In the present work, nanocomposite polymer electrolyte films were prepared by solution casting technique using nanosized fumed silica to polyethylene oxide (PEO)-based polymer electrolytes containing ammonium bifluoride (NH 4 HF 2 ). The ionic conductivity of 1.19 × 10 −5 S cm −1 has been observed at room temperature (25°C) for 3 wt% fumed silica in PEO-10 wt% NH 4 HF 2 polymer electrolytes after which the conductivity was observed to decrease. Furthermore, the addition of high dielectric constant plasticizer propylene carbonate (PC) in the optimized composition of nanocomposite polymer electrolytes has increased the number of charge carriers by the large dissolution of ionic salt, amorphous content, and hence the ionic conductivity. Maximum ionic conductivity obtained at room temperature was found to be 1.55 × 10 −4 S cm −1 in the case of PEO-10 wt% NH 4 HF 2 -3 wt% fumed silica-0.3 (ml) PC polymer electrolytes which is five orders of magnitude higher than that of the polymer host material. Temperature-dependent ionic conductivity, activation energy, and dielectric constant studies have been described for all the compositions of polymer electrolytes. Ionic conductivity and dielectric constant studies were determined from impedance data. Polymer electrolytes containing both fumed silica and PC highlight that there is no phase transition in the polymer electrolyte and temperature dependence of ionic conductivity in the temperature range is of almost Arrhenius type. The lowest activation energy value for the highest conducting polymer electrolyte was found to be 0.172 eV. Change in melting temperature, % crystallinity ( χ c ), and mechanical properties have also been observed in polymer electrolytes containing fumed silica as well as PC as studied by Differential Scanning Calorimetry/Thermogravimetric Analysis (DSC/TGA) and universal testing machine, respectively.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced Battery Materials and Technologies · Advancements in Battery Materials · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Physics, Himachal Pradesh Technical University, Hamirpur, HP, India
Department of Physics, NSCBM Government College, Hamirpur, HP, India
References (59)
Show source-provided references
1. 10.1016/0032-3861(73)90146-810.1016/0032-3861(73)90146-8 ↗
2. Chandra S. Superionic solids: principles and applications. Amsterdam: North-Holland, 1981, p. 124.
3. 10.1016/0167-2738(94)90419-710.1016/0167-2738(94)90419-7 ↗
4. Bhide A · J Polymer · 2007 · 43 · 4253
5. 10.1016/j.memsci.2008.10.03610.1016/j.memsci.2008.10.036 ↗
6. 10.20964/2016.11.1810.20964/2016.11.18 ↗
7. 10.1021/cm00024a04810.1021/cm00024a048 ↗
8. Kim JH · Int J Electrochem Sci · 2011 · 6 · 436510.1016/S1452-3981(23)18334-9 ↗
9. 10.1007/BF0057628510.1007/BF00576285 ↗
10. 10.1002/masy.20125052310.1002/masy.201250523 ↗
11. 10.1016/j.matchemphys.2012.03.06410.1016/j.matchemphys.2012.03.064 ↗
12. Edwinraj S · J Chem Pharma Sci · 2016 · 9 · 172
13. Vijayan M · J Solid State Electrochem · 2018 · 22 · 1
14. Moniha V · Materials Today · 2019 · 8 · 449
15. 10.1149/1.139342310.1149/1.1393423 ↗
16. 10.1016/S0378-7753(03)00159-910.1016/S0378-7753(03)00159-9 ↗
17. 10.1021/jp045838d10.1021/jp045838d ↗
18. 10.1007/s12540-013-0643-z10.1007/s12540-013-0643-z ↗
19. 10.1063/1.9202310.1063/1.92023 ↗
20. 10.1016/0167-2738(82)90072-810.1016/0167-2738(82)90072-8 ↗
21. 10.1016/j.jpowsour.2004.05.05010.1016/j.jpowsour.2004.05.050 ↗
22. 10.1016/j.jpowsour.2007.09.05610.1016/j.jpowsour.2007.09.056 ↗
23. 10.1016/j.ssi.2008.01.09510.1016/j.ssi.2008.01.095 ↗
24. 10.1016/S0013-4686(02)00243-810.1016/S0013-4686(02)00243-8 ↗
25. 10.1016/j.jpowsour.2006.03.06910.1016/j.jpowsour.2006.03.069 ↗
26. 10.1016/S0014-3057(01)00310-X10.1016/S0014-3057(01)00310-X ↗
27. 10.1016/j.mseb.2006.11.02310.1016/j.mseb.2006.11.023 ↗
28. 10.1177/089270570810339310.1177/0892705708103393 ↗
29. 10.1021/acscentsci.5b0019510.1021/acscentsci.5b00195 ↗
30. 10.1177/095400831878021810.1177/0954008318780218 ↗
31. Gohel K · J Mater Sci · 2019 · 30 · 12260
32. Pradhan DK · Inter J Electrochem Sci · 2007 · 2 · 86110.1016/S1452-3981(23)17118-5 ↗
33. 10.1016/j.physb.2006.08.03810.1016/j.physb.2006.08.038 ↗
34. Chai MN · Inter J Phy Sci · 2014 · 9 · 397
35. 10.1016/j.ssi.2007.04.00810.1016/j.ssi.2007.04.008 ↗
36. Pradhan DK · Int J Electrochem Sci · 2008 · 3 · 59710.1016/S1452-3981(23)15547-7 ↗
37. 10.1016/j.ssi.2014.08.00210.1016/j.ssi.2014.08.002 ↗
38. 10.1007/s11581-014-1240-y10.1007/s11581-014-1240-y ↗
39. 10.1016/j.rinp.2019.10273510.1016/j.rinp.2019.102735 ↗
40. Ahmeda HT · Res Phys · 2020 · 16 · 102861
41. 10.1007/s10853-007-2100-110.1007/s10853-007-2100-1 ↗
42. 10.1143/JPSJS.79SA.16310.1143/JPSJS.79SA.163 ↗
43. 10.1007/s12034-016-1241-810.1007/s12034-016-1241-8 ↗
44. 10.1016/S0167-577X(03)00585-810.1016/S0167-577X(03)00585-8 ↗
45. 10.1016/j.physb.2010.08.00810.1016/j.physb.2010.08.008 ↗
46. 10.1007/BF0237407310.1007/BF02374073 ↗
47. 10.3390/polym811038710.3390/polym8110387 ↗
48. 10.1063/1.44614410.1063/1.446144 ↗
49. 10.1039/C6SC01813K10.1039/C6SC01813K ↗
50. 10.3390/polym906018710.3390/polym9060187 ↗
51. 10.1016/j.heliyon.2018.e0099210.1016/j.heliyon.2018.e00992 ↗
52. Ahmed HT · Res Phys · 2019 · 15 · 102735
53. 10.1016/S0022-0728(74)80077-X10.1016/S0022-0728(74)80077-X ↗
54. 10.1016/S0022-0728(76)80229-X10.1016/S0022-0728(76)80229-X ↗
55. Adachi K · J Non-Cryst Solids · 2002 · 667 · 307
56. 10.1007/s10853-009-3833-910.1007/s10853-009-3833-9 ↗
57. 10.1016/S0921-5107(02)00226-X10.1016/S0921-5107(02)00226-X ↗
58. 10.5012/bkcs.2012.33.9.294910.5012/bkcs.2012.33.9.2949 ↗
59. 10.1007/s11051-010-0194-x10.1007/s11051-010-0194-x ↗