Strength/flaw relationship for CRT panel glass (alkali strontium silicate glass)
Source abstract
Abstract
Abstract— Four‐point bend strength of samples of CRT panel glass was measured following sandblast, gritblast, and 150‐J abrasions, after either a 48‐hour soak in air or a 24‐hour soak in water. Strength/flaw characteristics were determined by examining the fracture surface and relating strength to flaw depth and mirror radius. Fracture toughness was also measured. Based on the strength and the fracture toughness values, the flaw shape factor or flaw severity for each type of abrasion was calculated.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Glass properties and applications · Recycling and utilization of industrial and municipal waste in materials production
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (6)
Show source-provided references
1. ASTM Designation C‐158 “Standard Methods of Flexural Testing of Glass ”in1988 Annual Book of ASTM Standards Vol. 15.02 pp.19–24.
2. G.Wightman “Procedure for Conducting Pressure Test on CRT Tubes ”unpublished report Corning Inc.
3. 10.1111/j.1151-2916.1989.tb06242.x10.1111/j.1151-2916.1989.tb06242.x ↗
4. 10.1007/BF0001339310.1007/BF00013393 ↗
5. 10.1111/j.1151-2916.1970.tb15962.x10.1111/j.1151-2916.1970.tb15962.x ↗
6. “Lifetime Prediction for Cathode Ray Tubes Based on Fatigue Data for Alkali Strontium Silicate Glass,”