journal article·2024-03-01

Effect of growth temperature on the microstructure and properties of epitaxial MoS2 monolayers grown by metalorganic chemical vapor deposition

Chen Chen, Nicholas Trainor, Shalini Kumari, Henrik Myja, Tilmar Kümmell, Zhiyu Zhang, Yuxi Zhang, Anuj Bisht, Muhtasim Ul Karim Sadaf, Najam U. Sakib, Ying Han, Thomas V. Mc Knight, Andrew R. Graves, Meghan E. Leger, Nicholas D. Redwing, Myeongok Kim, Dorota Anna Kowalczyk, Gerd Bacher, Nasim Alem, Yang Yang, Saptarshi Das, Joan M. Redwing

Publisher page

Abstract

Metalorganic chemical vapor deposition (MOCVD) is a promising technique for wafer-scale synthesis of MoS2 monolayers for 2D field-effect transistors (2D-FETs) and related devices. Epitaxial growth of MoS2 on sapphire provides films that are crystallographically well-oriented but typically contain low-angle grain boundaries (e.g., mirror twins), voids, and other defects depending on growth conditions and substrate characteristics. In this study, we investigate microstructure, optical properties, and field-effect characteristics of wafer-scale MoS2 monolayers grown by MOCVD on c-plane sapphire over a narrow window of growth temperatures (900–1000 °C). The density of low-angle grain boundaries in the MoS2 monolayer was found to decrease dramatically from 50% areal coverage for films grown at 900 °C to 5% at 1000 °C. This decrease in low-angle grain boundary density is correlated with an increase in the room-temperature photoluminescence intensity of A excitons and a decrease in the full-width-half maximum (FWHM) of the Raman A1g peak, which are typically indicative of a general reduction in defects in MoS2. However, the best transport properties (e.g., mean field-effect mobility mFE = 17.3 cm2/V s) were obtained in MoS2 monolayers grown at an intermediate temperature of 950 °C. It was found that as the growth temperature increased, small regions bound by high-angle boundaries begin to appear within the monolayer and increase in areal coverage, from ∼2% at 900 °C to ∼5% at 950 °C to ∼10% at 1000 °C. The growth temperature of 950 °C, therefore, provides an intermediate condition where the combined effects of low-angle and high-angle boundaries are minimized. The results of this study provide guidance on MOCVD growth and characterization that can be used to further optimize the performance of MoS2 2D-FETs.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: 2D Materials and Applications · Perovskite Materials and Applications · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

2D Crystal Consortium—Materials Innovation Platform, 1 Materials Research Institute, The Pennsylvania State University, University Park, Pennsylvania 16802

Department of Materials Science and Engineering, 2 The Pennsylvania State University, University Park, Pennsylvania 16802

Werkstoffe der Elektrotechnik and CENIDE, University of Duisburg-Essen 3 , Duisburg 47057, Germany

Department of Engineering Science and Mechanics, 4 The Pennsylvania State University, University Park, Pennsylvania 16802

Department of Metallurgical and Materials Engineering, Indian Institute of Technology Kharagpur 5 , Kharagpur 721302, India

School of Engineering, The University of Tokyo 6 , Tokyo 113-8656, Japan, Japan

Department of Solid-State Physics, Faculty of Physics and Applied Informatics, University of Lodz 7 , Pomorska 149/153, Lodz 90-236, Poland

Department of Electrical Engineering and Computer Science, The Pennsylvania State University 8 , University Park, Pennsylvania 16802

Funding

National Science Foundation · German Research Foundation · National Science Centre, Poland · Polsko-Amerykanska Komisja Fulbrighta · National Aeronautics and Space Administration · U.S. Air Office of Scientific Research and Clarkson Aerospace Corp.

References (28)

Show source-provided references
1. 2020 · 1.1.1
2. IEEE Trans. Electron. Dev. · 2015 · 62 · 345910.1109/TED.2015.2443039 ↗
3. Nature · 2015 · 520 · 65610.1038/nature14417 ↗
4. Nat. Nanotechnol. · 2023 · 18 · 45610.1038/s41565-023-01375-6 ↗
5. Nano Lett. · 2018 · 18 · 104910.1021/acs.nanolett.7b04521 ↗
6. Nanotechnology · 2018 · 29 · 42560210.1088/1361-6528/aad798 ↗
7. J. Cryst. Growth · 2017 · 464 · 10010.1016/j.jcrysgro.2016.11.020 ↗
8. ACS Nano · 2021 · 15 · 253210.1021/acsnano.0c06750 ↗
9. Nat. Nanotechnol. · 2021 · 16 · 120110.1038/s41565-021-00963-8 ↗
10. Nat. Nanotechnol. · 2022 · 17 · 3310.1038/s41565-021-01004-0 ↗
11. Nat. Nanotechnol. · 2023 · 18 · 129510.1038/s41565-023-01456-6 ↗
12. Nat. Mater. · 2013 · 12 · 55410.1038/nmat3633 ↗
13. Nano Lett. · 2021 · 21 · 648710.1021/acs.nanolett.1c01517 ↗
14. Nano Lett. · 2013 · 13 · 261510.1021/nl4007479 ↗
15. J. Cryst. Growth · 2019 · 527 · 12524710.1016/j.jcrysgro.2019.125247 ↗
16. Adv. Mater. Interfaces · 2023 · 10 · 220201610.1002/admi.202202016 ↗
17. Nanotechnology · 2018 · 29 · 05570610.1088/1361-6528/aaa1bd ↗
18. ACS Nano · 2010 · 4 · 269510.1021/nn1003937 ↗
19. Phys. Rev. B · 2015 · 91 · 19541110.1103/PhysRevB.91.195411 ↗
20. Nano Lett. · 2013 · 13 · 536110.1021/nl402875m ↗
21. Nanotechnology · 2014 · 25 · 46570110.1088/0957-4484/25/46/465701 ↗
22. APL Mater. · 2018 · 6 · 11110610.1063/1.5053699 ↗
23. Nano Lett. · 2013 · 13 · 362610.1021/nl4014748 ↗
24. J. Appl. Cryst. · 1976 · 9 · 40310.1107/S0021889876011709 ↗
25. J. Appl. Phys. · 1974 · 45 · 145610.1063/1.1663432 ↗
26. Nano Lett. · 2013 · 13 · 594410.1021/nl403036h ↗
27. Nat. Eletron. · 2021 · 4 · 78610.1038/s41928-021-00670-1 ↗
28. See supplementary material online for details of the MoS2 monolayers’ synthesis by MOCVD and characterization methods including AFM and FESEM imaging, in-plane XRD, Raman spectrum analysis, TEM imaging, 4D-STEM characterization, PL spectrum and PL mapping result, MoS2 monolayer transfer process and FET device fabrication and electrical characterization method.