Abstract
TiSiN ultrathin films (10–50 Å) deposited by reactive magnetron sputtering from TixSiy targets were used as anticorrosion overcoats to protect Co-containing recording media. Films’ growth, structure, composition, resistance against hydrolysis, and anticorrosion performances were studied by spectroscopy (x-ray reflectivity and diffraction, ellipsometry, x-ray photoelectron spectroscopy, Fourier transform infrared reflection–absorption spectroscopy) and simulated by molecular dynamics (using modified Tersoff-type interatomic interactions). TiSiN ultrathin overcoats were found to be dense amorphous oxynitrides containing Ti–O–Si linkages. The conversion of SiNx into SiOx by hydrolysis was prevented by introducing less than 20 at. % of Ti in the films. Thanks to the formation of Ti–O–Si linkages which densify the films and reduce oxygen diffusion, good corrosion protection of the magnetic media was achieved down to 28 Å TiSiN overcoat thickness.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Semiconductor materials and devices · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Hitachi Global Storage Technologies Inc. , San Jose Research Center, 3403 Yerba Buena Road, San Jose, California 95135
Hitachi Global Storage Technologies Inc. , Material Laboratory at San Jose, 5601 Great Oaks Parkway, San Jose, California 95119
Hitachi Ltd., Hitachi Research Laboratory, 832-2 Horiguchi, Hitachinaka, Ibaraki 312-0034, Japan
References (31)
Show source-provided references
1. IEEE Trans. Magn. · 2002 · 38 · 171110.1109/TMAG.2002.1017761 ↗
2. IEEE Trans. Magn. · 2003 · 39 · 71610.1109/TMAG.2003.808999 ↗
3. IEEE Trans. Magn. · 2000 · 36 · 11010.1109/20.824434 ↗
4. J. Vac. Sci. Technol. · 2003 · 21 · 189510.1116/1.1615974 ↗
5. Solid State Technol. · 2001 · 44 · 87
6. Q. Dai, B. Marchon, M. A. Scarpulla, R. L. White, and B. K. Yen, U.S. patent 6–586 (1 July 2003).
7. J. Mater. Sci. · 1976 · 11 · 50010.1007/BF00540931 ↗
8. J. Electrochem. Soc. · 1976 · 123 · 56010.1149/1.2132877 ↗
9. Chem. Mater. · 1989 · 1 · 19410.1021/cm00002a006 ↗
10. JSME Int. J., Ser. B · 2004 · 47 · 47010.1299/jsmeb.47.470 ↗
11. J. Appl. Phys. · 1997 · 81 · 65610.1063/1.364133 ↗
12. Thin Solid Films · 1995 · 268 · 6410.1016/0040-6090(95)06695-0 ↗
13. J. Vac. Sci. Technol. · 1999 · 17 · 240110.1116/1.581977 ↗
14. Palik · 1985
15. 2006
16. 1997
17. 2003
18. J. Appl. Phys. · 2001 · 90 · 205710.1063/1.1385803 ↗
19. Appl. Phys. Lett. · 1998 · 73 · 386610.1063/1.122919 ↗
20. J. Appl. Phys. · 1995 · 77 · 434310.1063/1.359459 ↗
21. J. Appl. Phys. · 2000 · 87 · 132210.1063/1.372017 ↗
22. Thin Solid Films · 1998 · 326 · 17110.1016/S0040-6090(98)00573-2 ↗
23. J. Solid State Chem. · 2006 · 179 · 138310.1016/j.jssc.2006.01.067 ↗
24. Phys. Rev. · 1963 · 130 · 219310.1103/PhysRev.130.2193 ↗
25. Thin Solid Films · 2007 · 515 · 478810.1016/j.tsf.2006.11.155 ↗
26. 2003
27. IEEE Trans. Magn. · 2003 · 39 · 245010.1109/TMAG.2003.816434 ↗
28. IEEE Trans. Magn. · 2006 · 42 · 250710.1109/TMAG.2006.878629 ↗
29. J. Phys. D: Appl. Phys. · 2009 · 42 · 22530810.1088/0022-3727/42/22/225308 ↗
30. Corros. Sci. · 2010 · 52 · 125810.1016/j.corsci.2010.01.004 ↗
31. IEEE Trans. Magn. · 2010 · 46 · 9210.1109/TMAG.2009.2034473 ↗