAT/JP-PP Program on Replacement of Hard Chrome Plating with HVOF Thermal Spray Coatings on Landing Gear, Proc. of AESF Aero. Plat. Met. Fin. For., 2000, p 131-139
19. A. Vackel, G. Dwivedi, and S. Sampath, Structurally Integrated, Damage-Tolerant, Thermal Spray Coatings, JOM, 2015, 67(7), p 1540-155310.1007/s11837-015-1400-1 ↗
20. A. Vackel and S. Sampath, Fatigue Behavior of Thermal Sprayed WC-CoCr- Steel Systems: Role of Process and Deposition Parameters, Surf. Coat. Technol., 2017, 315, p 408-41610.1016/j.surfcoat.2017.02.062 ↗
21. T. Varis, T. Suhonen, O. Calonius, J. Čuban, and M. Pietola, Optimization of HVOF Cr3C2NiCr Coating for Increased Fatigue Performance, Surf. Coat. Technol., 2016, 305, p 123-13110.1016/j.surfcoat.2016.08.012 ↗
22. J. Matejicek and S. Sampath, In Situ Measurement of Residual Stresses and Elastic Moduli in Thermal Sprayed Coatings: Part 1: Apparatus and Analysis, Acta Mater., 2003, 51(3), p 863-87210.1016/S1359-6454(02)00478-0 ↗
23. J. Matejicek, S. Sampath, D. Gilmore, and R. Neiser, In Situ Measurement of Residual Stresses and Elastic Moduli in Thermal Sprayed Coatings: Part 2: Processing Effects on Properties of Mo Coatings, Acta Mater., 2003, 51(3), p 873-88510.1016/S1359-6454(02)00477-9 ↗
24. O. Kirstein, V. Luzin, and U. Garbe, The Strain-Scanning Diffractometer Kowari, Neutron News, 2009, 20(4), p 34-3610.1080/10448630903241175 ↗
25. A.J. Allen, M.T. Hutchings, C.G. Windsor, and C. Andreani, Neutron Diffraction Methods for the Study of Residual Stress Fields, Adv. Phys., 1985, 34(4), p 445-47310.1080/00018738500101791 ↗
26. V. Luzin, K. Spencer, M. Zhang, N. Matthews, J. Davis, and M. Saleh, Residual Stresses in Cold Spray Coatings, Cold-Spray Coatings: Recent Trends and Future Perspectives, P. Cavaliere, Ed., Springer, Berlin, 2018, p 451-48010.1007/978-3-319-67183-3_16 ↗
27. J. Gibmeier, H.C. Back, M. Mutter, F. Vollert, J. Rebelo-Kornmeier, R. Mücke, and R. Vaßen, Study of Stability of Microstructure and Residual Strain After Thermal Loading of Plasma Sprayed YSZ by Through Surface Neutron, Scanning, 2018, 551, p 69-78
28. G.M. Smith and S. Sampath, Sustainability of Metal Structures Via Spray-Clad Remanufacturing, JOM, 2018, 70(4), p 512-52010.1007/s11837-017-2676-0 ↗
29. W.B. Choi, L. Li, V. Luzin, R. Neiser, T. Gnäupel-Herold, H.J. Prask, S. Sampath, and A. Gouldstone, Integrated Characterization of Cold Sprayed Aluminum Coatings, Acta Mater., 2007, 55(3), p 857-86610.1016/j.actamat.2006.09.006 ↗
30. J. Matějíček, S. Sampath, T. Gnäupel-Herold, and H.J. Prask, Residual Stress in Sprayed Ni + 5%Al Coatings Determined by Neutron Diffraction, Appl. Phys. A, 2002, 74(1), p 1692-169410.1007/s003390101264 ↗
31. V. Luzin, K. Spencer, and M.X. Zhang, Residual Stress and Thermo-Mechanical Properties of Cold Spray Metal Coatings, Acta Mater., 2011, 59(3), p 1259-127010.1016/j.actamat.2010.10.058 ↗
32. V. Luzin, A. Vackel, A. Valarezo, and S. Sampath, Neutron Through-Thickness Stress Measurements in Coatings with High Spatial Resolution, Mater. Sci. Forum, 2017, 905, p 165-17310.4028/www.scientific.net/MSF.905.165 ↗
33. Y. Sugimura, P.G. Lim, C.F. Shih, and S. Suresh, Fracture Normal to a Bimaterial Interface: Effects of Plasticity on Crack-Tip Shielding and Amplification, Acta Mater., 1995, 43(3), p 1157-116910.1016/0956-7151(94)00295-S ↗
34. S. Suresh, Fatigue of Materials, 2nd ed., Cambridge University Press, Cambridge, 199810.1017/CBO9780511806575 ↗
