journal article·2016-11

Effect of long time exposure on the chemical and physical properties of polyvinyl chloride/titanium dioxide nanocomposites

Shadi Ghaebi Mehmandoust, Parvane Sokhandani, Mohammad Adel Abdi, Ali Akbar Babaluo, Reza Alizadeh

Publisher page

Abstract

The photodegradation behavior of poly(vinyl chloride) (PVC) nanocomposites containing different amounts of synthesized titanium dioxide (TiO 2 ) nanoparticles and commercial rutile powder is investigated via the formation of carbonyl compounds, peroxides, and polyenes propagation over 5112 h exposure, as a function of irradiation wavelength and intensity. All the PVC/TiO 2 nanocomposites are found to exhibit lower concentration of mentioned species compared with the composite samples. The results show that added TiO 2 nanoparticles can retard the photodegradation processes, wherein increasing the amounts of these nanoparticles yields more reduction. With an increase in irradiation intensity the rate of formation of investigated groups increases, although in cases with raised temperature range, this pattern is not observed. An evaluation on the irradiation wavelength effect also shows that more photon energy provides more degradation. The loss of weight analysis shows a tremendous and novel result on evaluating a point of meaningful weight loss.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Polymer Science and PVC · Polymer Nanocomposites and Properties · Polymer Nanocomposite Synthesis and Irradiation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Nanostructure Materials Research Center, Department of Chemical Engineering, Sahand University of Technology, Tabriz, Islamic Republic of Iran

Chemical Engineering Department, Sahand University of Technology, Tabriz, Islamic Republic of Iran

References (37)

Show source-provided references
1. 10.1016/S0141-3910(02)00286-010.1016/S0141-3910(02)00286-0 ↗
2. 10.1016/S0141-3910(03)00202-710.1016/S0141-3910(03)00202-7 ↗
3. 10.1016/S0160-791X(01)00013-610.1016/S0160-791X(01)00013-6 ↗
4. 10.1016/j.polymdegradstab.2007.11.00810.1016/j.polymdegradstab.2007.11.008 ↗
5. 10.1016/j.polymertesting.2008.05.00910.1016/j.polymertesting.2008.05.009 ↗
6. 10.1016/0144-2880(82)90040-910.1016/0144-2880(82)90040-9 ↗
7. 10.1016/0144-2880(82)90029-X10.1016/0144-2880(82)90029-X ↗
8. 10.1016/0144-2880(86)90039-410.1016/0144-2880(86)90039-4 ↗
9. 10.1002/vnl.2003410.1002/vnl.20034 ↗
10. 10.1023/A:102114820536610.1023/A:1021148205366 ↗
11. 10.1007/s10924-009-0152-910.1007/s10924-009-0152-9 ↗
12. 10.1016/0014-3057(92)90089-K10.1016/0014-3057(92)90089-K ↗
13. 10.1002/polb.2034110.1002/polb.20341 ↗
14. 10.1016/S1010-6030(01)00499-310.1016/S1010-6030(01)00499-3 ↗
15. 10.1016/j.molcata.2006.12.01210.1016/j.molcata.2006.12.012 ↗
16. 10.1016/0141-3910(91)90031-L10.1016/0141-3910(91)90031-L ↗
17. 10.1016/0141-3910(90)90023-Z10.1016/0141-3910(90)90023-Z ↗
18. Ye X · J Appl Polym Sci · 2010 · 117 · 289910.1002/app.32214 ↗
19. Kubacka A · 2012 · 119
20. 10.1002/app.3898910.1002/app.38989 ↗
21. 10.1002/app.4022810.1002/app.40228 ↗
22. 10.1016/0144-2880(84)90037-X10.1016/0144-2880(84)90037-X ↗
23. 10.1016/0014-3057(82)90209-910.1016/0014-3057(82)90209-9 ↗
24. 10.1023/A:100448232820310.1023/A:1004482328203 ↗
25. 10.1016/S0141-3910(99)00033-610.1016/S0141-3910(99)00033-6 ↗
26. 10.1002/app.1976.07020121310.1002/app.1976.070201213 ↗
27. 10.1021/ac60207a06110.1021/ac60207a061 ↗
28. 10.1021/ma60012a00710.1021/ma60012a007 ↗
29. 10.1016/0141-3910(87)90090-510.1016/0141-3910(87)90090-5 ↗
30. 10.1007/s10965-005-9034-610.1007/s10965-005-9034-6 ↗
31. 10.1016/S0141-3910(97)00077-310.1016/S0141-3910(97)00077-3 ↗
32. 10.1016/0014-3057(75)90106-810.1016/0014-3057(75)90106-8 ↗
33. 10.1002/pola.1992.08030031610.1002/pola.1992.080300316 ↗
34. 10.1002/ceat.20100045010.1002/ceat.201000450 ↗
35. 10.1002/app.1993.07048110210.1002/app.1993.070481102 ↗
36. 10.1016/0144-2880(81)90021-X10.1016/0144-2880(81)90021-X ↗
37. Wright D. Failure of plastics and rubber products: causes, effects and case studies involving degradation. Billingham: Rapra Technology, 2006, pp.75–90.