Bond Strength of Multicomponent White Cast Iron Coatings Applied by HVOF Thermal Spray Process
Source abstract
Abstract
Multicomponent white cast iron is a new alloy that belongs to system Fe-C-Cr-W-Mo-V, and because of its excellent wear resistance it is used in the manufacture of hot rolling mills rolls. To date, this alloy has been processed by casting, powder metallurgy, and spray forming. The high-velocity oxyfuel process is now also considered for the manufacture of components with this alloy. The effects of substrate, preheating temperature, and coating thickness on bond strength of coatings have been determined. Substrates of AISI 1020 steel and of cast iron with preheating of 150 °C and at room temperature were used to apply coatings with 200 and 400 μm nominal thickness. The bond strength of coatings was measured with the pull-off test method and the failure mode by scanning electron microscopic analysis. Coatings with thickness of 200 μm and applied on substrates of AISI 1020 steel with preheating presented bond strength of 87 ± 4 MPa.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal Alloys Wear and Properties · High-Temperature Coating Behaviors · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. H.Q. Wu, N. Sasaguri, Y. Matsubara, and M. Hashimoto, Solidification of Multi-Alloyed White Cast Iron: Type and Morphology of Carbides, Trans. Am. Fish. Soc., 1996, 140, p 103-108
2. M. Boccalini, Jr., and H. Goldenstein, Solidification of High Speed Steels, Int. Mater. Rev., 2001, 46(2), p 92-11510.1179/095066001101528411 ↗
3. Y. Matsubara and M. Hashimoto, Metallurgical Aspect of Multi-Component White Cast Irons for Hot Rolling Mill Roll, Proceedings of the 44th MWSP Conference, 2002, Vol XL, p 23-31
4. A.H. Kasama, A.J. Mourisco, C.S. Kiminami, W.J. Bota Fo, and C. Bolfarini, Microstructure and Wear Resistance of Spray Formed High Chromium White Cast Iron, Mater. Sci. Eng. A, 2004, 375-377, p 589-59410.1016/j.msea.2003.10.093 ↗
5. T. Koseki, K. Ichino, and Y. Kataoka, Development of Centrifugal Cast Roll with High Wear Resistance for Finishing Stands of Hot Strip Mill, Kawasaki Steel Tech. Rep., 1997, 37, p 13-18
6. E. Lugscheider, H. Eschnauer, U. Muller, and T.H. Weber, Quo Vadis, Thermal Spray Technology, Powder Met. Int., 1991, 1(23), p 33-39
7. R.W. Smith and R. Novak, Advanced and Applications in U.S. Thermal Spray Technology, Powder Met. Int., 1991, 23(3), p 147-154
8. American Welding Society, Thermal Spraying Technology, Miami, 1985, p 184
9. J.R. Davis, Ed., Handbook of Thermal Spray Technology, ASM International, Materials Park, OH, 2004, p 338
10. M.L. Thorpe, Thermal Spray Industry in Transition, Adv. Mater. Processes, 1993, 5, p 50-61
11. R. Schwetzke and H. Kreye, Microstructure and Properties of Tungsten Carbide Coatings Sprayed with Various High-Velocity Oxygen Fuel Spray Systems, J. Therm. Spray Technol., 1999, 8(3), p 433-43910.1361/105996399770350395 ↗
12. O. Maranho, D. Rodrigues, M. Boccalini, Jr., and A. Sinatora, Influence of Parameters of the HVOF Thermal Spray Process on the Properties of Multicomponent White Cast Iron Coatings, Surf. Coat. Technol., 2008, 202, p 3494-350010.1016/j.surfcoat.2007.12.026 ↗
13. “Test Method for Adhesion or Cohesive Strength of Flame Sprayed Coatings,” C 633, ASTM, p 754-760
14. L. Pawlowski, The Science and Engineering of Thermal Spray Coatings, Wiley, New York, 1995, p 184
15. E. Bardal, P. Molde, and T.G. Eggen, Arc and Flame Sprayed Aluminium and Zinc Coatings on Mild Steel: Bond Strength, Surface Roughness, Structure and Hardness, Br. Corros. J., 1973, 8, p 15-1910.1179/000705973798322585 ↗
16. T.C. Totemeyer and J.K. Wright, Residual Stress Determination in Thermally Sprayed Coatings—A Comparison of Curvature Models and X-ray, Surf. Coat. Technol., 2006, 200, p 3955-396210.1016/j.surfcoat.2005.06.003 ↗
17. M.S.J. Hashmi, C. Pappalettere, and F. Ventola, Residual Stresses in Structures Coated by High Velocity Oxy-Fuel Technique, J. Mater. Process. Technol, 1998, 75, p 81-8610.1016/S0924-0136(97)00295-1 ↗
18. T.W. Clyne and S.C. Gill, Residual Stresses in Thermal Spray Coatings and Their Effect on Interfacial Adhesion: A Review of Recent Work, J. Therm. Spray Technol., 1996, 5(4), p 401-41810.1007/BF02645271 ↗
19. C. Godoy, E.A. Souza, M.M. Lima, and J.C.A. Batista, Correlation Between Stresses and Adhesion of Plasma Sprayed Coatings: Effects of a Post-Annealing Treatment, Thin Solid Films, 2002, 420-421, p 438-44510.1016/S0040-6090(02)00805-2 ↗
20. M. Vardelle, A. Vardelle, A.C. Leger, P. Fauchais, and D. Gobin, Influence of Particle Parameters at Impact on Splat Formation and Solidification in Plasma Spraying Processes, J. Therm. Spray Technol., 1994, 4(1), p 50-5810.1007/BF02648528 ↗
21. M. Parco, L. Zhao, J. Zwick, K. Bobzin, and E. Lugscheider, Investigation of Particle Flattening Behaviour and Bonding Mechanisms of APS Sprayed Coatings on Magnesium Alloys, Surf. Coat. Technol., 2007, 201, p 6290-629610.1016/j.surfcoat.2006.11.034 ↗
22. S. Sampath and X. Jiang, Splat Formation and Microstructure Development During Plasma Spraying: Deposition Temperature Effects, Mater. Sci. Eng. A, 2001, 304-306, p 144-15010.1016/S0921-5093(00)01464-7 ↗
23. V. Pershin, M. Lufitha, S. Chandra, and J. Mostaghimi, Effect of Substrate Temperature on Adhesion Strength of Plasma-Sprayed Nickel Coatings, J. Therm. Spray Technol., 2003, 12(3), p 370-37610.1361/105996303770348249 ↗
24. L. Li, X.Y. Wang, G. Wei, A. Vaidya, H. Zhang, and S. Sampath, Substrate Melting During Thermal Spray Splat Quenching, Thin Solid Films, 2004, 468, p 113-11910.1016/j.tsf.2004.05.073 ↗
25. J. Stokes and L. Looney, Residual Stress in HVOF Thermally Sprayed Thick Deposits, Surf. Coat. Technol., 2004, 177-178, p 18-2310.1016/j.surfcoat.2003.06.003 ↗
26. M. Mellali, P. Fauchais, and A. Grimaud, Influence of Substrate Roughness and Temperature on the Adhesion/Cohesion of Alumina Coatings, Surf. Coat. Technol., 1996, 81, p 275-28610.1016/0257-8972(95)02540-5 ↗