Abstract

Fe-Si alloys are widely applied materials in industrial fields due to their magnetic properties. However, these alloys are difficult to manufacture due to the high oxidation affinity of Fe-Si alloys at high temperature; further, the permanence of the formed oxides (i.e., Fe2SiO4) degrade their workability. In order to solve this problem, disposable workability-improving ‘thick’ coating layers were deposited on Fe-Si alloy substrates in this study using plain carbon steel wire and pure Fe powder via thermal and kinetic spraying processes. The resulting deposits were compared in terms of microstructure and mechanical properties. In thermal sprayed deposit, the oxides degraded mechanical properties, but were helpful for the deposition of a thick layer by restraining bending by thermally induced tensile residual stress. On the other hand, kinetic sprayed deposit showed better adhesive bond strength owing to the compressive residual stress. After a post heating, it was observed that the type of oxides was not affected by diffusion of Si elements from the substrate due to the limited diffusion length of Si elements. Imperfect chemical/metallurgical bonding between the deposit and substrate was also observed. Further, mechanical properties of post heat-treated specimens were enhanced relative to the as-sprayed state.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metal Alloys Wear and Properties · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. H. Shimanaka, Y. Ito, K. Matsumura, and B. Fukuda, Recent Development of Non Oriented Electrical Steel Sheets, J. Magn. Magn. Mater., 1982, 26, p 57-6410.1016/0304-8853(82)90116-0 ↗
2. M. Takeda, T. Onishi, S. Nakakubo, and S. Fujimoto, Physical Properties of Iron-Oxide Scales on Si-Containing Steels at High Temperature, Mater. Trans., 2009, 50(9), p 2242-224610.2320/matertrans.M2009097 ↗
3. T. Tanda, T. Ichi, N. Morito, T. Irie, and H. Shimanaka, On Insulating Coatings Improving Punchability of Non-oriented Electrical Steel Sheets, Tetsu-to-Hagane, 1980, 66(7), p 1010-101610.2355/tetsutohagane1955.66.7_1010 ↗
4. H. Shimanaka, T. Irie, T. Tanda, and T. Ichi, Method of Improving Punchability of Steel Sheets, US Patent 3,666,568, May 30, 1972
5. X. Liu, P.K. Chu, and C. Ding, Surface Modification of Titanium, Titanium Alloys, and Related Materials for Biomedical Applications, Mater. Sci. Eng. R, 2004, 47, p 49-12110.1016/j.mser.2004.11.001 ↗
6. K. Spencer and M.-X. Zhang, The Emergence of Cold Spray as a Tool for Surface Modification, Key Eng. Mater., 2008, 384, p 61-7410.4028/www.scientific.net/KEM.384.61 ↗
7. K. Cooke, G. Oliver, V. Buchanan, and N. Palmer, Optimization of the Electric Wire Arc-Spraying Process for Improved Wear Resistance of Sugar Mill Roller Shells, Surf. Coat. Technol., 2007, 202, p 185-18810.1016/j.surfcoat.2007.05.015 ↗
8. D.L. Ruckle, Plasma-Sprayed Ceramic Thermal Barrier Coatings for Turbine Vane Platforms, Thin Solid Films, 1980, 73, p 455-46110.1016/0040-6090(80)90514-3 ↗
9. Y. Wang, S. Jiang, M. Wang, S. Wang, T. Xiao, and P.R. Strutt, Abrasive Wear Characteristics of Plasma Sprayed Nanostructured Alumina/Titania Coatings, Wear, 2000, 237, p 176-18510.1016/S0043-1648(99)00323-3 ↗
10. D.A. Stewart, P.H. Shipway, and D.C. McCartney, Abrasive Wear Behavior of Conventional and Nanocomposite HVOF-sprayed WC-Co Coatings, Wear, 1999, 225-229, p 789-79810.1016/S0043-1648(99)00032-0 ↗
