journal article·2014-01-01

Capacitance and conductance versus voltage characterization of Al2O3 layers prepared by plasma enhanced atomic layer deposition at 25 °C≤ T ≤ 200 °C

Karsten Henkel, Hassan Gargouri, Bernd Gruska, Michael Arens, Massimo Tallarida, Dieter Schmeißer

Publisher page

Abstract

In this work, plasma enhanced atomic layer deposited (PE-ALD) samples were prepared at substrate temperatures in the range between room temperature (RT) and 200 °C and investigated by capacitance–voltage and conductance–voltage recordings. The measurements are compared to standard thermal atomic layer deposition (T-ALD) at 200 °C. Very low interface state density (Dit) ∼1011 eV−1 cm−2 could be achieved for the PE-ALD process at 200 °C substrate temperature after postdeposition anneal (PDA) in forming gas at 450 °C. The PDA works very effectively for both the PE-ALD and T-ALD at 200 °C substrate temperature delivering also similar values of negative fixed charge density (Nfix) around −2.5 × 1012 cm−2. At the substrate temperature of 150 °C, highest Nfix (−2.9 × 1012 cm−2) and moderate Dit (2.7 × 1011 eV−1 cm−2) values were observed. The as deposited PE-ALD layer at RT shows both low Dit in the range of (1 to 3) × 1011 eV−1 cm−2 and low Nfix (−4.4 × 1011 cm−2) at the same time. The dependencies of Nfix, Dit, and relative permittivity on the substrate temperatures and its adjustability are discussed.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Semiconductor materials and devices · Electronic and Structural Properties of Oxides · ZnO doping and properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Applied Physics and Sensors, Brandenburg University of Technology Cottbus-Senftenberg , K.-Wachsmann-Allee 17, D-03046 Cottbus, Germany

Sentech Instruments GmbH , Schwarzschildstraße 2, 12489 Berlin, Germany

References (42)

Show source-provided references
1. Adv. Mater. · 2007 · 19 · 342510.1002/adma.200700079 ↗
2. Chem. Rev. · 2010 · 110 · 11110.1021/cr900056b ↗
3. J. Vac. Sic. Technol. A · 2012 · 30 · 04080210.1116/1.4728205 ↗
4. J. Vac. Sci. Technol. A · 2011 · 29 · 05080110.1116/1.3609974 ↗
5. Semicond. Sci. Technol. · 2012 · 27 · 07401010.1088/0268-1242/27/7/074010 ↗
6. Phys. Status Solidi C · 2011 · 8 · 128710.1002/pssc.201084011 ↗
7. Org. Electron. · 2010 · 11 · 189610.1016/j.orgel.2010.08.020 ↗
8. Phys. Status Solidi A · 2011 · 208 · 31710.1002/pssa.201026404 ↗
9. J. Appl. Phys. · 2003 · 94 · 256310.1063/1.1590414 ↗
10. IOP Conf. Series: Mater. Sci. Eng. · 2010 · 8 · 01203610.1088/1757-899X/8/1/012036 ↗
11. J. Nanopart. Res. · 2011 · 13 · 597510.1007/s11051-011-0319-x ↗
12. Chem. Mater. · 2011 · 23 · 315910.1021/cm200276z ↗
13. Chem. Mater. · 2004 · 16 · 63910.1021/cm0304546 ↗
14. Phys. Status Solidi C · 2010 · 7 · 39810.1002/pssc.200982496 ↗
15. J. Vac. Sci. Technol. A · 2012 · 30 · 01080310.1116/1.3672027 ↗
16. J. Phys. Chem. Lett. · 2010 · 1 · 161110.1021/jz100361f ↗
17. J. Phys. Chem. C · 2010 · 114 · 1004810.1021/jp1023229 ↗
18. Chem. Sci. · 2011 · 2 · 73710.1039/c0sc00578a ↗
19. J. Electrochem. Soc. · 2010 · 157 · A7510.1149/1.3258274 ↗
20. Appl. Phys. Lett. · 2006 · 89 · 13150510.1063/1.2357886 ↗
21. J. Electrochem. Soc. · 2005 · 152 · F4910.1149/1.1884130 ↗
22. J. Phys. Chem. C · 2008 · 112 · 1953010.1021/jp804296a ↗
23. J. Appl. Phys. · 2002 · 92 · 673910.1063/1.1515951 ↗
24. J. Electrochem. Soc. · 2010 · 157 · G24110.1149/1.3491381 ↗
25. J. Electrochem. Soc. · 2011 · 158 · G2110.1149/1.3517430 ↗
26. Electrochem. Solid-State Lett. · 2011 · 14 · H110.1149/1.3501970 ↗
27. J. Appl. Phys. · 2008 · 104 · 04490310.1063/1.2963707 ↗
28. Electrochem. Solid-State Lett. · 2004 · 7/8 · F4510.1149/1.1756541 ↗
29. J. Appl. Phys. · 2012 · 111 · 09371310.1063/1.4709729 ↗
30. Beilstein J. Nanotechnol. · 2013 · 4 · 73210.3762/bjnano.4.83 ↗
31. K. Henkel, “Electrical investigations on praseodymium oxide/aluminum oxynitride containing metal–insulator–semiconductor stacks and on metal–ferroelectric–insulator–semiconductor structures consisting of poly(vinylidene fluoride trifluoroethylene),” Ph.D. thesis, Brandenburg University of Technology, Germany (Shaker-Verlag, Aachen, 2009).
32. 1982
33. 1981
34. 1998
35. J. Vac. Sci. Technol. A · 2001 · 19 · 135310.1116/1.1379316 ↗
36. Thin Solid Films · 2002 · 413 · 18610.1016/S0040-6090(02)00438-8 ↗
37. Appl. Phys. Lett. · 2006 · 89 · 04211210.1063/1.2240736 ↗
38. Solid State Technol. · 2005 · 48/9 · 43
39. Phys. Rev. B · 2006 · 73 · 05410810.1103/PhysRevB.73.054108 ↗
40. J. Phys. Chem. Ref. Data · 1980 · 9 · 129110.1063/1.555632 ↗
41. J. Vac. Sci. Technol. B · 1994 · 12 · 44110.1116/1.587141 ↗
42. Appl. Phys. Lett. · 2012 · 100 · 20210710.1063/1.4718596 ↗