Enhanced Cavitation Erosion–Corrosion Resistance of High-Velocity Oxy-Fuel-Sprayed Ni-Cr-Al2O3 Coatings Through Stationary Friction Processing
Source abstract
Abstract
Cavitation erosion is a huge problem in engineering structures working under hydrodynamic conditions. The synergistic effect of erosion and corrosion can aggravate the material removal by several orders of magnitude. Surface coatings are widely used to address material degradation by erosion–corrosion. However, non-homogenous microstructure and presence of defects leads to premature coating failure under erosion–corrosion conditions. Thus, it is imperative to identify plausible solutions to address cavitation-related material degradation. In this study, Ni-Cr-5Al2O3 coatings were deposited on stainless steel substrate using high-velocity-oxy-fuel technique. The as-sprayed coating showed highly non-homogeneous microstructure comprising splats, pores, intermetallic compounds and elemental segregation. A new thermo-mechanical processing technique, stationary friction processing (SFP), was utilized for achieving through-thickness microstructural refinement in as-sprayed coating. As-sprayed and SFP-treated coatings were tested in pure cavitation erosion, corrosion in 3.5% NaCl solution and erosion–corrosion. SFP treatment resulted in 5-times enhancement in the erosion and corrosion resistance compared to as-sprayed coating. The remarkable performance of Ni-Cr-5Al2O3 coatings after SFP treatment is attributed to significant enhancement in the mechanical properties including hardness and fracture toughness which is the consequence of complete removal of splat boundaries, pores, intermetallic compounds and uniform element distribution up to the coating–substrate interface.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Aluminum Alloys Composites Properties · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. A. Karimi and J.L. Martin, Cavitation Erosion of Materials, Int. Met. Rev., 1986, 31(1), p 1-2610.1179/imr.1986.31.1.1 ↗
2. H.G. Feller and Y. Kharrazi, Cavitation Erosion of Metals and Alloys, Wear, 1984, 93(3), p 249-26010.1016/0043-1648(84)90199-6 ↗
3. A. Al-Hashem, P.G. Caceres, W.T. Riad, and H.M. Shalaby, Cavitation Corrosion Behavior of Cast Nickel-Aluminum Bronze in Seawater, Corrosion, 1995, 51(5), p 331-34210.5006/1.3293598 ↗
4. C.T. Kwok, F.T. Cheng, and H.C. Man, Synergistic Effect of Cavitation Erosion and Corrosion of Various Engineering Alloys in 3.5% NaCl Solution, Mater. Sci. Eng. A, 2000, 290(1), p 145-15410.1016/S0921-5093(00)00899-6 ↗
5. J. Ryl, J. Wysocka, P. Slepski, and K. Darowicki, Instantaneous Impedance Monitoring of Synergistic Effect Between Cavitation Erosion and Corrosion Processes, Electrochim. Acta, 2016, 203, p 388-39510.1016/j.electacta.2016.01.216 ↗
6. R.B. Nair, H.S. Arora, S. Mukherjee, S. Singh, H. Singh, and H.S. Grewal, Exceptionally High Cavitation Erosion and Corrosion Resistance of a High Entropy Alloy, Ultrason. Sonochem., 2018, 41, p 252-26010.1016/j.ultsonch.2017.09.044 ↗