35. A. Vackel, T. Nakamura, and S. Sampath, Mechanical Behavior of Spray-Coated Metallic Laminates, J. Therm. Spray Technol., 2016, 25(5), p 1009-101910.1007/s11666-016-0404-x ↗
36. X. Luo, G.M. Smith, and S. Sampath, On the Interplay Between Adhesion Strength and Tensile Properties of Thermal Spray Coated Laminates—Part I: High Velocity Thermal Spray Coatings, J. Therm. Spray Technol., 2018, 27(3), p 296-30710.1007/s11666-018-0695-1 ↗
37. A. Valarezo and S. Sampath, An Integrated Assessment of Process-Microstructure-Property Relationships for Thermal-Sprayed NiCr Coatings, J. Therm. Spray Technol., 2011, 20(6), p 1244-125810.1007/s11666-011-9665-6 ↗
38. T. Gnäeupel-Herold, H.J. Prask, J. Barker, F.S. Biancaniello, R.D. Jiggetts, and J. Matejicek, Microstructure, Mechanical Properties, and Adhesion in IN625 Air Plasma Sprayed Coatings, Mater. Sci. Eng. A, 2006, 421(1), p 77-8510.1016/j.msea.2005.10.003 ↗
39. Z. Wang, A. Kulkarni, S. Deshpande, T. Nakamura, and H. Herman, Effects of Pores and Interfaces on Effective Properties of Plasma Sprayed Zirconia Coatings, Acta Mater., 2003, 51(18), p 5319-533410.1016/S1359-6454(03)00390-2 ↗
40. G.M. Smith, A. Smith, and S. Sampath, Fracture Toughness of Thermal Spray Ceramics: Measurement Techniques and Processing Dependence, J. Therm. Spray Technol., 2018, 27(7), p 1076-108910.1007/s11666-018-0755-6 ↗
41. G.M. Smith and S. Sampath, Sustainability of Metal Structures Via Spray-Clad Remanufacturing, JOM, 2018, 70, p 512-52010.1007/s11837-017-2676-0 ↗
42. J.M. Gere and S. Timoshenko, Mechanics of Materials, PWS Publishing Company, New Orleans, 1997
43. O. Kovářík, P. Haušild, J. Medřický, L. Tomek, J. Siegl, R. Mušálek, N. Curry, and S. Björklund, Fatigue Crack Growth in Bodies with Thermally Sprayed, Coating, 2016, 25(1), p 311-320
44. O. Kovarik, A. Materna, J. Siegl, J. Cizek, and J. Klecka, Fatigue Crack Growth in Plasma-Sprayed Refractory Materials, J. Therm. Spray Technol., 2019, 28(1), p 87-9710.1007/s11666-018-0790-3 ↗
45. X. Luo, G.M. Smith, and S. Sampath, On the Interplay between Adhesion Strength and Tensile Properties of Thermal Spray Coated Laminates—Part II: Low-Velocity Thermal Spray Coatings, J. Therm. Spray Technol., 2018, 27(3), p 308-31810.1007/s11666-018-0690-6 ↗
46. G.M. Smith, O. Higgins, and S. Sampath, In-Situ Observation of Strain and Cracking in Coated Laminates by Digital Image Correlation, Surf. Coat. Technol., 2017, 328, p 211-21810.1016/j.surfcoat.2017.08.057 ↗
47. M.A.M. Halmi, M.A. Harimon, L.M. Tobi, and M.F. Mahmod, Fatigue Performance of Thermal Spray Coatings on Carbon Steel: A Review, Int. J. Mech. Eng. Technol., 2019, 10(3), p 1285-1300
48. N.W. Sachs, Understanding the Surface Features of Fatigue Fractures: How They Describe the Failure Cause and the Failure History, J. Fail. Anal. Prev., 2005, 5(2), p 11-1510.1361/15477020522924 ↗
49. A. Silvello, P. Cavaliere, A. Rizzo, D. Valerini, S. Dosta Parras, and I. Garcia Cano, Fatigue Bending Behavior of Cold-Sprayed Nickel-Based Superalloy Coatings, J. Therm. Spray Technol., 2019, 28(5), p 930-93810.1007/s11666-019-00865-1 ↗
50. L. Janka, J. Norpoth, R. Trache, S. Thiele, and L.-M. Berger, HVOF- and HVAF-Sprayed Cr3C2-NiCr Coatings Deposited from Feedstock Powders of Spherical Morphology: Microstructure Formation and High-Stress Abrasive Wear Resistance up to 800 & #xB0;C, J. Therm. Spray Technol., 2017, 26(7), p 1720-173110.1007/s11666-017-0621-y ↗