journal article·2024-04Open access

Fretting Behavior of WC-Co-Cr Coatings Against QT Steel in Bolted Joint

Vilma Haaja, Tommi Varis, Jussi Laurila, Matti Isakov

Abstract

Abstract Fretting damage on contacting surfaces introduces major challenges in mechanical assemblies. Thermal sprayed hardmetal coatings are extensively used for surface modification in tribological applications under demanding conditions and may also be subjected to fretting-inducing loading. In the present work, the fretting behavior of High Velocity Oxy-Fuel (HVOF) and High Velocity Air–Fuel (HVAF) sprayed WC-10Co-4Cr coatings against quenched and tempered (QT) steel was studied by using a single bolt joint-type fretting experiment. This experimental approach was selected to obtain realistic data on the fretting fatigue performance of the contact pairs (both coating-to-steel and coating-to-coating). Experimental results were completed with continuum-scale linear elastic finite element method (FEM) calculations.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Mechanical stress and fatigue analysis · Metal Alloys Wear and Properties · Electrical Contact Performance and Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. A.R. Govande, A. Chandak, B.R. Sunil, and R. Dumpala, Carbide-Based Thermal Spray Coatings: A Review on Performance Characteristics and Post-Treatment, Int. J. Refract Metal Hard Mater., 2022, 103, p 105772. https://doi.org/10.1016/j.ijrmhm.2021.10577210.1016/j.ijrmhm.2021.105772 ↗
2. G. Bolelli, L.-M. Berger, T. Börner, H. Koivuluoto, L. Lusvarghi, C. Lyphout, N. Markocsan, V. Matikainen, P. Nylén, P. Sassatelli, R. Trache, and P. Vuoristo, Tribology of HVOF- and HVAF-Sprayed WC–10Co4Cr Hardmetal Coatings: A Comparative Assessment, Surf. Coat. Technol., 2015, 265, p 125–144. https://doi.org/10.1016/j.surfcoat.2015.01.04810.1016/j.surfcoat.2015.01.048 ↗
3. V. Eronen, S. Ahmaniemi, K. Niemi, and P. Vuoristo, Microwear in thermally sprayed hard coatings by different abrasives, in Proceedings of the ITSC2005. Thermal Spray 2005, in Proceedings from the International Thermal Spray Conference, ASM, Basel, (2005), pp. 815–822. https://doi.org/10.31399/asm.cp.itsc2005p081510.31399/asm.cp.itsc2005p0815 ↗
4. J. Kiilakoski, V. Eronen, and P. Vuoristo, Wear Properties of Thermally Sprayed Tungsten-Carbide Coatings in Paper Machine Environments, Finn. J. Tribol., 2015, 33, p 29–35.
5. A. Agüero, F. Camón, J. García de Blas, J.C. del Hoyo, R. Muelas, A. Santaballa, S. Ulargui, and P. Vallés, HVOF-Deposited WCCoCr as Replacement for Hard Cr in Landing Gear Actuators, J. Therm. Spray Technol., 2011, 20, p 1292–1309. https://doi.org/10.1007/s11666-011-9686-110.1007/s11666-011-9686-1 ↗
6. G. Matthäus, J. Henry, D. Ackermann, and W. Brandl, Further Developments in Internal Diameter HVOF Application of WC-CoCr for Hard Chrome Replacement in Critical Applications Such as Landing Gear, in Proceedings of the ITSC2009. Thermal Spray 2009, in Proceedings from the International Thermal Spray Conference, ASM, Las Vegas, Nevada, (2009) pp. 722–724. https://doi.org/10.31399/asm.cp.itsc2009p072210.31399/asm.cp.itsc2009p0722 ↗
