journal article·2016-07-01

Surface passivation of Fe3O4 nanoparticles with Al2O3 via atomic layer deposition in a rotating fluidized bed reactor

Chen-Long Duan, Zhang Deng, Kun Cao, Hong-Feng Yin, Bin Shan, Rong Chen

Publisher page

Abstract

Iron(II,III) oxide (Fe3O4) nanoparticles have shown great promise in many magnetic-related applications such as magnetic resonance imaging, hyperthermia treatment, and targeted drug delivery. Nevertheless, these nanoparticles are vulnerable to oxidation and magnetization loss under ambient conditions, and passivation is usually required for practical applications. In this work, a home-built rotating fluidized bed (RFB) atomic layer deposition (ALD) reactor was employed to form dense and uniform nanoscale Al2O3 passivation layers on Fe3O4 nanoparticles. The RFB reactor facilitated the precursor diffusion in the particle bed and intensified the dynamic dismantling of soft agglomerates, exposing every surface reactive site to precursor gases. With the aid of in situ mass spectroscopy, it was found that a thicker fluidization bed formed by larger amount of particles increased the residence time of precursors. The prolonged residence time allowed more thorough interactions between the particle surfaces and the precursor gas, resulting in an improvement of the precursor utilization from 78% to nearly 100%, even under a high precursor feeding rate. Uniform passivation layers around the magnetic cores were demonstrated by both transmission electron microscopy and the statistical analysis of Al mass concentrations. Individual particles were coated instead of the soft agglomerates, as was validated by the specific surface area analysis and particle size distribution. The results of thermogravimetric analysis suggested that 5 nm-thick ultrathin Al2O3 coatings could effectively protect the Fe3O4 nanoparticles from oxidation. The x-ray diffraction patterns also showed that the magnetic core crystallinity of such passivated nanoparticles could be well preserved under accelerated oxidation conditions. The precise thickness control via ALD maintained the saturation magnetization at 66.7 emu/g with a 5 nm-thick Al2O3 passivation layer. This good preservation of the magnetic properties with superior oxidation resistance will be beneficial for practical magnetic-based applications.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Catalytic Processes in Materials Science · Electrohydrodynamics and Fluid Dynamics · Iron oxide chemistry and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Huazhong University of Science and Technology State Key Laboratory of Digital Manufacturing Equipment and Technology, School of Mechanical Science and Engineering, , 1037 Luoyu Road, Wuhan, Hubei 430074, People's Republic of China

Chinese Academy of Sciences Ningbo Institute of Material Technology and Engineering, , Ningbo, Zhejiang 315201, People's Republic of China

Huazhong University of Science and Technology State Key Laboratory of Material Processing and Die and Mould Technology, School of Materials Science and Engineering, , 1037 Luoyu Road, Wuhan, Hubei 430074, People's Republic of China

Huazhong University of Science and Technology State Key Laboratory of Digital Manufacturing Equipment and Technology, School of Mechanical Science and Engineering, School of Optical and Electronic Information, , 1037 Luoyu Road, Wuhan, Hubei 430074, People's Republic of China

Funding

Changjiang Scholars and Innovative Research Teams in Universities · the Fundamental Research Funds for the Centural Universities · the Hubei Province Funds for Distinguished Young Scientists · the State Key Laboratory of Digital Manufacturing Equipment and Technology Funding

References (44)

