Impact of humidity on the electrical performance of amorphous oxide semiconductor thin‐film transistors
Source abstract
Abstract
Abstract An indium–gallium–zinc oxide or a zinc–tin oxide thin‐film transistor (TFT) fabricated when the relative humidity in the laboratory is less than 50% is found to exhibit good electrical performance, with an abrupt, distortion‐free transfer curve and a turn‐on voltage close to 0 V. In contrast, when such an amorphous oxide semiconductor (AOS) TFT is fabricated at a relative humidity greater than 50%, its “as‐fabricated” electrical performance is very poor, typically characterized by a large amount of hysteresis, a strongly negative turn‐on voltage, and a kink‐like distortion in the subthreshold region of its transfer curve. However, the electrical performance of such a poor‐quality TFT is observed to improve over time, if it is simply stored in the dark at room temperature without being subjected to electrical stress. This recovery usually requires weeks (months) for an unpassivated (passivated) AOS TFT. Recovery is tentatively ascribed to the gradual removal of moisture from the AOS TFT channel layer.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Thin-Film Transistor Technologies · ZnO doping and properties · Transition Metal Oxide Nanomaterials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Sharp Laboratories of America 5750 NW Pacific Rim Blvd. Camas WA 98607‐9489 USA
School of EECS Oregon State University Corvallis OR 97331‐5501 USA
References (21)
Show source-provided references
1. 10.1016/0022-3093(96)00367-510.1016/0022-3093(96)00367-5 ↗
2. Y.Matsueda “Required characteristics of TFTs for next generation flat panel display backplanes ”Dig. Int. Transistor Conf. pp. 314 (2010).
3. “Sharp begins production of world's first LCD panels incorporating IGZO oxide semiconductors ”Sharp corporation press release.http://www.sharp‐world.com/corporate/news/120413.html[April 13 2012].
4. 10.1889/1.325670110.1889/1.3256701 ↗
5. 10.1063/1.154267710.1063/1.1542677 ↗
6. 10.1063/1.302071410.1063/1.3020714 ↗
7. Interface and bulk effects for bias‐light‐illuminatin instability in amorphous‐In‐Ga‐Zn‐O thin‐film transistors
8. 10.1016/j.tsf.2009.10.13210.1016/j.tsf.2009.10.132 ↗
9. 10.1063/1.362212110.1063/1.3622121 ↗
10. 10.1063/1.299065710.1063/1.2990657 ↗
11. The effect of moisture on the photon‐enhanced negative bias thermal instability in In‐Ga‐Zn‐O thin‐film transistors
12. 10.1063/1.283838010.1063/1.2838380 ↗
13. 10.1021/am301308y10.1021/am301308y ↗
14. 10.1088/1468-6996/11/4/04430510.1088/1468-6996/11/4/044305 ↗
15. 10.1109/TDMR.2010.206956110.1109/TDMR.2010.2069561 ↗
16. 10.1016/j.tsf.2011.07.01810.1016/j.tsf.2011.07.018 ↗
17. 10.1109/TED.2009.202133910.1109/TED.2009.2021339 ↗
18. 10.1109/LED.2012.219153010.1109/LED.2012.2191530 ↗
19. K.Hoshino Fabrication process assessment and negative bias illumination stress study of IGZO and ZTO TFTs Ph.D. Thesis Oregon State University (2012).
20. Schroder D. K. · 2006
21. 10.1016/B978-0-12-396489-2.00009-610.1016/B978-0-12-396489-2.00009-6 ↗