Abstract
Chromium thin films are deposited by combining direct current magnetron sputtering and high power impulse magnetron sputtering (HiPIMS) on a single cathode in an industrial deposition system. While maintaining a constant deposition rate and unchanged metal ion energy distribution function, the fraction of the total power supplied by either deposition technique is altered, and thereby also the metal ion to metal neutral ratio of the deposition flux. It is observed that the required total average power needed to be proportionally increased as the HiPIMS fraction is increased to be able to keep a constant deposition rate. The influence on microstructure, electrical, and electrochemical properties of the films is investigated and shows improvements with the use of HiPIMS. However, considerable influence of the studied properties occurs already when only some 40% of the total power is supplied by the HiPIMS technique. Further increase of the HiPIMS power fraction results in comparatively minor influence of the studied properties yet significant deposition rate efficiency reduction. The results show that the degree of ionization can be controlled separately, and that the advantages associated with using HiPIMS can be obtained while much of the deposition rate reduction, often reported for HiPIMS, can be avoided.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Impact Coatings Plasma & Coatings Physics Division, IFM-Materials Physics, Linköping University, SE-581 83 Linköping, Sweden and , Westmansgatan 29, SE-582 16 Linköping, Sweden
Linköping University Plasma & Coatings Physics Division, IFM-Materials Physics, , SE-581 83 Linköping, Sweden
Uppsala University Department of Materials Chemistry, The A˚ngström Laboratory, , Box 538, SE-751 21 Uppsala, Sweden
Impact Coatings , Westmansgatan 29, SE-582 16 Linköping, Sweden
References (29)
Show source-provided references
1. Surf. Coat. Technol. · 1999 · 122 · 29010.1016/S0257-8972(99)00292-3 ↗
2. Thin Solid Films · 2006 · 513 · 110.1016/j.tsf.2006.03.033 ↗
3. Surf. Coat. Technol. · 2010 · 204 · 166110.1016/j.surfcoat.2009.11.013 ↗
4. Vacuum · 2010 · 84 · 136010.1016/j.vacuum.2009.12.022 ↗
5. Surf. Coat. Technol. · 2010 · 205 · 59110.1016/j.surfcoat.2010.07.041 ↗
6. J. Vac. Sci. Technol. A · 2005 · 23 · 33010.1116/1.1865133 ↗
7. J. Vac. Sci. Technol. A · 2007 · 25 · 4210.1116/1.2388954 ↗
8. Appl. Phys. Lett. · 2006 · 88 · 02150110.1063/1.2162671 ↗
9. Plasma Sources Sci. Technol. · 2008 · 17 · 03502110.1088/0963-0252/17/3/035021 ↗
10. J. Vac. Sci. Technol. A · 2012 · 30 · 03080110.1116/1.3691832 ↗
11. Appl. Phys. Lett. · 2006 · 89 · 15410410.1063/1.2362575 ↗
12. J. Vac. Sci. Technol. A · 2005 · 23 · 1810.1116/1.1818135 ↗
13. Surf. Coat. Technol. · 2011 · 205 · 482810.1016/j.surfcoat.2011.04.071 ↗
14. J. Phys. D: Appl. Phys. · 2009 · 42 · 01530410.1088/0022-3727/42/1/015304 ↗
15. JOM · 2011 · 63 · 4810.1007/s11837-011-0092-4 ↗
16. J. Phys. D: Appl. Phys. · 2008 · 41 · 09520310.1088/0022-3727/41/9/095203 ↗
17. J. Cryst. Growth · 1999 · 205 · 44110.1016/S0022-0248(99)00291-2 ↗
18. Appl. Phys. Lett. · 1993 · 63 · 3610.1063/1.109742 ↗
19. Thin Solid Films · 2010 · 518 · 408710.1016/j.tsf.2009.10.145 ↗
20. 2007 · 150
21. Thin Solid Films · 2008 · 517 · 123910.1016/j.tsf.2008.06.080 ↗
22. J. Optoelectron. Adv. Mater. · 2005 · 7 · 2481
23. 2007 · 477
24. H. Ljungcrantz and T. Rosell, U. S. Patent US2007/0084401 A1 (11 November 2003).
25. 1980 · 2606
26. Electrochim. Acta · 2003 · 48 · 318510.1016/S0013-4686(03)00368-2 ↗
27. 2008 · 317
28. 2007 · 160
29. Thin Solid Films · 2010 · 518 · 597810.1016/j.tsf.2010.05.064 ↗