Thermally Sprayed Coatings as Interlayers for DLC-Based Thin Films
Source abstract
Abstract
This article examines the usefulness of a thick thermally sprayed interlayer (plasma-sprayed Ni-50%Cr, plasma-sprayed Al2O3-13%TiO2, or high-velocity oxygen-fuel-sprayed WC-17%Co) for enhancing the wear resistance and the corrosion protectiveness of a diamond-like carbon (DLC)-based thin film deposited onto a carbon steel substrate. Scratch tests indicate that the Al2O3-13%TiO2 and WC-17%Co interlayers definitely increase the critical spallation load of the thin film, but the Al2O3-13%TiO2 interlayer itself undergoes brittle fracture under high-contact loads. Accordingly, during ball-on-disk tests at room temperature, no cracking and spallation occur in the DLC-based film deposited onto the WC-17%Co interlayer, whereas the one onto the Al2O3-13%TiO2 interlayer is rapidly removed because the interlayer itself is fractured. At 300 °C, by contrast, the DLC-based film on the Al2O3-13%TiO2 interlayer offers the best tribological performance, possibly thanks to the increased toughness of the ceramic interlayer at this temperature. Electrochemical polarization tests indicate that the thin film/WC-Co systems possess the lowest corrosion current density.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. D.W. Wheeler, Chemical Vapour Deposition Methods for Protection against Wear, Surface Coatings for Protection against Wear, B.G. Mellor, Ed., Woodhead Publishing Limited, Abington Hall, Cambridge, England, 2006, p 129.
2. F.E. Kennedy, D. Lidhagen, A. Erdemir, J.B. Woodford, T. Kato, Tribological Behavior of Hard Carbon Coatings on Steel Substrates, Wear, 2003, 255, p 854–858.10.1016/S0043-1648(03)00223-0 ↗
3. G.A. Jones, On the Tribological Behaviour of Mechanical Seal Face Materials in Dry Line Contact: Part II. Bulk Ceramics, Diamond and Diamond-Like Carbon Films, Wear, 2004, 256, p 433–455.10.1016/S0043-1648(03)00540-4 ↗
4. A. Leyland, A. Matthews, On the Significance of the H/E Ratio in Wear Control: a Nanocomposite Coating Approach to Optimised Tribological Behaviour, Wear, 2000, 246, p 1–11.10.1016/S0043-1648(00)00488-9 ↗
5. K. Holmberg, A. Laukkanen, H. Ronkainen, K. Wallin, S. Varjus, J. Koskinen, Tribological Contact Analysis of a Rigid Ball Sliding on a Hard Coated Surface: Part II: Material Deformations, Influence of Coating Thickness and Young’s Modulus, Surf. Coat. Technol., 2006, 200, p 3810–3823.10.1016/j.surfcoat.2005.03.041 ↗
6. S.A.G. Oliveira, A.F. Bower, An Analysis of Fracture and Delamination in Thin Coatings Subjected to Contact Loading, Wear, 1996, 198, p 15–32.10.1016/0043-1648(95)06885-6 ↗
7. J. Jiang, R.D. Arnell, J. Tong, Some Special Tribological Features of DLC Coatings Deposited on Soft Substrates, Wear, 1997, 211, p 254–264.10.1016/S0043-1648(97)00126-9 ↗
8. B. Podgornik, J. Vižintin, Influence of Substrate Treatment on the Tribological Properties of DLC Coatings, Diamond Relat. Mater., 2001, 10, p 2232–2237.10.1016/S0925-9635(01)00514-3 ↗
9. Y. Liu, E.I. Meletis, Tribological Behavior of DLC Coatings with Functionally Gradient Interfaces, Surf. Coat. Technol., 2002, 153, p 178–183.10.1016/S0257-8972(01)01688-7 ↗
