journal article·1986-05

14—THE EFFECT OF THE STRENGTH PROPERTIES OF WOOL STAPLES ON WORSTED PROCESSING PART I: THE LEVEL OF STAPLE STRENGTH

R. A. Rottenbury, M. W. Andrews, P. J. M. Bell, R. Bownass

Publisher page

Abstract

An account is given of an experimental study conducted specifically to examine the effects of large variations in the staple strength of greasy wool on subsequent performance in combing and spinning by means of pilot-scale processing techniques. Batches were processed for two levels of mean fibre diameter (20 and 22 μm), each at four levels of staple strength (nominally 20, 30, 45, and 60 N/ktex), and there was close control over other raw-wool properties. Three comb settings were used for each batch. Yarns were spun to five counts selected to include the normal commercial range and the limiting situation. The SAWTRI mean-spindle-speed test was employed to assess spinning performance. The resultant fibre length and its distribution for tops were found to be closely dependent on the staple strength and the comb setting. Differences in Hauteur of 11–14 mm were observed between the batches from the low- and high-staple-strength categories within each comb setting and fibre-diameter grouping. Differences in spinning performance were observed between the batches of the weakest wools and those of the other batches for which there were no marked trends in performance despite the differences in the fibre length of the tops.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Textile materials and evaluations · Dyeing and Modifying Textile Fibers

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

C.S.I.R.O.

Australian Wool Corporation

Wira Technology Group Ltd.

References (22)

Show source-provided references
1. Turpie , D. W. F. and Gee , E. 1980 . Proc. Int. Wool Text. Res. Conf. Pretoria III-293
2. Hunter , L. and Gee , E. 1980 . Proc. Int. Wool Text. Res. Conf. Pretoria III-327
3. 10.1177/00405175830530010610.1177/004051758305300106 ↗
4. 10.1080/19447027.1961.1075046010.1080/19447027.1961.10750460 ↗
5. Turpie , D. W. F. and Hunter , L. 1980 . Proc. Int. Wool Text. Res. Conf. Pretoria , Vol. 3 : 203 – -216 .
6. 10.1080/1944702600866253010.1080/19447026008662530 ↗
7. 10.1080/1944702640866022510.1080/19447026408660225 ↗
8. 10.1080/1944702650866225910.1080/19447026508662259 ↗
9. Rottenbury , R. A. and Smith , L. J. June 1979 . Proc. IWTO Tech. Cttee June , Report No. 5
10. Townend , P. P. , Matto , A. R. and Clegg , P. C. 1973 . Text. Month , May : 58
11. Andrews , M. W. 1979. Dec. . ‘Proceedings of a Seminar on Staple Length and Staple Strength of Greasy Wool’ 73 Ryde, N.S.W. : C.S.I.R.O. Division of Textile Physics . Paper 5
12. 1980–81 . C.S.I.R.O. Division of Textile Physics. Annual Report 3
13. Rottenbury , R. A. , Kavanagh , W. J. , Eley , J. R. and Andrews , M. W. 1985 . Proc. IWTO Tech. Cttee , Jan. Report No. 0
14. Turpie , D. W. F. 1975 . SAWTRI Technical Report No. 240
15. Standards Association of Australia. Australian Standards AS2720–1983 and AS2722–1983
16. Jan 1984 . ‘TEAM Interim Report’ (Report to the Wool Distribution Research Advisory Committee of the Australian Wool Corporation) Jan , Melbourne : Australian Wool Corporation .
17. 10.1080/0040500790865880210.1080/00405007908658802 ↗
18. Lowe , J. 1972 . Wira Report No. 189
19. Wilks , R. and Lowe , J. 1970 . Wira Report No. 210
20. IWTO Technical Committee. Specification for Test Methods , IWTO-5–60
21. IWTO Technical Committee. Specification for Test Methods , IWTO-32–82.
22. Rottenbury , R. A. April 1983 . ‘Proceedings of a Seminar on Clip-preparation Research’ April , 61 Ryde, N.S.W. : C.S.I.R.O. Division of Textile Physics . Paper No. 7