Degradation of ZrN films at high temperature under controlled atmosphere
Source abstract
Abstract
The degradation of ZrN films deposited onto Si substrates by unbalanced magnetron sputtering was investigated over temperatures of 300–1200°C in different atmospheres by analyzing changes in color and appearance, as well as microstructures. The atmospheres contained air, nitrogen, and forming gas (N2∕H2=9), which exhibited drastically different oxygen/nitrogen partial pressure ratios. The resultant degradation included mainly color changes and formation of blisters on the film surface. Color change was associated with the oxidation of the nitride film, which was analyzed by looking into the Gibbs free-energy changes at various temperatures and oxygen partial pressures. Two types of blisters occurred at different temperature ranges. Several large round blisters, denoted as A-type blisters, occurring at low temperatures originated from the large residual stress in the films. Many small irregular blisters, denoted as B-type blisters, appearing at relatively high temperatures resulted from the oxidation of the film.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Semiconductor materials and devices · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Materials Engineering , National Chung Hsing University, 250 Kuo Kuang Road, Taichung 402, Taiwan
References (22)
Show source-provided references
1. Thin Solid Films · 2000 · 375 · 12310.1016/S0040-6090(00)01225-6 ↗
2. J. Vac. Sci. Technol. A · 2003 · 21 · 67110.1116/1.1566784 ↗
3. J. Vac. Sci. Technol. A · 2003 · 21 · 69510.1116/1.1566787 ↗
4. J. Vac. Sci. Technol. A · 1986 · 4 · 266110.1116/1.573700 ↗
5. Thin Solid Films · 1983 · 107 · 14110.1016/0040-6090(83)90016-0 ↗
6. J. Vac. Sci. Technol. B · 2000 · 18 · 133310.1116/1.591382 ↗
7. Thin Solid Films · 1983 · 107 · 11110.1016/0040-6090(83)90013-5 ↗
8. Thin Solid Films · 1996 · 281–282 · 298
9. Thin Solid Films · 1997 · 303 · 24610.1016/S0040-6090(97)00069-2 ↗
10. Thin Solid Films · 1996 · 290–291 · 289
11. Thin Solid Films · 1996 · 280 · 26510.1016/0040-6090(95)08194-1 ↗
12. Proc. R. Soc. London, Ser. A · 1909 · 82 · 17210.1098/rspa.1909.0021 ↗
13. Barin · 1995 · 187810.1002/9783527619825 ↗
14. Thin Solid Films · 2002 · 405 · 16210.1016/S0040-6090(01)01762-X ↗
15. 1978 · 87
16. Phys. Rev. B · 1991 · 44 · 1351910.1103/PhysRevB.44.13519 ↗
17. Surf. Coat. Technol. · 2003 · 168 · 4310.1016/S0257-8972(03)00007-0 ↗
18. Surf. Coat. Technol. · 1988 · 34 · 12310.1016/0257-8972(88)90073-4 ↗
19. Metall. Trans. A · 1989 · 20 · 221710.1007/BF02666659 ↗
20. Thin Solid Films · 1996 · 281–282 · 298
21. Cardarelli · 2000 · 36210.1007/978-1-4471-3648-4 ↗
22. 1976 · 197