11. D. Zhang, S.J. Harris, and D.G. McCartney, Microstructure Formation and Corrosion Behavior in HVOF-sprayed Inconel 627 Coatings, Mater. Sci. Eng. A, 2003, 344, p 45-5610.1016/S0921-5093(02)00420-3 ↗
12. F.F. Khan, G. Bae, K. Kang, T. Jeong, and C. Lee, Development of Cermet Coatings by Kinetic Spray Technology for the Application of Die-Soldering and Erosion Resistance, Surf. Coat. Technol., 2009, 204, p 345-35210.1016/j.surfcoat.2009.07.033 ↗
13. J.R. Davis and Davis & Associates, Handbook of Thermal Spray Technology, 2004
14. L. Pawlowski, The Science and Engineering of Thermal Spray Coatings, John Wiley & Sons Ltd., Hoboken, 1995
15. G. Bae, S. Kumar, S. Yoon, K. Kang, H. Na, H. Kim, and C. Lee, Bonding Features and Associated Mechanisms in Kinetic Sprayed Titanium Coatings, Acta Mater., 2009, 57, p 5654-566610.1016/j.actamat.2009.07.061 ↗
16. S. Sampath, X.Y. Jiang, J. Matejicek, L. Prchlik, A. Kulkarni, and A. Vaidya, Role of Thermal Spray Processing Method on the Microstructure, Residual Stress and Properties of Coatings: An Integrated Study for Ni-5 wt.% Al Bond Coats, Mater. Sci. Eng. A, 2004, 364, p 216-23110.1016/j.msea.2003.08.023 ↗
17. B. Vrancken, R. Wauthle, J.-P. Kruth, and J.V. Humbeeck, Study of Influence of Material Properties on Residual Stress in Selective Laser Melting, Lirias KU Leuven, 2013, p 393-407
18. W.D. Callister and D.G. Rethwisth, Fundamentals of Materials Science and Engineering, John Wiley & Sons Ltd., New York, 2008
19. V.V. Sobelev and J.M. Guilemany, Effect of Oxidation on Droplet Flattening and Splat-Substrate Interaction in Thermal Spraying, J. Therm. Spray Technol., 1999, 8(4), p 523-53010.1361/105996399770350205 ↗
20. ASTM C633-79, Standard Test Method for Adhesion or Cohesive Strength of Flame-sprayed Coatings, Annual Book of ASTM Standard, American Society for Testing and Materials, West Conshohocken, 1982
21. M. Grujicic, J.R. Saylor, D.E. Beasley, W.S. DeRosset, and D. Helfritch, Computational Analysis of the Interfacial Bonding Between Feed-powder Particles and the Substrate in the Cold-Gas Dynamic-Spray Process, Appl. Surf. Sci., 2003, 219, p 211-22710.1016/S0169-4332(03)00643-3 ↗
22. H. Assadi, F. Gartner, T. Stoltenhoff, and H. Kreye, Bonding Mechanism in Cold Gas Spraying, Acta Mater., 2003, 51, p 3494-437910.1016/S1359-6454(03)00274-X ↗
23. T. Adachi and G.H. Meier, Oxidation of Iron-Silicon Alloys, Oxid. Met., 1987, 27, p 347-36610.1007/BF00659276 ↗
24. A. Atkinson, A Theoretical Analysis of the Oxidation of Fe-Si Alloys, Corros. Sci., 1982, 22(2), p 87-10210.1016/0010-938X(82)90071-3 ↗
25. H.-D. Steffens, B. Wielage, and J. Drozak, Interface Phenomena and Bonding Mechanism of Thermally-Sprayed Metal and Ceramic Composites, Surf. Coat. Technol., 1991, 45, p 299-30810.1016/0257-8972(91)90236-P ↗
26. T. Hussain, D.G. McCartney, P.H. Shipway, and D. Zhang, Bonding Mechanisms in Cold Spraying: The Contributions of Metallurgical and Mechanical Components, J. Therm. Spray Technol., 2009, 18(3), p 364-37910.1007/s11666-009-9298-1 ↗
27. N.M. Chavan, M. Ramakrishna, P.S. Phani, D.S. Rao, and G. Sundararajan, The Influence of Process Parameters and Heat Treatment on the Properties of Cold Sprayed Silver Coatings, Surf. Coat. Technol., 2011, 205, p 4798-480710.1016/j.surfcoat.2011.04.063 ↗