Abstract

Abstract Device degradation behaviors of n‐channel low‐temperature polycrystalline silicon thin film transistors under negative bias stress and positive bias stress were investigated. It was found that the threshold‐voltage has a two‐stage degradation, shifting to different direction with time. The mobility and the subthreshold swing SS both show a dependence on the stress time. It was determined that the interface trap states, the grain boundary trap states, and electron trapping together dominate the time‐dependent degradation behaviors. The trap is caused by the rupture of Si─H and Si─O bonds. A comprehensive model is proposed to explain the time‐dependent degradation behaviors clearly. In addition, after removing the stress, the recovery behaviors of threshold voltage Vth can be observed, which provide the evidence supporting the degradation model proposed.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Thin-Film Transistor Technologies · Semiconductor materials and devices · Advancements in Semiconductor Devices and Circuit Design

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Optics and Photonics, Beijing Engineering Research Center of Mixed Reality and Advanced Display Beijing Institute of Technology Beijing China

Beijing BOE Optoelectronics Technology Co., Ltd Beijing China

References (20)

Show source-provided references
1. 10.1109/LED.2004.83921710.1109/LED.2004.839217 ↗
2. 10.1109/LED.2008.200083110.1109/LED.2008.2000831 ↗
3. 10.1109/TED.2006.88872310.1109/TED.2006.888723 ↗
4. 10.1049/el:2002079410.1049/el:20020794 ↗
5. 10.1109/TED.2007.90890710.1109/TED.2007.908907 ↗
6. 10.1109/TDMR.2010.210415210.1109/TDMR.2010.2104152 ↗
7. 10.1109/55.6178510.1109/55.61785 ↗
8. 10.1109/55.7575710.1109/55.75757 ↗
9. 10.1109/TED.2006.88554310.1109/TED.2006.885543 ↗
10. 10.1109/TED.2004.83359210.1109/TED.2004.833592 ↗
11. 10.1016/j.sse.2015.09.00910.1016/j.sse.2015.09.009 ↗
12. 10.1109/LED.2005.85273910.1109/LED.2005.852739 ↗
13. Mahapatra'S AlamMA.A predictive reliability model for PMOS bias temperature degradation” IEDM Tech. Digest 2002 505‐508.https://doi.org/10.1109/IEDM.2002.117589010.1109/IEDM.2002.1175890 ↗
14. 10.1063/1.35990510.1063/1.359905 ↗
15. 10.1109/16.59593710.1109/16.595937 ↗
16. 10.1109/LED.2007.91409110.1109/LED.2007.914091 ↗
17. 10.1063/1.35644610.1063/1.356446 ↗
18. 10.1109/16.12348410.1109/16.123484 ↗
19. 10.1063/1.219182810.1063/1.2191828 ↗
20. 10.1109/LED.2007.91408310.1109/LED.2007.914083 ↗