journal article·2013-11

Nonoxidative thermal degradation kinetic of polyamide 6,6 reinforced with carbon nanotubes

B Ribeiro, LB Nohara, SS Oishi, ML Costa, EC Botelho

Publisher page

Abstract

The thermal degradation of the polyamide 6,6 (abbreviated henceforth as PA 6,6) reinforced with different concentrations of carbon nanotubes (CNTs) was investigated by means of thermal analysis. In this study, the nanostructured composites were produced using 0.1, 0.5 and 1.0 wt% of CNT. X-ray diffraction analyses were performed in order to evaluate the crystallographic properties of nanostructured composite. The degradation kinetics of PA 6,6/CNT nanostructured composites were measured by thermogravimetric analysis at different heating rates under nitrogen flow. TGA experiments were performed to elucidate the thermal behavior and supply the data that characterize the degradation kinetic. The degradation parameter kinetics was determined using the Ozawa–Wall–Flynn (O-W-F) methods, which do not require knowledge of the reaction mechanism. In this work, the results show that the addition of CNT up to the amount of 0.5 wt% increases the thermal stability of PA 6,6.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Polymer Nanocomposites and Properties · Carbon Nanotubes in Composites · Polymer crystallization and properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Materials and Technology, São Paulo State University, Guaratinguetá, São Paulo, Brazil

Materials Division, Department of Aerospace Science and Technology, Institute of Aeronautics and Space, São José dos Campos, São Paulo, Brazil

References (31)

Show source-provided references
1. 10.1002/mren.20070002010.1002/mren.200700020 ↗
2. 10.1002/pol.1969.16007060710.1002/pol.1969.160070607 ↗
3. 10.1016/j.polymer.2006.01.07710.1016/j.polymer.2006.01.077 ↗
4. 10.1016/S0043-1648(01)00794-310.1016/S0043-1648(01)00794-3 ↗
5. 10.1021/ed065p80310.1021/ed065p803 ↗
6. Billmeyer Jr · 1984
7. Selley I · 1985
8. Kohan MI · 1995
9. Kumar A · 1998
10. 10.1002/pen.76033220610.1002/pen.760332206 ↗
11. 10.1016/j.polymer.2004.09.07410.1016/j.polymer.2004.09.074 ↗
12. 10.1002/pi.192010.1002/pi.1920 ↗
13. 10.1007/s10973-009-0426-410.1007/s10973-009-0426-4 ↗
14. 10.1016/j.polymdegradstab.2007.12.01210.1016/j.polymdegradstab.2007.12.012 ↗
15. Kim JY · Poly (butyilene therephthalate) nanocomposites containing carbon nanotubes, advances in nanocomposites—synthesis, characterization and industrial applications, InTech · 2011 · 707
16. 10.1002/1521-3927(20020901)23:13<761::AID-MARC761>3.0.CO;2-K10.1002/1521-3927(20020901)23:13<761::AID-MARC761>3.0.CO;2-K ↗
17. 10.1016/S0141-3910(03)00061-210.1016/S0141-3910(03)00061-2 ↗
18. 10.1007/s10853-006-0011-110.1007/s10853-006-0011-1 ↗
19. 10.1016/j.polymdegradstab.2005.08.01210.1016/j.polymdegradstab.2005.08.012 ↗
20. 10.1016/S0045-6535(00)00233-210.1016/S0045-6535(00)00233-2 ↗
21. 10.1016/S0141-3910(99)00155-X10.1016/S0141-3910(99)00155-X ↗
22. 10.1016/j.polymdegradstab.2007.12.01210.1016/j.polymdegradstab.2007.12.012 ↗
23. 10.1016/j.polymdegradstab.2006.11.00410.1016/j.polymdegradstab.2006.11.004 ↗
24. 10.1016/S0141-3910(02)00041-110.1016/S0141-3910(02)00041-1 ↗
25. 10.1016/j.polymdegradstab.2005.04.03710.1016/j.polymdegradstab.2005.04.037 ↗
26. Huadong W · Polym Degrad Stabil · 2003 · 83 · 229
27. ASTM-E1641 · 1999
28. ASTM-E1877 · 1999
29. 10.1590/S0100-4042201000010002510.1590/S0100-40422010000100025 ↗
30. 10.1021/ma060733p10.1021/ma060733p ↗
31. 10.1080/0360255050037361810.1080/03602550500373618 ↗