7. K. Selvam, P. Mandal, H.S. Grewal, and H.S. Arora, Ultrasonic Cavitation Erosion-Corrosion Behavior of Friction Stir Processed Stainless Steel, Ultrason. Sonochem., 2018, 44, p 331-33910.1016/j.ultsonch.2018.02.041 ↗
8. K. Selvam, J. Saini, G. Perumal, A. Ayyagari, R. Salloom, R. Mondal, S. Mukherjee, H.S. Grewal, and H.S. Arora, Exceptional Cavitation Erosion-Corrosion Behavior of Dual-Phase Bimodal Structure in Austenitic Stainless Steel, Tribol. Int., 2019, 134, p 77-8610.1016/j.triboint.2019.01.018 ↗
9. S. Hanke, A. Fischer, M. Beyer, and J. dos Santos, Cavitation Erosion of NiAl-Bronze Layers Generated by Friction Surfacing, Wear, 2011, 273(1), p 32-3710.1016/j.wear.2011.06.002 ↗
10. A.K. Krella, Cavitation Erosion Resistance of Ti/TiN Multilayer Coatings, Surf. Coat. Technol., 2013, 228, p 115-12310.1016/j.surfcoat.2013.04.016 ↗
11. S. Momeni, W. Tillmann, and M. Pohl, Composite Cavitation Resistant PVD Coatings Based on NiTi Thin Films, Mater. Des., 2016, 110, p 830-83810.1016/j.matdes.2016.08.054 ↗
12. N. Frees, Cavitation Erosion of Titanium Carbide Coatings on Cemented Carbides and Other Substrates, Wear, 1983, 88(1), p 57-6610.1016/0043-1648(83)90312-5 ↗
13. C. Pflitsch, B. Curdts, V. Buck, and B. Atakan, Wear Properties of MOCVD-Grown Aluminium Oxide Films Studied by Cavitation Erosion Experiments, Surf. Coat. Technol., 2007, 201(22), p 9299-930310.1016/j.surfcoat.2007.04.092 ↗
14. A. Babu, H.S. Arora, and H.S. Grewal, Microwave-Assisted Post-Processing of Detonation Gun-Sprayed Coatings for Better Slurry and Cavitation Erosion Resistance, J. Therm. Spray Technol., 2019, 28(7), p 1565-157810.1007/s11666-019-00914-9 ↗
15. A. Babu, H.S. Arora, H. Singh, and H.S. Grewal, Microwave Synthesized Composite Claddings with Enhanced Cavitation Erosion Resistance, Wear, 2019, 422–423, p 242-25110.1016/j.wear.2019.01.072 ↗
16. R.B. Nair, H.S. Arora, and H.S. Grewal, Microwave Synthesized Complex Concentrated Alloy Coatings: Plausible Solution to Cavitation Induced Erosion-Corrosion, Ultrason. Sonochem., 2019, 50, p 114-12510.1016/j.ultsonch.2018.09.004 ↗
17. W. Yuping, L. Pinghua, C. Chenglin, W. Zehua, C. Ming, and H. Junhua, Cavitation Erosion Characteristics of a Fe–Cr–Si–B-Mn Coating Fabricated by High Velocity Oxy-Fuel (HVOF) Thermal Spray, Mater. Lett., 2007, 61(8), p 1867-187210.1016/j.matlet.2006.07.147 ↗
18. J.F. Santa, L.A. Espitia, J.A. Blanco, S.A. Romo, and A. Toro, Slurry and Cavitation Erosion Resistance of Thermal Spray Coatings, Wear, 2009, 267(1), p 160-16710.1016/j.wear.2009.01.018 ↗
19. S. Hong, Y. Wu, Q. Wang, G. Ying, G. Li, W. Gao, B. Wang, and W. Guo, Microstructure and Cavitation–Silt Erosion Behavior of High-Velocity Oxygen–Fuel (HVOF) Sprayed Cr3C2-NiCr Coating, Surf. Coat. Technol., 2013, 225, p 85-9110.1016/j.surfcoat.2013.03.020 ↗
20. G. Hou, X. Zhao, H. Zhou, J. Lu, Y. An, J. Chen, and J. Yang, Cavitation Erosion of Several Oxy-Fuel Sprayed Coatings Tested in Deionized Water and Artificial Seawater, Wear, 2014, 311(1), p 81-9210.1016/j.wear.2013.12.026 ↗
