journal article·2025-02

Wear Characteristics of Thermally Sprayed Diamond-Reinforced Ni-P Coatings

Akshay R. Govande, Subrat Kumar Baral, Ravikumar Dumpala, Shrikant Joshi

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Electrodeposition and Electroless Coatings · Diamond and Carbon-based Materials Research · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. M. Rossetti, S. Mathiyalagan, S. Björklund, S. Sowers, and S. Joshi, Advanced Diamond-Reinforced Metal Matrix Composite (DMMC) Coatings Via HVAF Process: Effect of Particle Size and Nozzle Characteristics on Tribological Properties, Ceram. Int. Int., 2023, 49, p 17838-17850.10.1016/j.ceramint.2023.02.150 ↗
2. B. Yang, W. Lu, W. Feng, X. Yang, and D. Zuo, Adsorption and Deposition of Micro Diamond Particles in Preparing Diamond Magnetic Abrasives by Electroless Composite Plating, Diam. Related Mater., 2017, 73, p 137-142.10.1016/j.diamond.2016.08.015 ↗
3. O. Kovarik, J. Cizek, S. Yin, R. Lupoi, M. Janovska, J. Cech, J. Capek, J. Siegl, and T. Charska, Mechanical and Fatigue Properties of Diamond-Reinforced Cu and Al Metal Matrix Composites Prepared by Cold Spray, J. Therm. Spray Technol. Therm. Spray Technol., 2022, 31, p 217-233.10.1007/s11666-022-01321-3 ↗
4. K. Venkateswarlu, A.K. Ray, M.K. Gunjan, D.P. Mondal, and L.C. Pathak, Tribological Wear Behavior of Diamond Reinforced Composite Coating, Mater. Sci. Eng. A, 2006, 418, p 357-363.10.1016/j.msea.2005.12.004 ↗
5. A.F. Richardson, A. Neville, and J.I.B. Wilson, Developing Diamond MMCs to Improve Durability in Aggressive Abrasive Conditions, Wear, 2003, 255, p 593-605.10.1016/S0043-1648(03)00049-8 ↗
6. K. Venkateswarlu, V. Rajinikanth, T. Naveen, D.P. Sinha, and A.K. Ray, Abrasive Wear Behavior of Thermally Sprayed Diamond Reinforced Composite Coating Deposited with Both Oxy-Acetylene and HVOF Techniques, Wear, 2009, 266, p 995-1002.10.1016/j.wear.2009.02.001 ↗
7. L. Yang, B. Li, J. Yao, and Z. Li, Effects of diamond size on the deposition characteristic and tribological behavior of diamond/Ni60 composite coating prepared by supersonic laser deposition, Diam. Related Mater., 2015, 58, p 139-148.10.1016/j.diamond.2015.06.014 ↗
8. J. Yao, L. Yang, B. Li, and Z. Li, Beneficial effects of laser irradiation on the deposition process of diamond/Ni60 composite coating with cold spray, Appl. Surf. Sci., 2015, 330, p 300-308.10.1016/j.apsusc.2015.01.029 ↗
9. J. Wang, F.-L. Zhang, T. Zhang, W.-G. Liu, W.-X. Li, and Y.-M. Zhou, Preparation of Ni-P-Diamond Coatings with Dry Friction Characteristics and Abrasive Wear Resistance, Int. J. Refract. Metals Hard Mater., 2018, 70, p 32-38.10.1016/j.ijrmhm.2017.09.012 ↗
10. R.K. Gautam, V.M. Tripathi, S. Singhania, S. Mishra, P. Jha, A.K. Singh, N. Gariya, S. Shahab, and H. Nautiyal, Evaluation of Tribological Characteristics of Atmospheric Plasma Spray Deposited Ni-Based Coatings, J. Therm. Spray Technol., 2024, 33, p 1-5.10.1007/s11666-024-01771-x ↗
11. A.K. Grain, O.S.A. Rahman, S. Kumari, S.S. Maurya, K.V. Kumar, A. Islam, S.K. Gosh, and A.K. Keshri, Plasma-Sprayed Nanodiamond-Reinforced NiCrBSi Composite Coating for Improved Wear and Corrosion Resistance, J. Therm. Spray Technol., 2024, 33, p 1-20.10.1007/s11666-024-01729-z ↗
12. M. Petrova, M. Georgieva, V. Chakarova, and E. Dobreva, Electroless Deposition of Composite Nickel-Phosphorous Coatings with Diamond Dispersoid, Arch. Metall. Mater., 2016, 61, p 493-498.10.1515/amm-2016-0086 ↗
13. M. Petrova, Z. Noncheva and E. Dobreva, Electroless Deposition of Diamond Powder Dispersed Nickel-Phosphorus Coatings on Steel Substrate, Trans. IMF, 2011, 89, p 89-94.10.1179/174591911X12971865404438 ↗
