Transparent conductive Al-doped ZnO thin films grown at room temperature
Source abstract
Abstract
Aluminum-doped ZnO (ZnO:Al, AZO) thin films were prepared on glass substrates by dc reactive magnetron sputtering from a Zn–Al alloy target at room temperature. The effects of the Ar-to-O2 partial pressure ratios on the structural, electrical, and optical properties of AZO films were studied in detail. AZO films grown using 100:4 to 100:8 Ar-to-O2 ratio result in acceptable quality films with c-axis orientated crystals, uniform grains, 10−3 Ω cm resistivity, greater than 1020 cm−3 electron concentration, and high transmittance, 90%, in the visible region. The lowest resistivity of 4.11×10−3 Ω cm was obtained under the Ar-to-O2 partial pressure ratio of 100:4. A relatively strong UV emission at ∼3.26 eV was observed in the room-temperature photoluminescence spectrum. X-ray photoelectron spectroscopy analysis confirmed that Al was introduced into ZnO and substitutes for Zn and doped the film n-type.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: ZnO doping and properties · Gas Sensing Nanomaterials and Sensors · Ga2O3 and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Zhejiang University State Key Laboratory of Silicon Materials, Department of Materials Science and Engineering, , Hangzhou 310027, China
References (40)
Show source-provided references
1. J. Electron. Mater. · 2009 · 38 · 156810.1007/s11664-009-0747-x ↗
2. J. Eur. Ceram. Soc. · 2008 · 28 · 306510.1016/j.jeurceramsoc.2008.05.008 ↗
3. Phys. Status Solidi A · 2002 · 193 · 13910.1002/1521-396X(200209)193:1<139::AID-PSSA139>3.0.CO;2-D ↗
4. Appl. Phys. Lett. · 2004 · 85 · 313410.1063/1.1803935 ↗
5. J. Mater. Sci. · 1984 · 19 · 110.1007/BF02403106 ↗
6. J. Cryst. Growth · 2006 · 287 · 4410.1016/j.jcrysgro.2005.10.040 ↗
7. J. Mater. Sci.: Mater. Electron. · 2008 · 19 · 113510.1007/s10854-007-9489-9 ↗
8. Thin Solid Films · 2003 · 435 · 7810.1016/S0040-6090(03)00376-6 ↗
9. Appl. Phys. Lett. · 2003 · 83 · 187510.1063/1.1605805 ↗
10. Appl. Phys. Lett. · 2009 · 94 · 04210310.1063/1.3074373 ↗
11. Vacuum · 2009 · 83 · 143510.1016/j.vacuum.2009.05.006 ↗
12. Appl. Phys. Lett. · 2008 · 93 · 07330810.1063/1.2975176 ↗
13. J. Cryst. Growth · 2007 · 299 · 110.1016/j.jcrysgro.2006.10.251 ↗
14. Sol. Energy Mater. Sol. Cells · 2005 · 89 · 9910.1016/j.solmat.2005.01.012 ↗
15. Microelectron. J. · 2009 · 40 · 38110.1016/j.mejo.2008.09.003 ↗
16. J. Cryst. Growth · 1998 · 192 · 43010.1016/S0022-0248(98)00422-9 ↗
17. Curr. Appl. Phys. · 2009 · 9 · 68310.1016/j.cap.2008.06.006 ↗
18. Thin Solid Films · 2009 · 517 · 632310.1016/j.tsf.2009.02.056 ↗
19. Mater. Chem. Phys. · 2008 · 112 · 16210.1016/j.matchemphys.2008.05.047 ↗
20. Sol. Energy Mater. Sol. Cells · 2009 · 93 · 135610.1016/j.solmat.2009.02.018 ↗
21. J. Cryst. Growth · 2005 · 274 · 45310.1016/j.jcrysgro.2004.10.026 ↗
22. Appl. Surf. Sci. · 2009 · 255 · 566910.1016/j.apsusc.2008.12.021 ↗
23. J. Electroceram. · 2009 · 23 · 51210.1007/s10832-008-9523-1 ↗
24. Solid-State Electron. · 2009 · 53 · 114910.1016/j.sse.2009.07.006 ↗
25. Appl. Surf. Sci. · 2010 · 256 · 505610.1016/j.apsusc.2010.03.059 ↗
26. J. Appl. Phys. · 2006 · 100 · 07371410.1063/1.2357638 ↗
27. J. Appl. Phys. · 2007 · 101 · 08370510.1063/1.2721374 ↗
28. Thin Solid Films · 2005 · 491 · 5410.1016/j.tsf.2005.05.021 ↗
29. J. Appl. Phys. · 1998 · 84 · 228710.1063/1.368295 ↗
30. J. Mater. Sci.: Mater. Electron. · 2008 · 19 · 107310.1007/s10854-007-9469-0 ↗
31. Thin Solid Films · 2007 · 515 · 287910.1016/j.tsf.2006.08.047 ↗
32. 1979 · 171
33. Appl. Phys. Lett. · 1986 · 49 · 39410.1063/1.97598 ↗
34. J. Appl. Phys. · 1995 · 78 · 621110.1063/1.360567 ↗
35. J. Appl. Phys. · 1977 · 48 · 352410.1063/1.324149 ↗
36. Appl. Surf. Sci. · 2000 · 158 · 13410.1016/S0169-4332(99)00601-7 ↗
37. J. Electron Spectrosc. Relat. Phenom. · 2009 · 173 · 710.1016/j.elspec.2009.03.001 ↗
38. J. Chem. Phys. · 2000 · 113 · 633410.1063/1.1309131 ↗
39. J. Electrochem. Soc. · 2003 · 150 · H22510.1149/1.1602458 ↗
40. 1979 · 50