7. R. de Medeiros Castro, A. de Silva Rocha, E. Isaías Mercado Curi, and F. Peruch, A Comparison of Microstructural, Mechanical and Tribological Properties of WC-10Co4Cr-HVOF Coating and Hard Chrome to Use in Hydraulic Cylinders, Am. J. Mater. Sci., 2018, 8, p 15–26. https://doi.org/10.5923/j.materials.20180801.0310.5923/j.materials.20180801.03 ↗
8. J. Pulsford, F. Venturi, Z. Pala, S. Kamnis, and T. Hussain, Application of HVOF WC-Co-Cr Coatings on the Internal Surface of Small Cylinders: Effect of Internal Diameter on the Wear Resistance, Wear, 2019, 432–433, p 202965. https://doi.org/10.1016/j.wear.2019.20296510.1016/j.wear.2019.202965 ↗
9. K. Bobzin, W. Wietheger, H. Heinemann, M. Schulz, M. Oechsner, T. Engler, H. Scheerer, and Y. Joung, Thermally Sprayed Coatings for the Valve Industry, Materialwissenschaft und Werkstofftechik, 2021, 52, p 997–1011. https://doi.org/10.1002/mawe.20210003210.1002/mawe.202100032 ↗
10. B.S. Mann and V. Arya, Abrasive and Erosive Wear Characteristics of Plasma Nitriding and HVOF Coatings: Their Application in Hydro Turbines, Wear, 2001, 249, p 354–360. https://doi.org/10.1016/S0043-1648(01)00537-310.1016/S0043-1648(01)00537-3 ↗
11. P. Vuoristo, Thermal Spray Coating Processes, Comprehensive Materials Processing Coatings and films, 1st ed., D. Cameron Ed., Elsevier, 2014, p 229–27610.1016/B978-0-08-096532-1.00407-6 ↗
12. J. Juoksukangas, A. Lehtovaara, and A. Mäntylä, Experimental and Numerical Investigation of Fretting Fatigue Behavior in Bolted Joints, Tribol. Int., 2016, 103, p 440–448. https://doi.org/10.1016/j.triboint.2016.07.02110.1016/j.triboint.2016.07.021 ↗
13. R.B. Waterhouse, Fretting Fatigue, Applied Science Publishers, London, 1981.
14. D.A. Hills and D. Nowell, Mechanics of Fretting Fatigue, Springer, 1994.10.1007/978-94-015-8281-0 ↗
15. S. Fouvry, V. Fridrici, C. Langlade, P. Kapsa, and L. Vincent, Palliatives in Fretting: A Dynamical Approach, Tribol. Int., 2006, 39, p 1005–1015. https://doi.org/10.1016/j.triboint.2006.02.03810.1016/j.triboint.2006.02.038 ↗
16. Y. Fu, J. Wei, and A.W. Batchelor, Some Considerations on the Mitigation of Fretting Damage by the Application of Surface-Modification Technologies, J. Mater. Process. Technol., 2000, 99, p 231–245. https://doi.org/10.1016/S0924-0136(99)00429-X10.1016/S0924-0136(99)00429-X ↗
17. I.P. Okokpujie, L.K. Tartibu, H.O. Musa-Basheer, and A.O.M. Adeoye, Effect of Coatings on Mechanical Corrosion and Tribological Properties of Industrial Materials: A Comprehensive Review, J. Bio- Tribo-Corros., 2024, 10, p 2. https://doi.org/10.1007/s40735-023-00805-110.1007/s40735-023-00805-1 ↗
18. G. Bolelli, L.M. Berger, M. Bonetti, and L. Lusvarghi, Comparative Study of the Dry Sliding Wear Behaviour of HVOF-Sprayed WC-(W, Cr)2C-Ni and WC-CoCr Hardmetal Coatings, Wear, 2014, 309, p 96–111. https://doi.org/10.1016/j.wear.2013.11.00110.1016/j.wear.2013.11.001 ↗
