33—SHRINKPROOFING WOOLLEN FABRIC BY THE APPLICATION OF POLYACRYLATES
Source abstract
Abstract
Woollen fabric can be shrinkproofed by the application of a polyacrylate and a cross-linking agent, provided that the fabric is first given a reductive pre-treatment and then rinsed with water. The main function of the reductive pre-treatment, including the rinsing step, is to degrade and clean the surface of the fibres in preparation for polymer deposition. If the rinsing step is omitted, the pre-treatment is ineffective. The pre-treatment also inhibits felting by setting the fibres.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Textile materials and evaluations
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (8)
Show source-provided references
1. Feldtman H. D. · Text. Res. J. · 1965 · 35 · 15010.1177/004051756503500209 ↗
2. Feldtman H. D. · Text, Inst. Industr. · 1970 · 8 · 249
3. Cook J. R. · Text. Inst. Industr. · 1968 · 6 · 153
4. Feldtman H. D. · Amer. Dyest. Rep. · 1964 · 53 · 199
5. Katz H. J. · Text. Res. J. · 1966 · 36 · 87410.1177/004051756603601004 ↗
6. Makinson K. R. · Text. Res. J. · 1960 · 30 · 59810.1177/004051756003000807 ↗
7. Alexander, P. and Hudson., R. F. 1954.Wool: Its Chemistry and Physics, 250London: Chapman & Hall.
8. Cook J. R. · J. Text. Inst. · 1971 · 62 · 438