journal article·2003-07-01

Effects of Si addition on the microstructural evolution and hardness of Ti–Al–Si–N films prepared by the hybrid system of arc ion plating and sputtering techniques

In-Wook Park, Sung Ryong Choi, Mi-Hye Lee, Kwang Ho Kim

Publisher page

Abstract

Ti–Al–Si–N films were deposited on WC–Co substrates by the hybrid coating system of arc ion plating method for Ti–Al sources and dc magnetron sputtering technique for Si incorporation. The synthesized Ti–Al–Si–N films were revealed as composites of solid-solution (Ti,Al,Si)N crystallites and amorphous Si3N4 by instrumental analyses such as x-ray diffraction, high-resolution transmission electron microscopy, and x-ray photoelectron spectroscopy. The Si addition in Ti–Al–N films affected the refinement and uniform distribution of crystallites by percolation phenomenon of amorphous silicon nitride similar to that of the Si effect in TiN film. The solubility limit of Si in the Ti0.76Al0.24N crystal is believed to be about 6 at. %. No free Si was observed due to the very high ionization rate of nitrogen gas in the arc plasma. As the Si content increased up to about 9 at. %, the hardness of Ti–Al–N film steeply increased from 30 GPa to about 50 GPa. Ti–Al–Si–N films having the maximum hardness showed the nanocomposite microstructure consisting of fine (Ti,Al,Si)N crystallites, about 8 nm in size, dispersed uniformly in the amorphous Si3N4 matrix.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials Science and Engineering, Pusan National University, San 30, Jangjeon-Dong, Keumjung-Ku, Busan 609-735, South Korea

Technical Appraisal Center, Korea Technology Credit Guarantee Fund, Busan 600-777, South Korea

References (34)

Show source-provided references
1. Surf. Coat. Technol. · 1999 · 120 · 194
2. Wear · 2001 · 250 · 56110.1016/S0043-1648(01)00638-X ↗
3. Thin Solid Films · 1996 · 283 · 16510.1016/0040-6090(96)08766-4 ↗
4. Thin Solid Films · 1999 · 348 · 21010.1016/S0040-6090(99)00143-1 ↗
5. Surf. Coat. Technol. · 2001 · 141 · 23210.1016/S0257-8972(01)01237-3 ↗
6. J. Appl. Phys. · 1990 · 67 · 154210.1063/1.345664 ↗
7. Mater. Sci. Eng., A · 2003 · 342 · 5810.1016/S0921-5093(02)00259-9 ↗
8. J. Vac. Sci. Technol. A · 1986 · 4 · 271710.1116/1.573713 ↗
9. J. Vac. Sci. Technol. A · 1986 · 4 · 269510.1116/1.573708 ↗
10. Thin Solid Films · 1997 · 300 · 17110.1016/S0040-6090(96)09503-X ↗
11. Thin Solid Films · 1997 · 307 · 11310.1016/S0040-6090(97)00212-5 ↗
12. Surf. Coat. Technol. · 1995 · 76 · 499
13. Vacuum · 1999 · 53 · 12710.1016/S0042-207X(98)00407-2 ↗
14. Appl. Phys. Lett. · 1995 · 66 · 264010.1063/1.113110 ↗
15. Surf. Coat. Technol. · 2000 · 133 · 307
16. Surf. Coat. Technol. · 1998 · 108 · 241
17. J. Vac. Sci. Technol. A · 1999 · 17 · 240110.1116/1.581977 ↗
18. Thin Solid Films · 1995 · 268 · 6410.1016/0040-6090(95)06695-0 ↗
19. Thin Solid Films · 2001 · 398 · 397
20. Surf. Coat. Technol. · 2001 · 146 · 215
21. IEEE Trans. Plasma Sci. · 1994 · 22 · 104910.1109/27.370251 ↗
22. Physica C · 1981 · 104 · 9110.1016/0378-4363(81)90040-1 ↗
23. Surf. Coat. Technol. · 1999 · 120 · 388
24. Surf. Coat. Technol. · 1998 · 120 · 438
25. Surf. Coat. Technol. · 2002 · 298 · 243
26. Thin Solid Films · 2002 · 420 · 360
27. Thin Solid Films · 2002 · 420 · 371
28. Thin Solid Films · 1991 · 195 · 9910.1016/0040-6090(91)90262-V ↗
29. Thin Solid Films · 2000 · 365 · 10410.1016/S0040-6090(00)00653-2 ↗
30. Thin Solid Films · 1999 · 339 · 20310.1016/S0040-6090(98)01364-9 ↗
31. Plasma Chem. Plasma Process. · 1992 · 12 · 28710.1007/BF01447027 ↗
32. J. Vac. Sci. Technol. B · 1998 · 16 · 1910.1116/1.589778 ↗
33. J. Mater. Sci. · 1986 · 21 · 183710.1007/BF00547918 ↗
34. Surf. Coat. Technol. · 2001 · 146 · 201