The study of crystallinity of ZnS:TbOF thin films and green thin‐film electroluminescent devices with different stacked insulating layers
Source abstract
Abstract
Abstract— In order to improve the characteristics of thin‐film electroluminescent (TFEL) devices, the dependence of crystallinity on deposition conditions of ZnS:TbOF thin films deposited by rf‐magnetron sputtering have been studied. The optimal deposition conditions obtained are: rf power density, 1.54 W/cm2; substrate temperature, 175°C; pressure, 5 mTorr; and sputtering gas, pure Ar. Several types of ZnS:TbOF green ACTFEL devices with different stacked insulating‐layer structures were prepared and compared. The ACTFEL device obtained with the superior structure is ITO/SiO2/Ta2O5/ZnS:TbOF/SiO2/Ta2O5/Al. This result suggests that a high‐resistivity dielectric can be used as the second insulating layer adjacent to the phosphor layer and can improve the luminous characteristics of ACTFEL devices in this study.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Glass properties and applications · Luminescence Properties of Advanced Materials · Solid State Laser Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (5)
Show source-provided references
1. 10.1063/1.33785410.1063/1.337854 ↗
2. 10.1063/1.9687010.1063/1.96870 ↗
3. 10.1143/JJAP.28.137810.1143/JJAP.28.1378 ↗
4. 10.1109/T-ED.1977.1885010.1109/T-ED.1977.18850 ↗
5. 10.1149/1.208641510.1149/1.2086415 ↗