10. R. Gadow, D. Scherer, Composite Coatings with Dry Lubrication Ability on Light Metal Substrates, Surf. Coat. Technol., 2000, 151 –152, p 471–477.10.1016/S0257-8972(01)01636-X ↗
11. F. Casadei, R. Pileggi, R. Valle, A. Matthews, Studies on a Combined Reactive Plasma Sprayed/Arc Deposited Duplex Coating for Titanium Alloys, Surf. Coat. Technol., 2006, 201, p 1200–1206.10.1016/j.surfcoat.2006.01.066 ↗
12. E. Bemporad, M. Sebastiani, F. Casadei, F. Carassiti, Modelling, Production and Characterisation of Duplex Coatings (HVOF and PVD) on Ti–6Al–4 V Substrate for Specific Mechanical Applications, Surf. Coat. Technol., 2007, 201, p 7652–7662.10.1016/j.surfcoat.2007.02.041 ↗
13. X. Nie, A. Wilson, A. Leyland, A. Matthews, Deposition of Duplex Al2O3/DLC Coatings on Al Alloys for Tribological Applications Using a Combined Micro-Arc Oxidation and Plasma-Immersion Ion Implantation Technique, Surf. Coat. Technol., 2000, 131, p 506–513.10.1016/S0257-8972(00)00816-1 ↗
14. S.H. Awad, H.C. Qian, Deposition of Duplex Al2O3/TiN Coatings on Aluminum Alloys for Tribological Applications Using a Combined Microplasma Oxidation (MPO) and Arc Ion Plating (AIP), Wear, 2006, 260, p 215–222.10.1016/j.wear.2005.01.029 ↗
15. G. Bolelli, L. Lusvarghi, F. Pighetti Mantini, F. Pitacco, H. Volz, Enhanced Tribological Properties of PECVD DLC Coated Thermally Sprayed Coatings, Surf. Coat. Technol., 2008, 202, p 4382–4386.10.1016/j.surfcoat.2008.04.013 ↗
16. J.M. Guilemany, J. Nin, Thermal Spraying Methods for Protection against Wear, Surface Coatings for Protection against Wear, B.G. Mellor, Ed., Woodhead Publishing Limited, Abington Hall, Cambridge, England, 2006, p. 249.10.1533/9781845691561.249 ↗
17. H. Herman, S. Sampath, R. McCune, Thermal Spray: Current Status and Future Trends, MRS Bulletin, 2000, 25(7), p 17–25.10.1557/mrs2000.119 ↗
18. J.R. Davis, Handbook of Thermal Spray Technology, ASM International, Materials Park, OH, USA, 2004, p. 169.
19. G. Bolelli, V. Cannillo, L. Lusvarghi, T. Manfredini, Wear Behaviour of Thermally Sprayed Ceramic Oxide Coatings, Wear, 2006, 261, p 1298–1315.10.1016/j.wear.2006.03.023 ↗
20. G. Bolelli, V. Cannillo, L. Lusvarghi, S. Riccò, Mechanical and Tribological Properties of Electrolytic Hard Chrome and HVOF-Sprayed Coatings, Surf. Coat. Technol., 2006, 200, p 2995–3009.10.1016/j.surfcoat.2005.04.057 ↗
21. J. Jiang, R.D. Arnell, The Effect of Substrate Surface Roughness on the Wear of DLC Coatings, Wear, 2000, 239, p 1–9.10.1016/S0043-1648(99)00351-8 ↗
22. J. C. Lascovich, R. Giorgi, S. Scaglione, Evaluation of the sp2/sp3 Ratio in Amorphous Carbon Structure by XPS and XAES, Appl. Surf. Sci., 1991, 47, p 17–21.10.1016/0169-4332(91)90098-5 ↗
23. W.C. Oliver, G.M. Pharr, An Improved Technique for Determining Hardness and Elastic Modulus Using Load and Displacement Sensing Indentation Experiments, J. Mater. Res., 1992, 7, p 1564–1583.10.1557/JMR.1992.1564 ↗
24. S.J. Bull, Failure Modes in Scratch Adhesion Testing, Surf. Coat. Technol., 1991, 50, p 25–32.10.1016/0257-8972(91)90188-3 ↗
25. P.J. Burnett, D.S. Rickerby, The Mechanical Properties of Wear-Resistant Coatings : I: Modelling of Hardness Behaviour, Thin Solid Films, 1987, 148, p 41–50.10.1016/0040-6090(87)90119-2 ↗