19. J.K.N. Murthy and B. Venkataraman, Abrasive Wear Behaviour of WC-CoCr and Cr3C2-20(NiCr) Deposited by HVOF and Detonation Spray Processes, Surf. Coat. Technol., 2006, 200, p 2642–2652. https://doi.org/10.1016/j.surfcoat.2004.10.13610.1016/j.surfcoat.2004.10.136 ↗
20. Q. Wang, S. Zhang, Y. Cheng, J. Xiang, X. Zhao, and G. Yang, Wear and Corrosion Performance of WC-10Co4Cr Coatings Deposited by Different HVOF and HVAF Spraying Processes, Surf. Coat. Technol., 2013, 218, p 127–136. https://doi.org/10.1016/j.surfcoat.2012.12.04110.1016/j.surfcoat.2012.12.041 ↗
21. A.C. Karaoglanli, M. Oge, K.M. Doleker, and M. Hotamis, Comparison of Tribological Properties of HVOF Sprayed Coatings with Different Composition, Surf. Coat. Technol., 2017, 318, p 299–308. https://doi.org/10.1016/j.surfcoat.2017.02.02110.1016/j.surfcoat.2017.02.021 ↗
22. T. Varis, T. Suhonen, J. Laakso, M. Jokipii, and P. Vuoristo, Evaluation of Residual Stresses and Their Influence on Cavitation Erosion Resistance of High Kinetic HVOF and HVAF-Sprayed WC-CoCr Coatings, J. Therm. Spray Technol., 2020, 29, p 1365–1381. https://doi.org/10.1007/s11666-020-01037-210.1007/s11666-020-01037-2 ↗
23. V. Matikainen, H. Koivuluoto, P. Vuoristo, J. Schubert, and Š Houdková, Effect of Nozzle Geometry on the Microstructure and Properties of HVAF-Sprayed WC-10Co4Cr and Cr3C2-25NiCr Coatings, J. Therm. Spray Technol., 2018, 27, p 680–694. https://doi.org/10.1007/s11666-018-0717-z10.1007/s11666-018-0717-z ↗
24. V. Matikainen, S. Rubio Peregrina, N. Ojala, H. Koivuluoto, J. Schubert, Š Houdková, and P. Vuoristo, Erosion Wear Performance of WC-10Co4Cr and Cr3C2-25NiCr Coatings Sprayed with High-Velocity Thermal Spray Processes, Surf. Coat. Technol., 2019, 370, p 196–212. https://doi.org/10.1016/j.surfcoat.2019.04.06710.1016/j.surfcoat.2019.04.067 ↗
25. A. Vackel and S. Sampath, Fatigue Behavior of Thermal Sprayed WC-CoCr- Steel Systems: Role of Process and Deposition Parameters, Surf. Coat. Technol., 2017, 315, p 408–416. https://doi.org/10.1016/j.surfcoat.2017.02.06210.1016/j.surfcoat.2017.02.062 ↗
26. R.T.R. McGrann, D.J. Greving, J.R. Shadley, E.F. Rybicki, T.L. Kruecke, and B.E. Bodger, The Effect of Coating Residual Stress on the Fatigue Life of Thermal Spray-Coated Steel and Aluminum, Surf. Coat. Technol., 1998, 108–109, p 59–64. https://doi.org/10.1016/S0257-8972(98)00665-310.1016/S0257-8972(98)00665-3 ↗
27. H.J.C. Voorwald, R.C. Souza, W.L. Pigatin, and M.O.H. Cioffi, Evaluation of WC-17Co and WC-10Co-4Cr Thermal Spray Coatings by HVOF on the Fatigue and Corrosion Strength of AISI 4340 Steel, Surf. Coat. Technol., 2005, 190, p 155–164. https://doi.org/10.1016/j.surfcoat.2004.08.18110.1016/j.surfcoat.2004.08.181 ↗
28. J.G. La Barbera-Sosa, Y.Y. Santana, C. Villalobos-Gutiérrez, D. Chicot, J. Lesage, X. Decoopman, A. Iost, M.H. Staia, and E.S. Puchi-Cabrera, Fatigue Behavior of a Structural Steel Coated with a WC-10Co-4Cr/Colmonoy 88 Deposit by HVOF Thermal Spraying, Surf. Coat. Technol., 2013, 220, p 248–256. https://doi.org/10.1016/j.surfcoat.2012.05.09810.1016/j.surfcoat.2012.05.098 ↗