Show source-provided references
1. Molecules · 2014 · 19 · 2150610.3390/molecules191221506 ↗
2. Int. J. Nanomed. · 2015 · 10 · 331510.2147/ijn.s68719 ↗
3. J. Vac. Sci. Technol., A · 2012 · 30 · 04151410.1116/1.4727737 ↗
4. J. Phys.: Condens. Matter · 2012 · 24 · 26600710.1088/0953-8984/24/26/266007 ↗
5. Glass Phys. Chem. · 2013 · 39 · 32910.1134/S1087659613030164 ↗
6. Chem. Mater. · 2012 · 24 · 457210.1021/cm302828d ↗
7. J. Vac. Sci. Technol., A · 2012 · 30 · 04080210.1116/1.4728205 ↗
8. J. Mater. Chem. · 2012 · 22 · 823510.1039/c2jm30472d ↗
9. Biosens. Bioelectron. · 2011 · 26 · 300510.1016/j.bios.2010.12.003 ↗
10. Surf. Coat. Technol. · 2008 · 202 · 430210.1016/j.surfcoat.2008.04.001 ↗
11. Nanotechnology · 2007 · 18 · 34560310.1088/0957-4484/18/34/345603 ↗
12. Chem. Eng. Sci. · 2007 · 62 · 619910.1016/j.ces.2007.07.013 ↗
13. Surf. Coat. Technol. · 2009 · 204 · 110.1016/j.surfcoat.2009.06.025 ↗
14. Adv. Mater. · 2012 · 24 · 101710.1002/adma.201104129 ↗
15. J. Mater. Chem. A · 2013 · 1 · 464710.1039/c3ta01665j ↗
16. J. Vac. Sci. Technol., A · 2015 · 33 · 01a12910.1116/1.4902085 ↗
17. Chem. Rev. · 2010 · 110 · 11110.1021/cr900056b ↗
18. Chem. Eng. J. · 2015 · 259 · 21310.1016/j.cej.2014.07.105 ↗
19. S. M. George , U.S. patent 6,913,827 (5 July 2005);
20. S. M. George , U.S. patent 6,713,177 (30 March 2004);
21. S. M. George , U.S. patent 6,613,383 (2 September 2003).
22. Powder Technol. · 2012 · 221 · 1310.1016/j.powtec.2011.12.020 ↗
23. Angew. Chem. Int. Ed. · 2010 · 49 · 254710.1002/anie.200907168 ↗
24. J. Vac. Sci. Technol., A · 2014 · 32 · 01080210.1116/1.4851676 ↗
25. J. Vac. Sci. Technol., A · 2007 · 25 · 6710.1116/1.2393299 ↗
26. Surf. Coat. Technol. · 2012 · 213 · 18310.1016/j.surfcoat.2012.10.045 ↗
27. Nanotechnology · 2005 · 16 · S37510.1088/0957-4484/16/7/010 ↗
28. Chem. Vap. Deposition · 2005 · 11 · 42010.1002/cvde.200506392 ↗
29. J. Vac. Sci. Technol., A · 2012 · 30 · 01A10810.1116/1.3644952 ↗
30. J. Am. Ceram. Soc. · 2006 · 89 · 307010.1111/j.1551-2916.2006.01216.x ↗
31. Powder Technol. · 2008 · 183 · 35610.1016/j.powtec.2008.01.025 ↗
32. Surf. Coat. Technol. · 2007 · 201 · 916310.1016/j.surfcoat.2007.05.002 ↗
33. Powder Technol. · 2005 · 160 · 14910.1016/j.powtec.2005.08.019 ↗
34. J. Nanopart. Res. · 2012 · 14 · 73710.1007/s11051-012-0737-4 ↗
35. Chem. Eng. Sci. · 2014 · 106 · 29310.1016/j.ces.2013.11.018 ↗
36. Chem. Eng. Process. · 2011 · 50 · 7710.1016/j.cep.2010.11.010 ↗
37. AICHE J. · 2006 · 52 · 240110.1002/aic.10826 ↗
38. Chem. Eng. J. · 2012 · 207 · 19510.1016/j.cej.2012.06.048 ↗
39. Chem. Eng. J. · 2000 · 78 · 10710.1016/S1385-8947(00)00148-0 ↗
40. Rev. Sci. Instrum. · 2015 · 86 · 07510110.1063/1.4926349 ↗
41. 2012
42. Chem. Eng. J. · 2015 · 268 · 38410.1016/j.cej.2015.01.067 ↗
43. Surf. Sci. · 1995 · 322 · 1310.1016/0039-6028(95)90033-0 ↗
44. Nanoscale · 2011 · 3 · 70110.1039/C0NR00497A ↗