Atomic layer deposition of environmentally benign SnTiOx as a potential ferroelectric material

Siliang Chang, Sathees Kannan Selvaraj, Yoon-Young Choi, Seungbum Hong, Serge M. Nakhmanson, Christos G. Takoudis

Abstract

Inspired by the need to discover environmentally friendly, lead-free ferroelectric materials, here the authors report the atomic layer deposition of tin titanate (SnTiOx) aiming to obtain the theoretically predicted perovskite structure that possesses ferroelectricity. In order to establish the growth conditions and probe the film structure and ferroelectric behavior, the authors grew SnTiOx films on the commonly used Si(100) substrate. Thin films of SnTiOx have been successfully grown at a deposition temperature of 200 °C, with a Sn/Ti atomic layer deposition (ALD) cycle ratio of 2:3 and postdeposition heat treatments under different conditions. X-ray photoelectron spectroscopy revealed excellent composition tunability of ALD. X-ray diffraction spectra suggested anatase phase for all films annealed at 650 and 350 °C, with peak positions shifted toward lower 2-theta angles indicating enlarged unit cell volume. The film annealed in O2 at 350 °C exhibited piezoresponse amplitude and phase hysteresis loops, indicative of the existence of switchable polarization.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Semiconductor materials and devices · Electronic and Structural Properties of Oxides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

University of Illinois at Chicago Department of Chemical Engineering, , Chicago, Illinois 60607

Argonne National Laboratory Materials Science Division, , Lemont, Illinois 60439

University of Connecticut Department of Materials Science and Engineering, Institute of Materials Science, , Storrs, Connecticut 06269

University of Illinois at Chicago Department of Bioengineering and Chemical Engineering, , Chicago, Illinois 60607

Funding

Division of Materials Research · Division of Engineering Education and Centers · Division of Chemical, Bioengineering, Environmental, and Transport Systems

References (23)

Show source-provided references
1. Mater. Res. Soc. Symp. Proc. · 2003 · 748 · U3.13.110.1557/PROC-748-U3.13 ↗
2. Jpn. J. Appl. Phys. · 2008 · 47 · 773510.1143/JJAP.47.7735 ↗
3. Chem. Phys. · 2009 · 355 · 4310.1016/j.chemphys.2008.11.002 ↗
4. Phys. Rev. B · 2011 · 84 · 24512610.1103/PhysRevB.84.245126 ↗
5. Int. J. Mod. Phys. B · 2013 · 27 · 135014410.1142/S0217979213501440 ↗
6. Phys. Solid State · 2009 · 51 · 36210.1134/S1063783409020279 ↗
7. Chem. Mater. · 1998 · 10 · 259210.1021/cm9802797 ↗
8. Cryst. Growth Des. · 2011 · 11 · 142210.1021/cg200333q ↗
9. J. Cryst. Growth · 2011 · 322 · 3310.1016/j.jcrysgro.2011.03.004 ↗
10. J. Cryst. Growth · 2014 · 398 · 1810.1016/j.jcrysgro.2014.04.006 ↗
11. Electrochem. Solid-State Lett. · 2010 · 13 · G7510.1149/1.3457485 ↗
12. Chem. Mater. · 2012 · 24 · 373210.1021/cm301864c ↗
13. ACS Nano · 2015 · 9 · 180910.1021/nn5067232 ↗
14. ECS J. Solid State Sci. Technol. · 2012 · 1 · N10710.1149/2.013206jss ↗
15. J. Vac. Sci. Technol., A · 2014 · 32 · 01A11210.1116/1.4837915 ↗
16. J. Appl. Phys. · 2005 · 97 · 12130110.1063/1.1940727 ↗
17. CrystEngComm · 2013 · 15 · 994910.1039/c3ce40893k ↗
18. Chem. Mater. · 2013 · 25 · 293410.1021/cm303703r ↗
19. J. Hazard. Mater. · 2007 · 140 · 6910.1016/j.jhazmat.2006.06.057 ↗
21. ACS Nano · 2011 · 5 · 910410.1021/nn203342v ↗
22. ACS Nano · 2012 · 6 · 702610.1021/nn3020757 ↗
23. J. Appl. Phys. · 2015 · 118 · 07201310.1063/1.4927811 ↗