29. D. Du, D. Liu, X. Zhang, J. Tang, and B. Meng, Effects of WC-17Co Coating Combined with Shot Peening Treatment on Fatigue Behaviors of TC21 Titanium Alloy, Materials, 2016, 9, p 865. https://doi.org/10.3390/ma911086510.3390/ma9110865 ↗
30. C.H. Sathisha, B.N. Ravikumar, K. Anand, and T. Shalini, Elevated Temperature Fretting Wear Behavior of Cobalt-Based Alloys, J. Tribol., 2016, 138, p 031601. https://doi.org/10.1115/1.403183110.1115/1.4031831 ↗
31. G. Lv, X. Yang, T. Gao, S. Wang, J. Xiao, Y. Zhang, K. Chen, and H. Yang, Investigation on Fretting Wear Performance of Laser Cladding WC/Co06 Coating on 42CrMo Steel for Hydraulic Damper, Int. J. Refract Metal Hard Mater., 2023, 111, p 106068. https://doi.org/10.1016/j.ijrmhm.2022.10606810.1016/j.ijrmhm.2022.106068 ↗
32. K. Kubiak, S. Fouvry, and A.M. Marechal, A Practical Methodology to Select Fretting Palliatives: Application to Shot Peening, Hard Chromium and WC-Co Coatings, Wear, 2005, 259, p 367–376. https://doi.org/10.1016/j.wear.2005.01.03010.1016/j.wear.2005.01.030 ↗
33. K. Kubiak, S. Fouvry, A.M. Marechal, and J.M. Vernet, Behaviour of Shot Peening Combined with WC-Co HVOF Coating under Complex Fretting Wear and Fretting Fatigue Loading Conditions, Surf. Coat. Technol., 2006, 201, p 4323–4328. https://doi.org/10.1016/j.surfcoat.2006.08.09410.1016/j.surfcoat.2006.08.094 ↗
34. M. Okane, K. Shiozawa, M. Hiki, and K. Suzuki, Fretting Fatigue Properties of WC-Co Thermal Sprayed NiCrMo Steel, Fretting Fatigue, Advances in the Basic Understanding and Applications ASTM STP 1425. Y. Mutoh, S.E. Kinyon, D.W. Hoeppner Ed., ASTM International, West Conshohocken, 2003, p 385–399
35. X.X. Wang, X.C. Ping, X. Zeng, R.J. Wang, Q. Zhao, S.J. Ying, and T. Hu, Fretting Fatigue Experiment and Simulation of WC-12Co Coating Taking into Account the Wear Effects, Surf. Coat. Technol., 2022, 441, p 128555. https://doi.org/10.1016/j.surfcoat.2022.12855510.1016/j.surfcoat.2022.128555 ↗
36. X. Zeng, X. Wang, X. Ping, R. Wang, and T. Hu, Research on Fretting Fatigue of Tungsten Carbide Coating Based on Strain Energy Density Methods, Arch. Metall. Mater., 2023, 68(1), p 21–30. https://doi.org/10.24425/amm.2023.14146710.24425/amm.2023.141467 ↗
37. J. Hintikka, A. Lehtovaara, and A. Mäntylä, Fretting-Induced Friction and Wear in Large Flat-on-Flat Contact with Quenched and Tempered Steel, Tribol. Int., 2015, 92, p 191–202. https://doi.org/10.1016/j.triboint.2015.06.00810.1016/j.triboint.2015.06.008 ↗
38. Y.C. Tsui and T.W. Clyne, An Analytical Model for Predicting Residual Stresses in Progressively Deposited Coatings: Part 1: Planar Geometry, Thin Solid Films, 1997, 306, p 23–33. https://doi.org/10.1016/S0040-6090(97)00199-510.1016/S0040-6090(97)00199-5 ↗
39. T. Suhonen, T. Varis, E. Turunen, X. Liu, Y. Ge, O. Söderberg, and S.-P. Hannula, The Effect of Microstructure on Mechanical Properties of HVOF Sprayed WC-CoCr Composite Coatings, Tribology, 2009, 28, p 14–28.
