journal article·2017-11-01

Effect of Mo on the thermal stability, oxidation resistance, and tribo-mechanical properties of arc evaporated Ti-Al-N coatings

Stefan A. Glatz, Vincent Moraes, Christian M. Koller, Helmut Riedl, Hamid Bolvardi, Szilárd Kolozsvári, Paul H. Mayrhofer

Publisher page

Abstract

The general tendency in industrial machining and forming operations toward further reduced operation time and increased efficiency requires continuous improvements of protective coatings regarding their tribo-mechanical properties. Alloying arc evaporated Ti1-xAlxN with small amounts of molybdenum (Mo) has shown very promising results to further improve the tribological properties of the industrially widely used Ti-Al-N. Therefore, the authors study in detail the effect of Mo on the thermo-mechanical properties of Ti1-xAlxN coatings, as well as their wear behavior at elevated temperatures. First principle density functional theory (DFT) calculations are conducted for face-centered cubic c-Al1-yMoyN, c-Ti1-yMoyN, and c-Ti1-x-yAlxMoyN showing increasing energy of formation with increasing Mo incorporation for all structures investigated. However, the thereby (DFT) obtained/calculated lattice parameters for comparable compositions perfectly matches with those of the single-phase face-centered cubic structured c-Ti0.55Al0.42Mo0.03N, c-Ti0.53Al0.41Mo0.06N, and c-Ti0.50Al0.38Mo0.12N coatings studied. These coatings have an as deposited hardness of about 28 GPa, which can be maintained upon vacuum annealing up to Ta = 800 °C. At higher temperatures, their hardness decreases as the formation of the weaker w-AlN and Mo3Al phases occurs. In contrast to that, the abrasive wear of Mo-containing c-Ti1-x-yAlxMoyN during dry-sliding high temperature ball-on-disk tests (against 6 mm alumina balls at 700 °C) is significantly reduced to 1–2.0 × 10−6 mm3/N m, as compared to the Mo-free Ti0.56Al0.44N counterpart. This is the result of the presence of solid lubricant MoO3 phases in the wear tracks of the arc evaporated c-Ti1-x-yAlxMoyN coatings investigated—confirmed by a combined energy dispersive spectroscopy and x-ray photoelectron spectroscopy analysis. Based on their findings, the authors can conclude that the addition of up to 12 at.% Mo (of the metal fraction) to Ti0.56Al0.44N significantly improves their high temperature wear resistance by simultaneously keeping the outstanding coating characteristics of pure Ti1-xAlxN.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · MXene and MAX Phase Materials · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Christian Doppler Laboratory for Application Oriented Coating Development, Institute of Materials Science and Technology, TU Wien , 1060 Vienna, Austria

Oerlikon Balzers, Oerlikon Surface Solutions AG , 9496 Balzers, Liechtenstein

Plansee Composite Materials GmbH , 86983 Lechbruck am See, Germany

Institute of Materials Science and Technology, TU Wien , 1060 Vienna, Austria

Funding

Christian Doppler Forschungsgesellschaft

References (54)

