Low sheet resistance titanium nitride films by low-temperature plasma-enhanced atomic layer deposition using design of experiments methodology
Source abstract
Abstract
A design of experiments methodology was used to optimize the sheet resistance of titanium nitride (TiN) films produced by plasma-enhanced atomic layer deposition (PE-ALD) using a tetrakis(dimethylamino)titanium precursor in a N2/H2 plasma at low temperature (250 °C). At fixed chamber pressure (300 mTorr) and plasma power (300 W), the plasma duration and N2 flow rate were the most significant factors. The lowest sheet resistance values (163 Ω/sq. for a 20 nm TiN film) were obtained using plasma durations ∼40 s, N2 flow rates >60 standard cubic centimeters per minute, and purge times ∼60 s. Time of flight secondary ion mass spectroscopy data revealed reduced levels of carbon contaminants in the TiN films with lowest sheet resistance (163 Ω/sq.), compared to films with higher sheet resistance (400–600 Ω/sq.) while transmission electron microscopy data showed a higher density of nanocrystallites in the low-resistance films. Further significant reductions in sheet resistance, from 163 Ω/sq. to 70 Ω/sq. for a 20 nm TiN film (corresponding resistivity ∼145 μΩ·cm), were achieved by addition of a postcycle Ar/N2 plasma step in the PE-ALD process.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Semiconductor materials and devices · Copper Interconnects and Reliability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Tyndall National Institute, University College Cork , Cork, Ireland
References (35)
Show source-provided references
1. Thin Solid Films · 2000 · 377–378 · 51210.1016/S0040-6090(00)01438-3 ↗
2. Biomed. Mater. · 2009 · 4 · 02500110.1088/1748-6041/4/2/025001 ↗
3. Mater. Sci. Eng. A · 2000 · 286 · 32410.1016/S0921-5093(00)00744-9 ↗
4. Opt. Mater. Express · 2012 · 2 · 47810.1364/OME.2.000478 ↗
5. Microelectron. Eng. · 2005 · 82 · 24810.1016/j.mee.2005.07.083 ↗
6. Solid-State Electron. · 2007 · 51 · 61710.1016/j.sse.2007.02.008 ↗
7. Mater. Lett. · 2005 · 59 · 61510.1016/j.matlet.2004.09.030 ↗
8. J. Electron. Mater. · 2003 · 32 · 89010.1007/s11664-003-0206-z ↗
9. J. Electrochem. Soc. · 1998 · 145 · 417310.1149/1.1838932 ↗
10. Chem. Vapor Depos. · 2000 · 6 · 11510.1002/(SICI)1521-3862(200006)6:3<115::AID-CVDE115>3.0.CO;2-G ↗
11. J. Electrochem. Soc. · 1993 · 140 · 321510.1149/1.2221013 ↗
12. Thin Solid Films · 1995 · 270 · 62110.1016/0040-6090(95)06898-8 ↗
13. J. Vac. Sci. Technol. B · 2000 · 18 · 201610.1116/1.1305809 ↗
14. 2001
15. Electrochem. Solid-State Lett. · 2002 · 5 · C410.1149/1.1420925 ↗
16. Jpn. J. Appl. Phys., Part 2 · 2002 · 41 · L41810.1143/JJAP.41.L418 ↗
17. J. Vac. Sci. Technol. B · 2002 · 20 · 132110.1116/1.1486233 ↗
18. J. Vac. Sci. Technol. B · 2003 · 21 · 109910.1116/1.1577568 ↗
19. J. Vac. Sci. Technol. A · 2003 · 21 · 9610.1116/1.1524145 ↗
20. Mater. Sci. Eng. C · 2004 · 24 · 28910.1016/j.msec.2003.09.062 ↗
21. J. Electrochem. Soc. · 2005 · 152 · G58910.1149/1.1938108 ↗
22. J. Vac. Sci. Technol. A · 2005 · 23 · L510.1116/1.1938981 ↗
23. Thin Solid Films · 2006 · 514 · 9710.1016/j.tsf.2006.03.013 ↗
24. J. Vac. Sci. Technol. A · 2007 · 25 · 135710.1116/1.2753846 ↗
25. Microelectron. Eng. · 2009 · 86 · 7210.1016/j.mee.2008.09.036 ↗
26. J. Vac. Sci. Technol. B · 2009 · 27 · 37810.1116/1.3021036 ↗
27. ECS Trans. · 2011 · 41 · 15710.1149/1.3633664 ↗
28. J. Non-Cryst. Solids · 2008 · 354 · 127210.1016/j.jnoncrysol.2006.11.036 ↗
29. J. Vac. Sci. Technol. A · 2013 · 31 · 01A13710.1116/1.4769204 ↗
30. Thin Solid Films · 1986 · 140 · 27710.1016/0040-6090(86)90271-3 ↗
31. Am. Stat. · 1999 · 53 · 12610.2307/2685731 ↗
32. See supplementary material at http://dx.doi.org/10.1116/1.4868215 for a full run card for an ALD run (S1) and for cross-sectional TEM data for samples from runs 1,3,7,11 (S2).
33. 2005
34. J. Phys. D: Appl. Phys. · 2013 · 46 · 15530810.1088/0022-3727/46/15/155308 ↗
35. 1999