Comparison of thermal and plasma-enhanced atomic layer deposition of niobium oxide thin films
Source abstract
Abstract
Niobium pentoxide was deposited using tBuN=Nb(NEt2)3 as niobium precursor by both thermal atomic layer deposition (ALD) and plasma-enhanced atomic layer deposition (PE-ALD) with H2O and O2 plasma as coreactants, respectively. The deposition temperature was varied between 150 and 350 °C in both ALD processes. Amorphous films were obtained in all cases. Self-limiting saturated growth was confirmed for both ALD processes along with high uniformity over a 200 mm Si wafer. The PE-ALD process enabled a higher growth per cycle (GPC) than the thermal ALD process (0.56 Å vs 0.38 Å at 200 °C, respectively), while the GPC decreases with increasing temperature in both cases. The high purity of the film was confirmed using Rutherford backscattering spectrometry, elastic recoil detection, and x-ray photoelectron spectroscopy, while the latter technique also confirmed the Nb+5 oxidation state of the niobium oxide films. The thermal ALD deposited films were substoichiometric due to the presence of oxygen vacancies (VO), of which a more dominant presence was observed with increasing deposition temperature. The PE-ALD deposited films were found to be near stoichiometric for all investigated deposition temperatures.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Catalytic Processes in Materials Science · Electronic and Structural Properties of Oxides
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Applied Physics, Eindhoven University of Technology , P.O. Box 513, 5600 MB Eindhoven, The Netherlands
Department of Applied Physics, Eindhoven University of Technology , P.O. Box 513, 5600 MB Eindhoven, The Netherlands and , North end, Bristol BS49 4AP, United Kingdom
Oxford Instruments Plasma Technology , P.O. Box 513, 5600 MB Eindhoven, The Netherlands and , North end, Bristol BS49 4AP, United Kingdom
Funding
FP7 Ideas: European Research Council
References (45)
Show source-provided references
1. Prog. Mater. Sci. · 2016 · 80 · 110.1016/j.pmatsci.2016.02.001 ↗
2. J. Mater. Chem. A · 2014 · 2 · 1568310.1039/C4TA02561J ↗
3. Microelectron. Eng. · 2011 · 88 · 244710.1016/j.mee.2011.01.050 ↗
4. Semicond. Sci. Technol. · 2013 · 28 · 5500510.1088/0268-1242/28/5/055005 ↗
5. J. Vac. Sci. Technol., A · 2014 · 32 · 01A12210.1116/1.4843555 ↗
6. Microporous Mesoporous Mater. · 1999 · 28 · 11310.1016/S1387-1811(98)00291-1 ↗
7. Sens. Actuator, B · 1999 · 56 · 12110.1016/S0925-4005(99)00191-4 ↗
8. Langmuir · 2017 · 33 · 929810.1021/acs.langmuir.7b00683 ↗
9. J. Mater. Chem. A · 2015 · 3 · 1183010.1039/C5TA01544H ↗
10. Mater. Chem. Phys. · 2008 · 109 · 18410.1016/j.matchemphys.2007.11.026 ↗
11. J. Mater. Sci. · 2017 · 52 · 1012710.1007/s10853-017-1228-x ↗
12. Thin Solid Films · 1996 · 277 · 16210.1016/0040-6090(95)08011-2 ↗
13. Appl. Opt. · 2009 · 48 · 453610.1364/AO.48.004536 ↗
14. J. Phys. D: Appl. Phys. · 2016 · 49 · 26530410.1088/0022-3727/49/26/265304 ↗
15. J. Electrochem. Soc. · 1969 · 116 · 23410.1149/1.2411804 ↗
16. Surf. Interface Anal. · 2004 · 36 · 88810.1002/sia.1793 ↗
17. Sol. Energy Mater. Sol. Cell · 2009 · 93 · 22210.1016/j.solmat.2008.10.012 ↗
18. Thin Solid Films · 2006 · 515 · 167410.1016/j.tsf.2006.05.047 ↗
19. Chem. Vap. Deposition · 1998 · 4 · 2910.1002/(SICI)1521-3862(199801)04:01<29::AID-CVDE29>3.3.CO;2-I ↗
20. Energy Environ. Sci. · 2015 · 8 · 292810.1039/C5EE02608C ↗
21. J. Phys. Chem. C · 2016 · 120 · 802310.1021/acs.jpcc.6b01728 ↗
22. Chem. Mater. · 2012 · 24 · 97510.1021/cm2026812 ↗
23. ECS Trans. · 2010 · 33 · 10110.1149/1.3485246 ↗
24. Chem. Mater. · 2012 · 24 · 155510.1021/cm202933g ↗
25. ECS Solid State Lett. · 2012 · 1 · N110.1149/2.002201ssl ↗
26. Ceram. Int. · 2017 · 43 · 658010.1016/j.ceramint.2017.02.089 ↗
27. Mater. Lett. · 2011 · 65 · 218210.1016/j.matlet.2011.04.067 ↗
28. Proc. Electrochem. Soc. · 2005 · 2005-09 · 598
29. Appl. Surf. Sci. · 1994 · 82–83 · 46810.1016/0169-4332(94)90260-7 ↗
30. 2015 · 110110.1016/B978-0-444-63304-0.00027-5 ↗
31. J. Vac. Sci. Technol., A · 2011 · 29 · 5080110.1116/1.3609974 ↗
32. J. Vac. Sci. Technol., A · 2009 · 27 · 71610.1116/1.3147215 ↗
33. J. Electrochem. Soc. · 2007 · 154 · G16510.1149/1.2737629 ↗
34. J. Vac. Sci. Technol., A · 2007 · 25 · 135710.1116/1.2753846 ↗
35. J. Phys. D: Appl. Phys. · 2009 · 42 · 7300110.1088/0022-3727/42/7/073001 ↗
36. J. Vac. Sci. Technol., A · 2012 · 30 · 2150510.1116/1.3683057 ↗
37. Chem. Vap. Deposition · 2013 · 19 · 12510.1002/cvde.201207033 ↗
38. ECS Trans. · 2008 · 16 · 24710.1149/1.2980000 ↗
39. Chem. Vap. Deposition · 2006 · 12 · 1310.1002/cvde.200500024 ↗
40. Surf. Interface Anal. · 2013 · 45 · 120610.1002/sia.5253 ↗
41. ACS Appl. Mater. Interfaces · 2017 · 9 · 1328610.1021/acsami.7b00778 ↗
42. J. Appl. Phys. · 2011 · 110 · 2411510.1063/1.3606416 ↗
43. J. Mater. Chem. A · 2014 · 2 · 743910.1039/C4TA00354C ↗
44. Phys. Status Solidi · 1966 · 15 · 62710.1002/pssb.19660150224 ↗
45. J. Vac. Sci. Technol., A · 2018 · 36 · 01B10310.1116/1.4986202 ↗