Dielectric and thermo-kinetic properties of SiC/PS composite: Depending on the filler concentration
Source abstract
Abstract
In this study, the structural, dielectric, electrical, thermal, and thermo-kinetic properties of silicon carbide (SiC)/polystyrene (PS) nanocomposites containing 1–10% SiC were systematically investigated. Degradation kinetics were analyzed using the Coats–Redfern method. Pure PS exhibited low dielectric loss (tan δ ≈ 0.01–0.02) with weak frequency and temperature dependence, indicating efficient energy storage and minimal dissipation. Incorporation of SiC progressively increased low-frequency dielectric loss, reaching 0.12–0.15 at 7–10% loading. This behavior is attributed to Maxwell–Wagner–Sillars interfacial polarization and the gradual formation of quasi-conductive pathways near the percolation threshold. Temperature effects became more pronounced at higher SiC concentrations, reflecting thermally activated carrier transport and reduced interfacial relaxation times. AC conductivity (σac) evolved from polarization-limited conduction in pure PS (10 −12 –10 −11 S cm −1 ) to enhanced hopping and tunneling transport with increasing SiC content. At intermediate loadings (3–5%), conductivity increased by one to two orders of magnitude, while 7–10% composites exhibited strong frequency-dependent behavior and elevated plateau conductivity, indicating the formation of quasi-continuous conductive networks separated by thin insulating barriers. These results are consistent with Jonscher’s universal power law. Thermal analysis revealed a non-linear dependence of glass transition temperature (T g ) and degradation behavior on SiC concentration. The 7% SiC/PS composite showed the highest thermal stability, whereas the 10% composite displayed decreased and broadened T g , indicating structural heterogeneity and agglomeration at high filler loading. Activation energy decreased from 288 kJ mol −1 for pure PS to 194 kJ mol −1 at 7% SiC (α = 0.4), suggesting modified degradation pathways associated with increased free volume and altered intermolecular interactions. In contrast, Gibbs free energy remained nearly constant, indicating preservation of the overall thermodynamic degradation barrier. Overall, the 5–7 % SiC/PS range provided the best balance between enhanced dielectric performance and thermal stability.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Silicon Carbide Semiconductor Technologies · High voltage insulation and dielectric phenomena · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Baku State University
Ministry of Science and Education of the Republic of Azerbaijan
University of Calabria
Universidad Ecotec
Universidad Técnica Particular de Loja
Research and Development, Qi srl
References (71)
Show source-provided references
1. 10.3390/ma306365410.3390/ma3063654 ↗
2. 10.3390/ceramics504005210.3390/ceramics5040052 ↗
3. 10.1021/acsami.0c0242110.1021/acsami.0c02421 ↗
4. 10.1007/0-387-25100-6_610.1007/0-387-25100-6_6 ↗
5. 10.1016/j.compositesa.2015.09.00510.1016/j.compositesa.2015.09.005 ↗
6. 10.1021/acs.langmuir.4c0180510.1021/acs.langmuir.4c01805 ↗
7. 10.3390/polym1319336910.3390/polym13193369 ↗
8. 10.1016/j.heliyon.2023.e1557110.1016/j.heliyon.2023.e15571 ↗
9. 10.1007/s12633-023-02543-y10.1007/s12633-023-02543-y ↗
10. 10.1149/1.211392110.1149/1.2113921 ↗
11. 10.1016/j.tsf.2003.11.29110.1016/j.tsf.2003.11.291 ↗
12. 10.1109/AERO.2004.136804810.1109/AERO.2004.1368048 ↗
13. 10.1016/j.ceramint.2022.03.05610.1016/j.ceramint.2022.03.056 ↗
14. 10.1002/1521-3951(199707)202:1<35::AID-PSSB35>3.0.CO;2-810.1002/1521-3951(199707)202:1<35::AID-PSSB35>3.0.CO;2-8 ↗
15. 10.32604/jrm.2021.01546510.32604/jrm.2021.015465 ↗
16. 10.1109/SeFet48154.2021.937581510.1109/SeFet48154.2021.9375815 ↗
17. 10.1080/24701556.2017.128409110.1080/24701556.2017.1284091 ↗
18. 10.1007/s00339-022-05894-210.1007/s00339-022-05894-2 ↗
19. 10.1177/1465801124122983610.1177/14658011241229836 ↗
20. 10.3390/nano1111289110.3390/nano11112891 ↗
21. Nurazzi NM, Khalina A, Sapuan SM, et al. A review: fibres, polymer matrices and composites. Pertanika Journal of Science and Technology 2017; 25: 1085–1102.