14. M. Abdoli and A. SabourRouhaghdam, Preparation and Characterization of Ni-P/nanodiamond Coatings: Effects of Surfactants, Diam. Related Mater., 2013, 31, p 30-37.10.1016/j.diamond.2012.10.003 ↗
15. K.U.V. Kiran, A. Arora, B.R. Sunil, and R. Dumpala, Effect of Heat Treatment on the Temperature Dependent Wear Characteristics of Electroless Ni-P-BN(h) Composite Coatings, SN Appl. Sci., 2020, 2, p 1101.10.1007/s42452-020-2920-z ↗
16. A.R.K. Rana and Z. Farhat, Preparation and Tribological Characterization of Graphene Incorporated Electroless Ni-P Composite Coatings, Surf. Coat. Technol., 2019, 369, p 334-346.10.1016/j.surfcoat.2019.04.043 ↗
17. Y. Zhang, L. Feng, and W. Qiu, Enhancement of the Wear Resistance of Ni-Diamond Composite Coatings Via Glycine Modification, Diam. Related Mater., 2020, 109, p 108086.10.1016/j.diamond.2020.108086 ↗
18. S. Mathiyalagan, M. Rossetti, S. Björklund, S. Basu, N.J. Balila, S. Sowers, and S. Joshi, Deposition Characteristics and Tribological Performance of Atmospheric Plasma Sprayed Diamond Metal Matrix Composite (DMMC) Coatings, Mater. Chem. Phys., 2024, 315, p 128920.10.1016/j.matchemphys.2024.128920 ↗
19. E.J. Ekoi and D.P. Dowling, Evaluation of the Microstructure, Mechanical and Tribological Properties of Nickel-Diamond Nanocomposite Coatings, Diam. Related Mater., 2019, 94, p 118-128.10.1016/j.diamond.2019.02.026 ↗
20. W. Tillmann, A. Brinkhoff, C. Schaak, and J. Zajaczkowski, Self-Sharpening-Effect of Nickel-Diamond Coatings Sprayed by HVOF, IOP Conf. Ser.: Mater. Sci. Eng., 2017, 181, p 012016.10.1088/1757-899X/181/1/012016 ↗
21. K.A. Weidenmann, R. Tavangar, and L. Weber, Mechanical behaviour of diamond reinforced metals, Mater. Sci. Eng. A, 2009, 523, p 226-234.10.1016/j.msea.2009.05.069 ↗
22. S. Mahade, A. Mulone, S. Björklund, U. Klement, and S. Joshi, Investigating Load-Dependent Wear Behavior and Degradation Mechanisms in Cr3C2-NiCr Coatings Deposited by HVAF and HVOF, J. Mater. Res. Technol., 2021, 15, p 4595-4609.10.1016/j.jmrt.2021.10.088 ↗
23. A.R. Govande, A. Chandak, B.R. Sunil, and R. Dumpala, Carbide-Based Thermal Spray Coatings: A Review on Performance Characteristics and Post-Treatment, Int. J. Refract. Metals Hard Mater., 2022, 103, p 105772.10.1016/j.ijrmhm.2021.105772 ↗
24. S. Joshi and P. Nylen, Advanced Coatings by Thermal Spray Processes, Technologies, 2019, 7(4), p 79.10.3390/technologies7040079 ↗
25. V.S. Gorelik and A.Y. Pyatyshev, Raman scattering in diamond nano- and microcrystals, synthesized at high temperatures and high pressures, Diam. Related Mater., 2020, 110, p 108104.10.1016/j.diamond.2020.108104 ↗
26. T.R. Tamilarasan, R. Rajendran, M. Siva shankar, U. Sanjith, G. Rajagopal, and J. Sudagar, Wear and Scratch Behaviour of Electroless Ni-P-Nano-TiO2: Effect of Surfactants, Wear, 2016, 346-347, p 148-157.10.1016/j.wear.2015.11.015 ↗
27. A. Dychalska, P. Popielarski, W. Franków, K. Fabisiak, K. Paprocki, and M. Szybowicz, Study of CVD Diamond Layers with Amorphous Carbon Admixture by Raman Scattering Spectroscopy, Mater. Sci. Pol., 2015, 33, p 799-805.10.1515/msp-2015-0067 ↗
28. S. Mathiyalagan, M. Rossetti, S. Björklund, S. Sowers, T. Dumm, C. Kim, and S. Joshi, High Velocity Air Fuel (HVAF) Spraying of Nickel Phosphorus-Coated Cubic-Boron Nitride Powders for Realizing High-Performance Tribological Coatings, J. Mater. Res. Technol., 2022, 18, p 59-74.10.1016/j.jmrt.2022.02.058 ↗
29. W. Riedel, Electroless Nickel Plating. Metal Finishing. 1997, p. 101
30. R. Duncan, The Metallurgical Structure of Electroless Nickel Deposits: Effect on Coating Properties, Plat. Surf. Finish., 1996, 83, p 65-69.
