Structural and electrical characteristics of Y2O3 films grown on oxidized Si(100) surface
Source abstract
Abstract
Heteroepitaxial Y2O3 films were grown on oxidized and clean Si (100) surfaces by ion assisted evaporation under an ultrahigh vacuum. The crystalline structure, crystallinity, morphology, and electrical properties were investigated using various techniques. The crystallinity assessed by x-ray diffraction and Rutherford backscattering spectroscopy shows that the films grown on the oxidized Si substrates have better crystallinity and smoother morphology compared to those on the clean Si. As the annealing temperature increases, the crystallinity and morphology are stable for the films grown on the oxidized Si, while those of the films grown on clean Si substrates degrade. The difference between the two films is attributed to the formation of hillocks and a chemical reaction at the interface between the film and SiO2. The low crystallinity, strain change, and the reaction of excess Y in the films grown on the clean Si contribute to the crystalline structure and the formation of hillock. These changes of crystallinity and morphology show that the films grown on the oxidized Si surface are more suitable for device applications. Thus, the films grown on the oxidized Si result in higher breakdown field strength and lower trap charge density than those on clean Si after the annealing treatment.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Ga2O3 and related materials · ZnO doping and properties · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Atomic-scale Surface Science Research Center and Department of Physics, Yonsei University, Seoul 120-749, Korea
Department of Ceramic Engineering, Yonsei University, Seoul 120-749, Korea
Department of Material Science and Engineering, Kwangju Institute of Science and Technology (K-JIST), Kwangju 500-712, Korea
References (25)
Show source-provided references
1. IEEE Electron Device Lett. · 1988 · 9 · 18010.1109/55.682 ↗
2. J. Mater. Res. · 1993 · 8 · 211210.1557/JMR.1993.2112 ↗
3. J. Appl. Phys. · 1992 · 71 · 504110.1063/1.350605 ↗
4. Jpn. J. Appl. Phys., Part 1 · 1991 · 60 · 934
5. J. Appl. Phys. · 1990 · 68 · 431610.1063/1.346228 ↗
6. Appl. Phys. Lett. · 1990 · 56 · 133210.1063/1.103202 ↗
7. Appl. Phys. Lett. · 1990 · 57 · 113710.1063/1.104220 ↗
8. Appl. Phys. Lett. · 1988 · 53 · 150610.1063/1.100431 ↗
9. Appl. Phys. Lett. · 1987 · 51 · 91910.1063/1.98801 ↗
10. Appl. Phys. Lett. · 1989 · 55 · 36010.1063/1.102420 ↗
11. Jpn. J. Appl. Phys., Part 1 · 1991 · 60 · 934
12. J. Vac. Sci. Technol. A · 1993 · 11 · 154810.1116/1.578503 ↗
13. Thin Solid Films · 1986 · 193 · 121
14. J. Cryst. Growth · 1995 · 147 · 13010.1016/0022-0248(94)00623-7 ↗
15. Appl. Phys. Lett. · 1997 · 71 · 90310.1063/1.119683 ↗
16. Phys. Rev. B · 1990 · 42 · 758710.1103/PhysRevB.42.7587 ↗
17. Phys. Rev. B · 1997 · 56 · 14
18. RCA Rev. · 1970 · 31 · 207
19. RCA Rev. · 1970 · 31 · 234
20. Nucl. Instrum. Methods Phys. Res. B · 1998 · 142 · 39310.1016/S0168-583X(98)00332-2 ↗
21. J. Appl. Phys. · 1999 · 86 · 19810.1063/1.370717 ↗
22. Thin Solid Films · 1999 · 349 · 26610.1016/S0040-6090(99)00174-1 ↗
23. J. Appl. Phys. · 1999 · 85 · 290910.1063/1.369056 ↗
24. J. Appl. Phys. · 1989 · 66 · 299910.1063/1.344184 ↗
25. Appl. Phys. Lett. · 1981 · 38 · 53510.1063/1.92442 ↗