40. Y.C. Tsui, and T.W. Clyne, An Analytical Model for Predicting Residual Stresses in Progressively Deposited Coatings: Part 3: Further Development and Applications, Thin Solid Films, 1997, 306, p 52–61. https://doi.org/10.1016/S0040-6090(97)00208-310.1016/S0040-6090(97)00208-3 ↗
41. J. Matejicek, S. Sampath, D. Gilmore, and R. Neiser, In Situ Measurement of Residual Stresses and Elastic Moduli in Thermal Sprayed Coatings Part 2: Processing Effects on Properties of Mo Coatings, Acta Mater., 2003, 51, p 873–885. https://doi.org/10.1016/S1359-6454(02)00477-910.1016/S1359-6454(02)00477-9 ↗
42. T. Varis, T. Suhonen, M. Jokipii, and P. Vuoristo, Influence of Powder Properties on Residual Stresses Formed in High-Pressure Liquid Fuel HVOF Sprayed WC-CoCr Coatings, Surf. Coat. Technol., 2020, 388, p 125604. https://doi.org/10.1016/j.surfcoat.2020.12560410.1016/j.surfcoat.2020.125604 ↗
43. K. Fan, W. Jiang, V. Luzin, T. Gong, W. Feng, J. Ruiz-Hervias, and P. Yao, Influence of WC Particle Size on the Mechanical Properties and Residual Stress of HVOF Thermally Sprayed WC-10Co-4Cr Coatings, Materials, 2022, 15, p 5537. https://doi.org/10.3390/ma1516553710.3390/ma15165537 ↗
44. L. Rajanna, T.G. Mamatha, M.S. Prabhuswamy, V. Singh, and A. Bansal, Performance of HVAF Sprayed WC-10Co-4Cr Coating Onto Cast 21–4N Steel for Slurry Erosion: Characterization and Erosion Rate Studies, Proc. Inst. Mech. Eng. Part C J. Mech. Eng. Sci., 2023 https://doi.org/10.1177/0954406223121171710.1177/09544062231211717 ↗
45. E. Leidich, A. Maiwald, and J. Vidner, A Proposal for a Fretting Wear Criterion for Coated Systems with Complete Contact Based on Accumulated Friction Energy Density, Wear, 2013, 297, p 903–910. https://doi.org/10.1016/j.wear.2012.11.00610.1016/j.wear.2012.11.006 ↗
46. V. Nurmi, J. Hintikka, J. Juoksukangas, M. Honkanen, M. Vippola, A. Lehtovaara, A. Mäntylä, J. Vaara, and T. Frondelius, The Formation and Characterization of Fretting-Induced Degradation Layers Using Quenched and Tempered Steel, Tribol. Int., 2019, 131, p 258–267. https://doi.org/10.1016/j.triboint.2018.09.01210.1016/j.triboint.2018.09.012 ↗
47. B.D. Leonard, A. Ghosh, F. Sadeghi, S. Shinde, and M. Mittelbach, Third Body Modeling in Fretting Using the Combined Finite-Discrete Element Method, Int. J. Solids Struct., 2014, 51, p 1375–1389. https://doi.org/10.1016/j.ijsolstr.2013.12.03610.1016/j.ijsolstr.2013.12.036 ↗
48. A.M. Kirk, P.H. Shipway, W. Sun, and C.J. Bennett, The Effect of Frequency on Both the Debris and the Development of the Tribologically Transformed Structure During Fretting Wear of a High Strength Steel, Wear, 2019, 426–427, p 694–703. https://doi.org/10.1016/j.wear.2018.12.03510.1016/j.wear.2018.12.035 ↗
49. J. Hintikka, A. Lehtovaara, and A. Mäntylä, Third Particle Ejection Effects on Wear with Quenched and Tempered Steel Fretting Contact, Tribol. Trans., 2017, 60, p 70–78. https://doi.org/10.1080/10402004.2016.114681310.1080/10402004.2016.1146813 ↗
50. C. Colombie, Y. Berthier, A. Floquet, L. Vincent, and M. Godet, Fretting: Load Carrying Capacity of Wear Debris, J. Tribol., 1984, 106, p 194–201. https://doi.org/10.1115/1.326088110.1115/1.3260881 ↗
51. M. Gui, R. Eybel, B. Asselin, and F. Monerie-Moulin, Cracking and Spalling Behavior of HVOF Thermally Sprayed WC-Co-Cr Coating in Bend and Axial Fatigue Tests, J. Mater. Eng. Perform., 2015, 24, p 1347–1356. https://doi.org/10.1007/s11665-014-1378-910.1007/s11665-014-1378-9 ↗
52. G.W. Schulze and F. Erdogan, Periodic Cracking of Elastic Coatings, Int. J. Solids Struct., 1998, 35, p 3615–3634. https://doi.org/10.1016/S0020-7683(97)00228-X10.1016/S0020-7683(97)00228-X ↗
53. V. Haaja, T. Varis, J. Laurila, and M. Isakov, PerforMat Project, Use Case 1, Microstructural Characterisation Data, IDA FAIRDATA, (2023). https://doi.org/10.23729/94675246-8435-436d-a872-110cb8ca699d10.23729/94675246-8435-436d-a872-110cb8ca699d ↗