Circuits and AMOLED display with self‐aligned a‐IGZO TFTs on polyimide foil
Source abstract
Abstract
Abstract A process to make self‐aligned top‐gate amorphous indium‐gallium‐zinc‐oxide (a‐IGZO) thin‐film transistors (TFTs) on polyimide foil is presented. The source/drain (S/D) region's parasitic resistance reduced during the SiN interlayer deposition step. The sheet resistivity of S/D region after exposure to SiN interlayer deposition decreased to 1.5 kΩ/□. TFTs show field‐effect mobility of 12.0 cm2/(V.s), sub‐threshold slope of 0.5 V/decade, and current ratio (ION/OFF) of >107. The threshold voltage shifts of the TFTs were 0.5 V in positive (+1.0 MV/cm) bias direction and 1.5 V in negative (−1.0 MV/cm) bias direction after extended stressing time of 104 s. We achieve a stage‐delay of ~19.6 ns at VDD = 20 V measured in a 41‐stage ring oscillator. A top‐emitting quarter‐quarter‐video‐graphics‐array active‐matrix organic light‐emitting diode display with 85 ppi (pixels per inch) resolution has been realized using only five lithographic mask steps. For operation at 6 V supply voltage (VDD), the brightness of the display exceeds 150 cd/m2.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Thin-Film Transistor Technologies · Silicon Nanostructures and Photoluminescence · Silicon and Solar Cell Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
imec Kapeldreef 75 Leuven B‐3001 Belgium
ESAT Katholieke Universiteit Leuven Oude Markt 13 Leuven 3000 Belgium
Holst Centre High Tech Campus 31 Eindhoven 5656 AE The Netherlands
Device Solutions Center Panasonic Corporation 1006 Oaza Kadoma Kadoma‐shi 571‐8501 Japan
References (25)
Show source-provided references
1. 10.1038/nature0309010.1038/nature03090 ↗
2. 10.1016/j.tsf.2011.07.01810.1016/j.tsf.2011.07.018 ↗
3. 10.1149/1.304981910.1149/1.3049819 ↗
4. 10.1002/jsid.11410.1002/jsid.114 ↗
5. 10.1002/jsid.15510.1002/jsid.155 ↗
6. 10.1002/jsid.18910.1002/jsid.189 ↗
7. 10.1002/jsid.21210.1002/jsid.212 ↗
8. 10.1109/TED.2011.217539810.1109/TED.2011.2175398 ↗
9. 10.1109/LED.2012.220144410.1109/LED.2012.2201444 ↗
10. 10.1109/LED.2012.222319210.1109/LED.2012.2223192 ↗
11. 10.1109/LED.2010.204142410.1109/LED.2010.2041424 ↗
12. 10.1889/1.362136010.1889/1.3621360 ↗
13. 10.1109/LED.2009.201418110.1109/LED.2009.2014181 ↗
14. Comparison of the effects of Ar and H2 plasmas on the performance of homo junctioned amorphous indium gallium zinc oxide thin film transistors
15. 10.1063/1.296614510.1063/1.2966145 ↗
16. 10.1109/JDT.2009.202618910.1109/JDT.2009.2026189 ↗
17. 10.1109/LED.2011.216156810.1109/LED.2011.2161568 ↗
18. 10.1016/j.sse.2006.02.00410.1016/j.sse.2006.02.004 ↗
19. 10.1002/j.2168-0159.2013.tb06178.x10.1002/j.2168-0159.2013.tb06178.x ↗
20. 10.1063/1.357952910.1063/1.3579529 ↗
21. 10.1002/j.2168-0159.2014.tb00068.x10.1002/j.2168-0159.2014.tb00068.x ↗
22. 10.1889/1.306959110.1889/1.3069591 ↗
23. 10.1889/1.306974010.1889/1.3069740 ↗
24. 10.1889/1.325676410.1889/1.3256764 ↗
25. H. N.Leeet al. Current status of challenges to and perspective view of AM‐OLED IDW'06 Proc. 663‐666 (2006).