21. S. Hong, Y. Wu, J. Zhang, Y. Zheng, Y. Qin, and J. Lin, Ultrasonic Cavitation Erosion of High-Velocity Oxygen-Fuel (HVOF) Sprayed Near-Nanostructured WC–10Co–4Cr coating in NaCl Solution, Ultrason. Sonochem., 2015, 26, p 87-9210.1016/j.ultsonch.2015.01.012 ↗
22. S. Hong, Y. Wu, J. Zhang, Y. Zheng, Y. Zheng, and J. Lin, Synergistic Effect of Ultrasonic Cavitation Erosion and Corrosion of WC–CoCr and FeCrSiBMn Coatings Prepared by HVOF Spraying, Ultrason. Sonochem., 2016, 31, p 563-56910.1016/j.ultsonch.2016.02.011 ↗
23. A. Kumar, J. Boy, R. Zatorski, and L. Stephenson, Thermal Spray and Weld Repair Alloys for the Repair of Cavitation Damage in Turbines and Pumps: A Technical Note, J. Therm. Spray Technol., 2005, 14(2), p 177-18210.1361/10599630523737 ↗
24. L. Thakur and N. Arora, A Study on erosive Wear Behavior of HVOF Sprayed Nanostructured WC-CoCr Coatings, J. Mech. Sci. Technol., 2013, 27(5), p 1461-146710.1007/s12206-013-0326-1 ↗
25. A. Babu, H. Arora, and H. Grewal, Microwave-Assisted Post-processing of Detonation Gun-Sprayed Coatings for Better Slurry and Cavitation Erosion Resistance, J. Therm. Spray Technol., 2019, 28(7), p 1565-157810.1007/s11666-019-00914-9 ↗
26. S. Hong, Y. Wu, J. Zhang, Y. Zheng, Y. Qin, W. Gao, and G. Li, Cavitation Erosion Behavior and Mechanism of HVOF SPRAYED WC-10Co-4Cr Coating in 3.5 wt% NaCl Solution, Trans. Indian Inst. Met., 2015, 68(1), p 151-15910.1007/s12666-014-0440-5 ↗
27. L. Qiao, Y. Wu, S. Hong, J. Zhang, W. Shi, and Y. Zheng, Relationships Between Spray Parameters, Microstructures and Ultrasonic Cavitation Erosion Behavior of HVOF Sprayed Fe-Based Amorphous/Nanocrystalline Coatings, Ultrason. Sonochem., 2017, 39, p 39-4610.1016/j.ultsonch.2017.04.011 ↗
28. S. Lavigne, F. Pougoum, S. Savoie, L. Martinu, J.E. Klemberg-Sapieha, and R. Schulz, Cavitation Erosion Behavior of HVOF CaviTec coatings, Wear, 2017, 386, p 90-9810.1016/j.wear.2017.06.003 ↗
29. J. Liu, T. Chen, C. Yuan, and X. Bai, Performance Analysis of Cavitation Erosion Resistance and Corrosion Behavior of HVOF-Sprayed WC-10Co-4Cr, WC-12Co, and Cr 3 C 2-NiCr Coatings, J. Therm. Spray Technol., 2020, 29, p 798-81010.1007/s11666-020-00994-y ↗
30. J. Ilavsky and J.K. Stalick, Phase Composition and Its Changes During Annealing of Plasma-Sprayed YSZ, Surf. Coat. Technol., 2000, 127(2), p 120-12910.1016/S0257-8972(00)00562-4 ↗
31. C.H. Lee and K.O. Min, Effects of Heat Treatment on the Microstructure and Properties of HVOF-Sprayed Ni-Cr–W–Mo–B alloy Coatings, Surf. Coat. Technol., 2000, 132(1), p 49-5710.1016/S0257-8972(00)00740-4 ↗
32. C. Zhang, G. Zhang, S. Leparoux, H. Liao, C.-X. Li, C.-J. Li, and C. Coddet, Microwave Sintering of Plasma-Sprayed Yttria Stabilized Zirconia Electrolyte Coating, J. Eur. Ceram. Soc., 2008, 28(13), p 2529-253810.1016/j.jeurceramsoc.2008.03.040 ↗