26. J. Lesage, A. Pertuz, E.S. Puchi-Cabrera, D. Chicot, A Model to Determine the Surface Hardness of Thin Films from Standard Micro-Indentation Tests, Thin Solid Films, 2006, 497, p 232–238.10.1016/j.tsf.2005.09.194 ↗
27. G. Antou, G. Montavon, F. Hlawka, A. Cornet, C. Coddet, Exploring Thermal Spray Gray Alumina Coating Pore Network Architecture by Combining Stereological Protocols and Impedance Electrochemical Spectroscopy, J. Therm. Spray Technol., 2006, 15, p 765–772.10.1361/105996306X147045 ↗
28. G. Antou, G. Montavon, F. Hlawka, A. Cornet, C. Coddet, Characterizations of the Pore-Crack Network Architecture of Thermal-Sprayed Coatings, Mater. Charact., 2004, 53, p 361–372.10.1016/j.matchar.2004.08.015 ↗
29. K.H. Lau, K.Y. Li, Y-W. Mai, Influence of Hardness Ratio on Scratch Failure of Coatings, Int. J. Surf. Sci. Eng., 2007, 1, p 3–21.10.1504/IJSURFSE.2007.013618 ↗
30. J. Jiang, R.D. Arnell, J. Tong, The Effect of Substrate Properties on Tribological Behaviour of Composite DLC Coatings, Tribol. Int., 1997, 30, p 613–625.10.1016/S0301-679X(97)00035-2 ↗
31. D-H. Kim, H-E. Kim, K-R. Lee, C-N. Whang, I-S. Lee, Characterization of Diamond-Like Carbon Films Deposited on Commercially Pure Ti and Ti–6Al–4 V, Mater. Sci. Eng. C, 2002, 22, p 9–14.10.1016/S0928-4931(02)00106-6 ↗
32. E. Sánchez-González, P. Miranda, J.J. Meléndez-Martínez, F. Guiberteau, A. Pajares, Temperature Dependence of Mechanical Properties of Alumina up to the Onset of Creep, J. Eur. Ceram. Soc., 2007, 27, p 3345–3349.10.1016/j.jeurceramsoc.2007.02.191 ↗
33. A.A. Ashary, R.C. Tucker, Electrochemical Corrosion Studies of Alloys Plasma Sprayed with Cr2O3, Surf. Coat. Technol., 1989, 39–40, p 701–709.10.1016/S0257-8972(89)80032-5 ↗
34. M. Fukumoto, Y. Wada, M. Umemoto, I. Okane, Effect of Connected Pores on the Corrosion Behavior of Plasma Sprayed Alumina Coatings, Surf. Coat. Technol., 1989, 39–40, p 711–720.10.1016/S0257-8972(89)80033-7 ↗
35. G. Bolelli, V. Cannillo, R. Giovanardi, L. Lusvarghi, Electrochemical Comparison between Corrosion Resistance of some Thermally Sprayed Coatings, Int. J. Surf. Sci. Eng., 2008, 2(3–4), p 222–239.10.1504/IJSURFSE.2008.020495 ↗
36. T.E. Lister, R.N. Wright, P.J. Pinhero, W.D. Swank, Corrosion of Thermal Spray Hastelloy C-22 Coatings in Dilute HCl, J. Therm. Spray Technol., 2002, 11, p 530–535.10.1361/105996302770348664 ↗
37. D. Zhang, S.J. Harris, D.G. McCartney, Microstructure Formation and Corrosion Behaviour in HVOF-Sprayed Inconel 625 Coatings, Mater. Sci. Eng. A, 2003, 344, p 45–56.10.1016/S0921-5093(02)00420-3 ↗
38. G. Bolelli, R. Giovanardi, L. Lusvarghi, T. Manfredini, Corrosion Resistance of HVOF-Sprayed Coatings for Hard Chrome Replacement, Corros. Sci., 2006, 48, p 3375–3397.10.1016/j.corsci.2006.03.001 ↗
39. C. Monticelli, A. Frignani, F. Zucchi, Investigation on the Corrosion Process of Carbon Steel Coated by HVOF WC/Co Cermets in Neutral Solution, Corros. Sci., 2004, 46, p 1225–1237.10.1016/j.corsci.2003.09.013 ↗
40. A. Neville, T. Hodgkiess, Corrosion Behaviour and Microstructure of two Thermal Spray Coatings, Surf. Eng., 1996, 12, p 303–312.10.1179/sur.1996.12.4.303 ↗