31. K.G. Keong, W. Sha, and S. Malinov, Hardness Evolution of Electroless Nickel-Phosphorus Deposits with Thermal Processing, Surf. Coat. Technol., 2003, 168, p 263-274.10.1016/S0257-8972(03)00209-3 ↗
32. J. Sudagar, J. Lian, and W. Sha, Electroless Nickel, Alloy, Composite and Nano Coatings—A Critical Review, J. Alloys Comp., 2013, 571, p 183-204.10.1016/j.jallcom.2013.03.107 ↗
33. M. Buchtík, M. Krystýnová, J. Másilko, and J. Wasserbauer, The Effect of Heat Treatment on Properties of Ni-P Coatings Deposited on a AZ91 Magnesium Alloy, Coatings, 2019, 9(7), p 461.10.3390/coatings9070461 ↗
34. C.A. León-Patiño, J. García-Guerra, and E.A. Aguilar-Reyes, Tribological Characterization of Heat-Treated Ni-P and Ni-P-Al2O3 Composite Coatings by Reciprocating Sliding Tests, Wear, 2019, 426-427, p 330-340.10.1016/j.wear.2019.02.015 ↗
35. B. Chen, J. Guo, M.F. Yan, F. Wang, and F. Liu, Study on a Ni-P-Nano TiN Composite Coating for Significantly Improving the Service Life of Copper Alloy Synchronizer Rings, Appl. Surf. Sci., 2020, 504, p 144116.10.1016/j.apsusc.2019.144116 ↗
36. H.-C. Huang, S.-T. Chung, S.-J. Pan, W.-T. Tsai, and C.-S. Lin, Microstructure evolution and hardening mechanisms of Ni-P electrodeposits, Surf. Coat. Technol., 2010, 205, p 2097-2103.10.1016/j.surfcoat.2010.08.115 ↗
37. O.A. León, M.H. Staia, and H.E. Hintermann, High Temperature Wear of an Electroless Ni-P-BN (h) Composite Coating, Surf. Coat. Technol., 2003, 163-164, p 578-584.10.1016/S0257-8972(02)00663-1 ↗
38. J.H. Liu, Y.D. Liu, Z.L. Pei, W.H. Li, W.B. Shi, J. Gong, and C. Sun, Influence of Particle Size and Content on the Friction and Wear Behaviors of as-Annealed Ni-Mo/Diamond Composite Coatings, Wear, 2020, 452-453, p 203300.10.1016/j.wear.2020.203300 ↗
39. A. Mukhopadhyay, T.K. Barman, and P. Sahoo, Co-Deposition of W and Mo in Electroless Ni-B Coating and Its Effect on the Surface Morphology, Structure, and Tribological Behavior, Proc. Inst. Mech. Eng., Part L: J. Mater.: Des. Appl., 2021, 235, p 149-161.10.1177/1350650120929501 ↗
40. Q. Hong, R. Zhou, X. Guo, Z. Wang, and S. Yin, A novel strategy for improving the wear resistance of electrodeposited Ni-diamond composite coatings by diamond surface morphology modification, Diam. Related Mater., 2023, 137, p 110093.10.1016/j.diamond.2023.110093 ↗
41. P. Sahoo and S.K. Das, Tribology of Electroless Nickel Coatings—A Review, Mater. Des., 2011, 32, p 1760-1775.10.1016/j.matdes.2010.11.013 ↗
42. Y.Y. Liu, J. Yu, H. Huang, B.H. Xu, X.L. Liu, Y. Gao, and X.L. Dong, Synthesis and Tribological Behavior of Electroless Ni-P-WC nanocomposite Coatings, Surf. Coat. Technol., 2007, 201, p 7246-7251.10.1016/j.surfcoat.2007.01.035 ↗
43. F. Wu, N. Liu, Y. Ma, X. Zhang, and Y. Han, Research on the influence of diamond coating microtexture on graphitization law and friction coefficient, Diam. Related Mater., 2022, 127, p 109153.10.1016/j.diamond.2022.109153 ↗
44. A. Aminzadeh and H. Sarikhani-fard, Raman Spectroscopic Study of Ni/Al2O3 Catalyst, Spectrochim. Acta Part A Mol. Biomol. Spectrosc., 1999, 55, p 1421-1425.10.1016/S1386-1425(98)00312-6 ↗
45. G. Hasemann, U. Betke, M. Krüger, H. Walles, and M. Scheffler, Refractory Metal Coated Alumina Foams as Support Material for Stem Cell and Fibroblasts Cultivation, Materials, 2021, 14(11), p 2813.10.3390/ma14112813 ↗
46. J.H. Liu, Z.L. Pei, W.B. Shi, Y.D. Liu, J. Gong, and C. Sun, Studies on Preparation, Microstructure, Mechanical Properties and Corrosion Resistance of NiMo/Micron-Sized Diamond Composite Coatings, Surf. Coat. Technol., 2020, 385, p 125451.10.1016/j.surfcoat.2020.125451 ↗