22. 10.1177/089270571142329110.1177/0892705711423291 ↗
23. Popovic IG, Katsikas L. The characterization of polymer composites by thermogravimetry. Mater Tehnol 2006; 40(1): 7.
24. 10.1177/009524431775365210.1177/0095244317753652 ↗
25. 10.1021/am401703m10.1021/am401703m ↗
26. 10.3390/polym1719258010.3390/polym17192580 ↗
27. 10.1088/1361-6528/abc0c610.1088/1361-6528/abc0c6 ↗
28. 10.1016/j.compscitech.2020.10842410.1016/j.compscitech.2020.108424 ↗
29. 10.1007/s11082-023-04929-z10.1007/s11082-023-04929-z ↗
30. 10.3390/polym1202041810.3390/polym12020418 ↗
31. 10.1166/jnn.2016.1168010.1166/jnn.2016.11680 ↗
32. 10.1002/app.3918610.1002/app.39186 ↗
33. 10.1109/TPEL.2025.354976910.1109/TPEL.2025.3549769 ↗
34. 10.1016/j.ijfatigue.2025.10932710.1016/j.ijfatigue.2025.109327 ↗
35. 10.1038/s41598-025-06196-210.1038/s41598-025-06196-2 ↗
36. 10.3390/polym1209193510.3390/polym12091935 ↗
37. 10.1007/s00339-025-08781-810.1007/s00339-025-08781-8 ↗
38. 10.1016/j.ceramint.2025.08.30810.1016/j.ceramint.2025.08.308 ↗
39. 10.1029/2025RS00823910.1029/2025RS008239 ↗
40. 10.1002/pat.7053610.1002/pat.70536 ↗
41. 10.1109/TMECH.2025.362957310.1109/TMECH.2025.3629573 ↗
42. 10.1007/s10853-025-11503-310.1007/s10853-025-11503-3 ↗
43. Gahramanli L, Jafarov M, Muradov M, et al. Correlation structural, optical, and dielectric properties of β-SiC/polypropylene nanocomposites. Fullerenes, Nanotub Carbon Nanostruct 2025; 34: 1–14. https://doi.org/10.1080/1536383X.2025.2596242
44. 10.1039/D5RA08712K10.1039/D5RA08712K ↗
45. 10.1039/C9RA03383A10.1039/C9RA03383A ↗
46. 10.1063/1.482103610.1063/1.4821036 ↗
47. 10.3390/polym1210232010.3390/polym12102320 ↗
48. 10.1016/j.materresbull.2020.11116210.1016/j.materresbull.2020.111162 ↗
49. 10.1080/21870764.2018.143960610.1080/21870764.2018.1439606 ↗
50. 10.1002/app.5536210.1002/app.55362 ↗
51. Chaki TK, Khastgir DK. Effect of frequency and temperature on dielectric properties of polystyrene at microwave frequencies. Die Angewandte Makromolekulare Chemie: Appl Macromol Chem Phys Angew Makromol Chem 1991; 184(1): 55–68. https://doi.org/10.1002/apmc.1991.05184010610.1002/apmc.1991.051840106 ↗
52. 10.1007/s10443-022-10026-310.1007/s10443-022-10026-3 ↗
53. 10.1016/j.aej.2023.12.00510.1016/j.aej.2023.12.005 ↗
54. Huang Y, Huang X. Dielectric loss of polymer nanocomposites and how to keep the dielectric loss low. Polymer Nanocomposites: Electrical and Thermal Properties 2016; 2: 29–50. https://doi.org/10.1007/978-3-319-28238-1_2
55. 10.3390/polym1513289910.3390/polym15132899 ↗
56. Ibrahim SS. Low percolation behaviour of polystyrene carbon nanoparticles (PS/CNPs) composite. J Mater Environ Sci 2011; 2(2): 118–127.
57. 10.1088/0022-3727/49/19/19530210.1088/0022-3727/49/19/195302 ↗
58. 10.1063/1.277925510.1063/1.2779255 ↗
59. 10.1109/TDEI.2017.00619810.1109/TDEI.2017.006198 ↗
60. 10.1109/TDEI.2018.00694210.1109/TDEI.2018.006942 ↗
61. 10.1016/0079-6700(94)00001-I10.1016/0079-6700(94)00001-I ↗
62. 10.1016/j.polymdegradstab.2020.10943010.1016/j.polymdegradstab.2020.109430 ↗
63. 10.1002/978047042383710.1002/9780470423837 ↗
64. Monga GR, Ngb JH, Chongc WWF, et al. Kinetic study of horse manure through thermogravimetric analysis. Chem Eng 2019; 72: 241–246. https://doi.org/10.3303/cet1972041
65. 10.1016/j.enconman.2020.11319410.1016/j.enconman.2020.113194 ↗
66. 10.1007/s13399-023-04017-y10.1007/s13399-023-04017-y ↗
67. 10.3390/polym1202042110.3390/polym12020421 ↗
68. 10.3390/jcs804011710.3390/jcs8040117 ↗
69. 10.3390/spectroscj103001410.3390/spectroscj1030014 ↗
70. 10.3390/app1210488810.3390/app12104888 ↗
71. Ferracane JL. Dental resin composites: state of the art and future perspectives. Dent Mater 2022; 38(1): 1–17. https://doi.org/10.1016/j.dental.2021.09.010