The physico-mechanical properties of γ-irradiated ethylene propylene diene rubber/high styrene butadiene rubber nanocomposites
Source abstract
Abstract
The mechanical properties of γ-irradiated ethylene propylene diene monomer (EPDM)/high styrene-butadiene rubber (HSBR) blends were investigated with special reference to the effects of blend ratio. Among the blends, the one with 80/20 EPDM/HSBR has been found to exhibit the highest tensile, hardness, thermal, and abrasion properties. The effect of γ-irradiation dose on the mechanical properties namely tensile strength and elongation at break was investigated. The effect of silane coupling agent on the mentioned properties of the EPDM/HSBR blend was studied. The results showed that the mechanical and the thermal properties of the γ-irradiated EPDM/HSBR blend improved with the addition of the silane coupling agent due to the increase in the cross-linking density. The inclusion of both the 30 phr fumed silica and N, N- m-phenylenedimaleimide coagent in the 80/20 EPDM/HSBR nanocomposite irradiated to 150 kGy leads to a synergistic effect. Thermogravimetric analysis was carried out to analyze the thermal stability of the nanocomposites. The mechanical properties have been interpreted in terms of the morphology of the blends as attested by scanning electron microscope.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Polymer Nanocomposites and Properties · Polymer Nanocomposite Synthesis and Irradiation · Silicone and Siloxane Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
National Center for Radiation Research and Technology (NCRRT), Egyptian Atomic Energy Authority, Nasr City, Cairo, Egypt
References (25)
Show source-provided references
1. 10.1016/j.matdes.2003.11.00310.1016/j.matdes.2003.11.003 ↗
2. 10.1016/j.clay.2015.02.01210.1016/j.clay.2015.02.012 ↗
3. 10.1016/j.compositesb.2012.05.02010.1016/j.compositesb.2012.05.020 ↗
4. 10.1007/s10118-013-1262-310.1007/s10118-013-1262-3 ↗
5. 10.1166/jnn.2010.234810.1166/jnn.2010.2348 ↗
6. Dunn JR, Wall DW. Presented at a Meeting of the Rubber Division, Am Chem Soc. Las Vegas, Nevada, Paper No. 48, 27 May-1 June 1990.
7. 10.1007/s12633-018-9836-x10.1007/s12633-018-9836-x ↗
8. 10.1002/app.2066910.1002/app.20669 ↗
9. 10.1002/app.2276510.1002/app.22765 ↗
10. Dubey KA, Bhardwaj YK, Chaudhari C, et al. Role of blend morphology in the radiation processing of SBR-EPDM blendes. BARC newsletter Founder’s Day Issue no. 273, 2006, 92–102.
11. 10.1002/polb.2082210.1002/polb.20822 ↗
12. Dubey KA · IAEA, INIS · 2011 · 45 · 88
13. 10.1016/j.matdes.2009.07.02310.1016/j.matdes.2009.07.023 ↗
14. 10.1016/j.matdes.2009.08.01410.1016/j.matdes.2009.08.014 ↗
15. 10.1002/pi.97510.1002/pi.975 ↗
16. Schawaiger B · Rubber World · 2000 · 222 · 32
17. 10.1007/s00289-015-1411-710.1007/s00289-015-1411-7 ↗
18. Mohamed M · J Vinyl Add · 2017 · 23 · 188
19. Mohamed M · J Rad Sci Applic · 2015 · 28 · 169
20. 10.1002/(SICI)1099-0488(19970730)35:10<1501::AID-POLB4>3.0.CO;2-U10.1002/(SICI)1099-0488(19970730)35:10<1501::AID-POLB4>3.0.CO;2-U ↗
21. 10.1002/vnl.73009020910.1002/vnl.730090209 ↗
22. 10.1177/0307174X040310080310.1177/0307174X0403100803 ↗
23. 10.1016/S0141-3910(99)00133-010.1016/S0141-3910(99)00133-0 ↗
24. 10.1016/j.apt.2013.10.01610.1016/j.apt.2013.10.016 ↗
25. 10.1016/S0141-3910(02)00361-010.1016/S0141-3910(02)00361-0 ↗