Ultrahigh purity plasma-enhanced atomic layer deposition and electrical properties of epitaxial scandium nitride

Gilbert B. Rayner, Noel O’Toole, Bangzhi Liu, Jeffrey Shallenberger, Jiadi Zhu, Tomás Palacios, Piush Behera, Suraj Cheema, Blaine Johs, Nicholas A. Strnad

Publisher page

Abstract

Scandium nitride (ScN) by plasma-enhanced atomic layer deposition (PEALD) was demonstrated on silicon (100), sapphire (0001), and magnesium oxide (001) substrates under ultrahigh purity conditions using a new Sc precursor, bis(ethylcyclopentadienyl)scandium-chloride [ClSc(EtCp)2]. Out-of-plane x-ray diffraction patterns indicated single-crystal, cubic phase ScN deposited at 215 °C on sapphire (0001) and magnesium oxide (001) substrates, whereas phi-scans confirmed epitaxial growth. The ScN thin films grown on silicon with native oxide were polycrystalline with no preferential orientation. The ScN films showed a nitrogen-to-scandium ratio of approximately 1:1 measured by x-ray photoelectron spectroscopy, with ultra-low levels of elemental impurities including 2.5 at. % chlorine, 0.9 at. % carbon, and 0.4 at. % oxygen. ClSc(EtCp)2 and N2–H2 plasma were evaluated as ScN co-precursors at substrate temperatures ranging from 200 to 300 °C, where we identified an atomic layer deposition window between 200 and 215 °C. Images by field emission scanning electron microscopy (FESEM) on 43 nm-thick films grown on untreated silicon revealed columnar grains with lateral sizes ranging from 16 to 28 nm. ScN conformality across 4:1 aspect ratio silicon trench structures with 312 nm-wide openings was also imaged by FESEM showing a top-to-bottom thickness ratio of 75%. ScN electrical properties were evaluated by performing Hall measurements to determine mobility, free electron concentration, and resistivity. For ScN PEALD on magnesium oxide (001), the average mobility was 298 cm2/V s with a carrier concentration of 2.35 × 1019 cm−3. The average resistivity was 1.01 mΩ cm.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Semiconductor materials and devices · Metal and Thin Film Mechanics · ZnO doping and properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

The Kurt J. Lesker Company 1 , 1925 PA-51, Jefferson Hills, Pennsylvania 15025

Materials Research Institute, The Pennsylvania State University 2 , University Park, Pennsylvania 16802

Department of Electrical Engineering and Computer Science, Massachusetts Institute of Technology 3 , 77 Massachusetts Avenue, Cambridge, Massachusetts 02139

Research Laboratory of Electronics, Massachusetts Institute of Technology 4 , 77 Massachusetts Avenue, Cambridge, Massachusetts 02139

Department of Materials Science and Engineering, Massachusetts Institute of Technology 5 , 77 Massachusetts Avenue, Cambridge, Massachusetts 02139

Film Sense 6 , 500 South St. #7, Lincoln, Nebraska 68522

Army Research Directorate, DEVCOM Army Research Laboratory 7 , 2800 Powder Mill Road, Adelphi, Maryland 20783

Funding

Kurt J. Lesker Company

References (37)

Show source-provided references
1. Phys. Rev. B · 2021 · 104 · 07511810.1103/PhysRevB.104.075118 ↗
2. Phys. Rev. Appl. · 2018 · 9 · 03401910.1103/PhysRevApplied.9.034019 ↗
3. Phys. Rev. B · 2015 · 91 · 04510410.1103/PhysRevB.91.045104 ↗
4. J. Appl. Phys. · 2014 · 115 · 15350810.1063/1.4871656 ↗
5. Thin Solid Films · 2008 · 516 · 856910.1016/j.tsf.2008.05.050 ↗
6. J. Vac. Sci. Technol. A · 1998 · 16 · 241110.1116/1.581360 ↗
7. J. Appl. Phys. · 2001 · 90 · 180910.1063/1.1388161 ↗
8. Appl. Phys. Lett. · 2023 · 123 · 11210210.1063/5.0164058 ↗
9. Appl. Phys. Lett. · 2011 · 99 · 23211310.1063/1.3665945 ↗
10. J. Phys.: Condens. Matter · 2012 · 24 · 41530310.1088/0953-8984/24/41/415303 ↗
11. J. Appl. Phys. · 2013 · 113 · 15370410.1063/1.4801886 ↗
12. J. Microelectromech. Syst. · 2014 · 23 · 67210.1109/JMEMS.2013.2282743 ↗
13. Phys. Rev. B · 2017 · 96 · 19541710.1103/PhysRevB.96.195417 ↗
14. Appl. Phys. Lett. · 2020 · 116 · 15210310.1063/5.0004761 ↗
15. Phys. B · 2007 · 401–402 · 29610.1016/j.physb.2007.08.170 ↗
16. J. Cryst. Growth · 2009 · 311 · 329510.1016/j.jcrysgro.2009.03.044 ↗
17. Phys. Status Solidi C · 2010 · 7 · 177810.1002/pssc.200983494 ↗
18. Adv. Mater. · 2009 · 21 · 59310.1002/adma.200802611 ↗
19. J. Appl. Phys. · 2019 · 125 · 11410310.1063/1.5084945 ↗
20. Surf. Coat. Technol · 2017 · 309 · 41710.1016/j.surfcoat.2016.11.083 ↗
21. Appl. Phys. Lett. · 1999 · 74 · 303210.1063/1.124055 ↗
22. 1994 · 135
23. Vacuum · 2011 · 86 · 2310.1016/j.vacuum.2011.03.026 ↗
24. 2021 · 1
25. J. Microelectromech. Syst. · 2017 · 26 · 113210.1109/JMEMS.2017.2712101 ↗
26. IEEE Electron Device Lett. · 2020 · 41 · 177410.1109/LED.2020.3034576 ↗
27. Micromachines · 2022 · 13 · 88710.3390/mi13060887 ↗
28. IEEE Trans. Emerg. Top. Comput. · 2022 · 10 · 165710.1109/TETC.2021.3115495 ↗
29. J. Vac. Sci. Technol. A · 2023 · 41 · 05080110.1116/6.0002431 ↗
30. APL Mater. · 2020 · 8 · 07110110.1063/5.0011331 ↗
31. J. Vac. Sci. Technol. A · 2021 · 39 · 03240310.1116/6.0000724 ↗
32. J. Vac. Sci. Technol. A · 2022 · 40 · 04240310.1116/6.0001633 ↗
33. Appl. Surf. Sci. · 2003 · 211 · 13610.1016/S0169-4332(03)00250-2 ↗
34. J. Vac. Sci. Technol. A · 2020 · 38 · 06240810.1116/6.0000454 ↗
35. Chem. Mater. · 2004 · 16 · 544510.1021/cm048667y ↗
36. J. Mater. Sci.: Mater. Electron. · 2004 · 15 · 55510.1023/B:JMSE.0000032591.54107.2c ↗
37. Moustakas · 1996 · 197