journal article·2006-11-01

Influence of thermal annealing on the resistivity of titanium/platinum thin films

U. Schmid, H. Seidel

Publisher page

Abstract

In this study, the authors investigate the influence of thermal annealing up to temperatures of 700°C on the room-temperature resistivity of electron-beam-evaporated titanium/platinum thin films. Oxidized silicon wafers are used as the substrate. The titanium has a fixed thickness of 5nm and serves as an adhesion layer. The thickness of the platinum top is varied between 21 and 97nm. Up to annealing temperatures of 450°C, the film resistivity of the bilayer system is a linear correlation with the reciprocal platinum film thickness, as expected from the size effect. In this annealing regime, the change in intrinsic film stress dominates the electrical behavior. At annealing temperatures of 600°C and above, however, the diffusion of titanium into the top layer leads to an enhanced increase in film resistivity, especially at low platinum thicknesses. The onset of plastic deformation of the platinum layer causes an additional effect that decreases the electrical conductivity above average.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Semiconductor materials and devices · Copper Interconnects and Reliability · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Saarland University Department of Micromechanics, Microfluidics/Microactuators, , 66123 Saarbruecken, Germany

References (34)

Show source-provided references
1. J. Appl. Phys. · 1995 · 78 · 192610.1063/1.360230 ↗
2. Appl. Phys. Lett. · 2003 · 83 · 216010.1063/1.1610809 ↗
3. Thin Solid Films · 2003 · 436 · 3410.1016/S0040-6090(03)00523-6 ↗
4. Sens. Actuators B · 2001 · 73 · 110.1016/S0925-4005(00)00639-0 ↗
5. Sens. Actuators B · 2000 · 64 · 4210.1016/S0925-4005(99)00481-5 ↗
6. Sens. Actuators, A · 2001 · 94 · 3210.1016/S0924-4247(01)00668-9 ↗
7. J. Micromechatronics · 2005 · 3 · 1510.1163/156856305323383892 ↗
8. J. Micromechatronics · 2005 · 3 · 3310.1163/156856305323383900 ↗
9. G. Krötz and U. Schmid, German Patent No. DE 19945677 C1 (2001).
10. J. Am. Ceram. Soc. · 2005 · 88 · 218810.1111/j.1551-2916.2005.00403.x ↗
11. J. Appl. Phys. · 1993 · 73 · 176410.1063/1.353212 ↗
12. Thin Solid Films · 1997 · 300 · 12210.1016/S0040-6090(96)09452-7 ↗
13. J. Vac. Sci. Technol. · 1971 · 9 · 27110.1116/1.1316577 ↗
14. Sens. Actuators B · 2000 · 65 · 19010.1016/S0925-4005(99)00301-9 ↗
15. J. Micromech. Microeng. · 2003 · 13 · 11310.1088/0960-1317/13/4/319 ↗
16. J. Microelectromech. Syst. · 1998 · 7 · 12810.1109/84.661395 ↗
17. 1982
18. Phys. Rev. B · 1970 · 1 · 138210.1103/PhysRevB.1.1382 ↗
19. Thin Solid Films · 2005 · 489 · 31010.1016/j.tsf.2005.05.003 ↗
20. Phys. Rev. B · 1980 · 22 · 606510.1103/PhysRevB.22.6065 ↗
21. Appl. Surf. Sci. · 2000 · 158 · 21710.1016/S0169-4332(00)00021-0 ↗
22. J. Vac. Sci. Technol. A · 1984 · 2 · 21810.1116/1.572727 ↗
23. J. Appl. Phys. · 1994 · 75 · 23210.1063/1.355889 ↗
24. Surf. Rev. Lett. · 2004 · 11 · 46310.1142/S0218625X04006396 ↗
25. Appl. Phys. A: Mater. Sci. Process. · 1998 · 66 · 43510.1007/s003390050690 ↗
26. 1970
27. Thin Solid Films · 2001 · 394 · 284
28. Jpn. J. Appl. Phys., Part 1 · 1995 · 34 · 522010.1143/JJAP.34.5220 ↗
29. Jpn. J. Appl. Phys., Part 1 · 1995 · 34 · 494510.1143/JJAP.34.4945 ↗
30. J. Appl. Phys. · 1999 · 86 · 490210.1063/1.371458 ↗
31. J. Vac. Sci. Technol. · 1971 · 9 · 27110.1116/1.1316577 ↗
32. J. Appl. Phys. · 1990 · 67 · 623710.1063/1.345190 ↗
33. Acta Metall. Mater. · 1993 · 41 · 354110.1016/0956-7151(93)90234-J ↗
34. Thin Solid Films · 2004 · 466 · 12310.1016/j.tsf.2004.03.041 ↗