33. L. Janka, J. Norpoth, S. Eicher, M. Rodríguez Ripoll, and P. Vuoristo, Improving the Toughness of Thermally Sprayed Cr3C2-NiCr Hardmetal Coatings by Laser Post-treatment, Mater. Des., 2016, 98, p 135-14210.1016/j.matdes.2016.03.007 ↗
34. Y. Yuanzheng, Z. Youlan, L. Zhengyi, and C. Yuzhi, Laser Remelting of Plasma Sprayed Al2O3 Ceramic Coatings and Subsequent Wear Resistance, Mater. Sci. Eng. A, 2000, 291(1), p 168-17210.1016/S0921-5093(00)00983-7 ↗
35. Z. Bergant, U. Trdan, and J. Grum, Effect of High-Temperature Furnace Treatment on the Microstructure and Corrosion Behavior of NiCrBSi Flame-Sprayed Coatings, Corros. Sci., 2014, 88, p 372-38610.1016/j.corsci.2014.07.057 ↗
36. Y. Morisada, H. Fujii, T. Mizuno, G. Abe, T. Nagaoka, and M. Fukusumi, Modification of Thermally Sprayed Cemented Carbide Layer by Friction Stir Processing, Surf. Coat. Technol., 2010, 204(15), p 2459-246410.1016/j.surfcoat.2010.01.021 ↗
37. C. Huang, W. Li, Z. Zhang, M. Fu, M.-P. Planche, H. Liao, and G. Montavon, Modification of a Cold Sprayed SiCp/Al5056 Composite Coating by Friction Stir Processing, Surf. Coat. Technol., 2016, 296, p 69-7510.1016/j.surfcoat.2016.04.016 ↗
38. R.S. Mishra, Z.Y. Ma, and I. Charit, Friction Stir Processing: A Novel Technique for Fabrication of Surface Composite, Mater. Sci. Eng. A, 2003, 341(1), p 307-31010.1016/S0921-5093(02)00199-5 ↗
39. R.S. Mishra and Z.Y. Ma, Friction stir Welding and Processing, Mater. Sci. Eng. R Rep., 2005, 50(1), p 1-7810.1016/j.mser.2005.07.001 ↗
40. J.-Q. Su, T.W. Nelson, and C.J. Sterling, Friction stir Processing of Large-Area Bulk UFG Aluminum Alloys, Scr. Mater., 2005, 52(2), p 135-14010.1016/j.scriptamat.2004.09.014 ↗
41. H.S. Arora, H. Singh, and B.K. Dhindaw, Parametric Study of Friction Stir Processing of Magnesium-Based AE42 Alloy, J. Mater. Eng. Perform., 2012, 21(11), p 2328-233910.1007/s11665-012-0205-4 ↗
42. K.J. Hodder, H. Izadi, A.G. McDonald, and A.P. Gerlich, Fabrication of Aluminum–Alumina Metal Matrix Composites Via Cold Gas Dynamic Spraying at Low Pressure Followed by Friction Stir Processing, Mater. Sci. Eng. A, 2012, 556, p 114-12110.1016/j.msea.2012.06.066 ↗
43. T. Peat, A. Galloway, A. Toumpis, P. McNutt, and N. Iqbal, The Erosion Performance of Cold Spray Deposited Metal Matrix Composite Coatings with Subsequent Friction Stir Processing, Appl. Surf. Sci., 2017, 396, p 1635-164810.1016/j.apsusc.2016.10.156 ↗
44. T. Peat, A. Galloway, A. Toumpis, R. Steel, W. Zhu, and N. Iqbal, Enhanced Erosion Performance of Cold Spray Co-deposited AISI316 MMCs Modified by Friction Stir Processing, Mater. Des., 2017, 120, p 22-3510.1016/j.matdes.2017.01.099 ↗
45. C.B. Ponton and R.D. Rawlings, Vickers Indentation Fracture Toughness Test Part 1 Review of Literature and Formulation of Standardised Indentation Toughness Equations, Mater. Sci. Technol., 1989, 5(9), p 865-87210.1179/mst.1989.5.9.865 ↗
46. A.G. Evans and T.R. Wilshaw, Quasi-static solid particle damage in brittle solids—I. Observations analysis and implications, Acta Metall., 1976, 24(10), p 939-95610.1016/0001-6160(76)90042-0 ↗