Behavior of thin Ta-based films in the Cu/barrier/Si system
Source abstract
Abstract
This work concentrates on the diffusion barrier stability of very thin (10 or 20 nm) α- or β-Ta, TaN, Ta(O) and Ta(N,O) films in the Cu/barrier/Si system. Based on the classical theory of the thin film growth and know how of material transport in thin films, the various Ta-based films were classified according to their density of free short-circuit paths. Using scanning electron microscopy, transmission electron microscopy, glow discharge optical emission spectroscopy and secondary ion mass spectrometry, the 20 nm thin polycrystalline columnar-structured β-Ta films were found to be stable up to 500 °C for 1 h. After 1 h at 600 °C Cu3Si was formed due to short-circuit diffusion of Cu throughout the β-Ta films. The 20 nm thin giant-grained α-Ta films show equivalent performance to the β-Ta films. On the other hand, the 10 nm thin stuffed nanocrystalline face-centered-cubic (fcc) TaN films were able to protect the Si from Cu diffusion up to at least 600 °C/1 h. Ten nm thin amorphous-like Ta(N,O) and Ta(O) films also show barrier stability that is comparable to fcc TaN. While Ta(N,O) tends to recrystallize mainly into hexagonal-close-packed Ta2N above 500 °C, the Ta(O) remains amorphous even at 600 °C. Besides the amorphous-like microstructure, the high recrystallization temperature of Ta(O) is the reason why the introduction of 5 nm thin Ta(O) film into the Cu/5 nm Ta(O)/5 nm β-Ta/Si structure leads to a stability increase up to at least 600 °C for 1 h.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Copper Interconnects and Reliability · Metal and Thin Film Mechanics · Integrated Circuits and Semiconductor Failure Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Semiconductor and Microsystems Technology Laboratory, Dresden University of Technology, 01062 Dresden, Germany
Institute of Solid State and Materials Research, 01069 Dresden, Germany
References (32)
Show source-provided references
1. Microelectron. Eng. · 1997 · 37/38 · 2910.1016/S0167-9317(97)00091-9 ↗
2. Thin Solid Films · 1978 · 52 · 41510.1016/0040-6090(78)90184-0 ↗
3. MRS Bull. · 1994 · XIX · 30
4. J. Vac. Sci. Technol. · 1974 · 11 · 66610.1116/1.1312732 ↗
5. Trans. Faraday Soc. · 1961 · 57 · 119110.1039/tf9615701191 ↗
6. J. Electrochem. Soc. · 1995 · 142 · 310910.1149/1.2048697 ↗
7. Appl. Surf. Sci. · 1995 · 91 · 25710.1016/0169-4332(95)00128-X ↗
8. Microelectron. Eng. · 1997 · 33 · 26910.1016/S0167-9317(96)00054-8 ↗
9. Thin Solid Films · 1997 · 307 · 7910.1016/S0040-6090(97)00319-2 ↗
10. Microelectron. Eng. · 1997 · 37/38 · 24510.1016/S0167-9317(97)00118-4 ↗
11. Surf. Interface Anal. · 1997 · 25 · 52210.1002/(SICI)1096-9918(199706)25:7/8<522::AID-SIA262>3.0.CO;2-F ↗
12. Fresenius J. Anal. Chem. · 1996 · 355 · 84010.1007/s0021663550840 ↗
13. Herndon · 1993 · 256
14. Appl. Phys. Lett. · 1990 · 57 · 61710.1063/1.104249 ↗
15. J. Vac. Sci. Technol. A · 1990 · 8 · 379610.1116/1.576496 ↗
16. Appl. Surf. Sci. · 1996 · 99 · 26510.1016/0169-4332(96)00464-3 ↗
17. J. Appl. Phys. · 1993 · 71 · 5433
18. J. Appl. Phys. · 1993 · 73 · 30010.1063/1.353904 ↗
19. J. Vac. Sci. Technol. A · 1992 · 10 · 331810.1116/1.577818 ↗
20. J. Appl. Phys. · 1991 · 70 · 136910.1063/1.349594 ↗
21. J. Vac. Sci. Technol. B · 1996 · 14 · 326310.1116/1.588818 ↗
22. J. Mater. Sci.: Mater. Electron. · 1996 · 7 · 271
23. J. Electrochem. Soc. · 1997 · 144 · 180710.1149/1.1837684 ↗
24. Jpn. J. Appl. Phys., Part 1 · 1993 · 32 · 91110.1143/JJAP.32.911 ↗
25. J. Vac. Sci. Technol. B · 1996 · 14 · 674
26. J. Appl. Phys. · 1996 · 79 · 693210.1063/1.361518 ↗
27. Mater. Res. Soc. Symp. Proc. · 1991 · 203 · 387
28. J. Appl. Phys. · 1991 · 70 · 136910.1063/1.349594 ↗
29. IEEE Electron Device Lett. · 1991 · 12 · 32110.1109/55.82074 ↗
30. Proc. SPIE · 1992 · 1805 · 11
31. Appl. Surf. Sci. · 1991 · 53 · 37310.1016/0169-4332(91)90288-U ↗
32. Thin Solid Films · 1993 · 236 · 31910.1016/0040-6090(93)90689-M ↗