Study on the electrical and rheological percolation threshold of single-walled carbon nanotube-reinforced thermoplastic elastomer based on polypropylene/ethylene–propylene–diene monomer nanocomposite
Source abstract
Abstract
The rheological and electrical percolation threshold of single-walled carbon nanotube (SWNT)-reinforced thermoplastic elastomer based on polypropylene/ethylene–propylene–diene monomer (PP/EPDM; 80/20) nanocomposite was investigated by melt-mixing process. The rheological properties revealed that the addition of SWNT increased the shear stress and shear viscosity. Both PP/EPDM and its nanocomposites exhibited non-Newtonian behavior. It was also found that the materials experience a fluid–solid transition at 0.5 wt% SWNT. The steady shear behaviors and die swell decreased with increasing temperature. The maximum flow activation energy corresponding to the minimum die swell was also observed. The scanning electron microscopic morphology of the PP/EPDM/SWNT nanocomposites showed that the EPDM particles were dispersed through PP and the size of dispersed phase decreased with the introduction of SWNT to 0.5 wt%. The electrical percolation threshold was formed at approximately 1 wt% of SWNT. In addition, difference between electrical and rheological percolation thresholds was observed due to the nanotube–nanotube distance after the formation of the percolating network.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Carbon Nanotubes in Composites · Polymer Nanocomposites and Properties · Dielectric materials and actuators
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Polymer Engineering, Islamic Azad University, South Branch, Tehran, Iran
Research Institute of Petroleum Industry (RIPI), Tehran, Iran
References (52)
Show source-provided references
1. 10.1007/s10965-010-9494-110.1007/s10965-010-9494-1 ↗
2. Oh JS · J Rheol · 2010 · 22 · 89
3. 10.1016/j.carbon.2004.08.01510.1016/j.carbon.2004.08.015 ↗
4. 10.1007/s00289-009-0064-910.1007/s00289-009-0064-9 ↗
5. 10.1002/pc.2049510.1002/pc.20495 ↗
6. 10.1016/j.polymertesting.2009.02.00210.1016/j.polymertesting.2009.02.002 ↗
7. 10.1002/pc.2102410.1002/pc.21024 ↗
8. Bryson JA · 1970
9. 10.1063/1.172587110.1063/1.1725871 ↗
10. 10.1002/macp.20039008110.1002/macp.200390081 ↗
11. Khosrokhavar R · Iran Polym J · 2011 · 20 · 41
12. 10.1016/j.polymer.2004.12.04410.1016/j.polymer.2004.12.044 ↗
13. 10.1016/S0266-3538(03)00036-810.1016/S0266-3538(03)00036-8 ↗
14. Chen X · J Mater Sci Technol · 2008 · 24 · 279
15. 10.1016/j.polymer.2006.12.02210.1016/j.polymer.2006.12.022 ↗
16. 10.1016/j.polymer.2004.11.03010.1016/j.polymer.2004.11.030 ↗
17. 10.1002/marc.20060089210.1002/marc.200600892 ↗
18. 10.1016/j.polymer.2005.06.09410.1016/j.polymer.2005.06.094 ↗
19. Qian D · Appl Phys Lett · 2000 · 56 · 2247
20. 10.1007/s12034-007-0061-210.1007/s12034-007-0061-2 ↗
21. 10.1007/s13233-010-1011-110.1007/s13233-010-1011-1 ↗
22. 10.1016/j.polymer.2005.09.06810.1016/j.polymer.2005.09.068 ↗
23. 10.3144/expresspolymlett.2008.8710.3144/expresspolymlett.2008.87 ↗
24. 10.1080/00914037.2010.53181010.1080/00914037.2010.531810 ↗
25. Dealy JM, Wissburn KF. Melt rheology and its role in plastic processing. London, UK: Chapman & Hall, 1996.
26. Ezzati P · Iran Polym J · 2008 · 17 · 669
27. Reddy MM · Korea-Australia Rheol J · 2007 · 19 · 133
28. 10.1080/0022234080240339610.1080/00222340802403396 ↗
29. 10.11113/jt.v39.43710.11113/jt.v39.437 ↗
30. 10.1002/app.1986.07032081110.1002/app.1986.070320811 ↗
31. 10.1002/1097-4628(20000815)77:7<1488::AID-APP10>3.0.CO;2-K10.1002/1097-4628(20000815)77:7<1488::AID-APP10>3.0.CO;2-K ↗
32. 10.1080/0022234070138910010.1080/00222340701389100 ↗
33. 10.1016/j.polymertesting.2009.08.00510.1016/j.polymertesting.2009.08.005 ↗
34. 10.1016/j.carbon.2005.09.03910.1016/j.carbon.2005.09.039 ↗
35. 10.1016/j.jnnfm.2003.08.00110.1016/j.jnnfm.2003.08.001 ↗
36. 10.1002/(SICI)1097-0126(199707)43:3<281::AID-PI800>3.0.CO;2-Q10.1002/(SICI)1097-0126(199707)43:3<281::AID-PI800>3.0.CO;2-Q ↗
37. 10.1007/s00289-008-0951-510.1007/s00289-008-0951-5 ↗
38. 10.1007/s00289-009-0063-x10.1007/s00289-009-0063-x ↗
39. 10.1002/app.1963.07007050810.1002/app.1963.070070508 ↗
40. Cheremisinoff NP · 1987
41. 10.1002/app.1340310.1002/app.13403 ↗
42. 10.1016/j.polymer.2007.07.01110.1016/j.polymer.2007.07.011 ↗
43. 10.1016/j.polymer.2009.04.06710.1016/j.polymer.2009.04.067 ↗
44. 10.1002/app.1369310.1002/app.13693 ↗
45. 10.1016/j.cplett.2004.07.04710.1016/j.cplett.2004.07.047 ↗
46. 10.1016/j.compscitech.2009.05.01410.1016/j.compscitech.2009.05.014 ↗
47. 10.3144/expresspolymlett.2010.3710.3144/expresspolymlett.2010.37 ↗
48. 10.1021/ma071179210.1021/ma0711792 ↗
49. 10.1016/j.polymer.2006.04.00810.1016/j.polymer.2006.04.008 ↗
50. 10.3144/expresspolymlett.2011.5010.3144/expresspolymlett.2011.50 ↗
51. 10.1021/ma049164g10.1021/ma049164g ↗
52. 10.1016/j.polymer.2004.10.04010.1016/j.polymer.2004.10.040 ↗