Show source-provided references
1. Surf. Coat. Technol. · 1995 · 76–77 · 71910.1016/0257-8972(95)02499-9 ↗
2. J. Vac. Sci. Technol., A · 1992 · 10 · 174910.1116/1.577742 ↗
3. Int. J. Mater. Res. · 2007 · 98 · 105410.3139/146.101570 ↗
4. J. Eur. Ceram. Soc. · 1997 · 17 · 197110.1016/S0955-2219(97)00050-2 ↗
5. J. Appl. Phys. · 2011 · 110 · 2351510.1063/1.3610451 ↗
6. J. Vac. Sci. Technol., A · 1986 · 4 · 271710.1116/1.573713 ↗
7. Surf. Coat. Technol. · 2011 · 206 · 295410.1016/j.surfcoat.2011.12.028 ↗
8. Vacuum · 2000 · 57 · 110.1016/S0042-207X(00)00143-3 ↗
9. Prog. Mater. Sci. · 2006 · 51 · 103210.1016/j.pmatsci.2006.02.002 ↗
10. Surf. Coat. Technol. · 1996 · 86–87 · 73910.1016/S0257-8972(96)03063-0 ↗
11. Surf. Coat. Technol. · 2005 · 200 · 240910.1016/j.surfcoat.2004.08.208 ↗
12. J. Appl. Phys. · 2016 · 119 · 6530410.1063/1.4941533 ↗
13. Vacuum · 2014 · 106 · 4910.1016/j.vacuum.2014.03.006 ↗
14. J. Vac. Sci. Technol., A · 2015 · 33 · 05E12910.1116/1.4929536 ↗
15. Surf. Coat. Technol. · 2014 · 257 · 24710.1016/j.surfcoat.2014.04.046 ↗
16. Wear · 2001 · 251 · 106810.1016/S0043-1648(01)00764-5 ↗
17. Surf. Coat. Technol. · 2007 · 202 · 105010.1016/j.surfcoat.2007.07.045 ↗
18. Surf. Coat. Technol. · 2005 · 200 · 173110.1016/j.surfcoat.2005.08.044 ↗
19. Acta Crystallogr. · 1953 · 6 · 49510.1107/S0365110X53001381 ↗
20. Acta Chem. Scand. · 1951 · 5 · 58110.3891/acta.chem.scand.05-0581 ↗
21. Surf. Coat. Technol. · 2006 · 201 · 333510.1016/j.surfcoat.2006.07.067 ↗
22. 2011
23. Surf. Coat. Technol. · 2017 · 311 · 33010.1016/j.surfcoat.2017.01.001 ↗
24. Int. J. Refract. Met. Hard Mater. · 2009 · 27 · 50210.1016/j.ijrmhm.2008.06.008 ↗
25. Surf. Coat. Technol. · 2004 · 177–178 · 34110.1016/j.surfcoat.2003.09.024 ↗
26. Thin Solid Films · 2012 · 520 · 408010.1016/j.tsf.2012.01.030 ↗
27. 2016
28. J. Electron Spectrosc. Relat. Phenom. · 1976 · 8 · 12910.1016/0368-2048(76)80015-1 ↗
29. 1993
30. “NIST X-Ray Photoelectron Spectroscopy Database, Version 4.1,” National Institute of Standards and Technology, Gaithersburg, 2012, http://srdata.nist.gov/xps/
31. J. Mater. Res. · 1992 · 7 · 156410.1557/JMR.1992.1564 ↗
32. Phys. Rev. B · 1994 · 47 · 55810.1103/PhysRevB.47.558 ↗
33. Comput. Mater. Sci. · 1996 · 6 · 1510.1016/0927-0256(96)00008-0 ↗
34. Phys. Rev. B · 1996 · 54 · 1116910.1103/PhysRevB.54.11169 ↗
35. Phys. Rev. Lett. · 1996 · 77 · 386510.1103/PhysRevLett.77.3865 ↗
36. Calphad · 2013 · 42 · 1310.1016/j.calphad.2013.06.006 ↗
37. Acta Mater. · 2016 · 107 · 27310.1016/j.actamat.2016.01.063 ↗
38. Phys. Rev. B · 2010 · 81 · 10410710.1103/PhysRevB.81.104107 ↗
39. Surf. Coat. Technol. · 2015 · 275 · 21410.1016/j.surfcoat.2015.05.017 ↗
40. Thin Solid Films · 2011 · 519 · 550310.1016/j.tsf.2011.03.139 ↗
41. Appl. Phys. Lett. · 2010 · 97 · 15190110.1063/1.3495783 ↗
42. Appl. Phys. Lett. · 2003 · 83 · 204910.1063/1.1608464 ↗
43. Scr. Mater. · 2010 · 63 · 80710.1016/j.scriptamat.2010.06.020 ↗
44. Surf. Coat. Technol. · 2005 · 191 · 38410.1016/j.surfcoat.2004.04.056 ↗
45. Acta Mater. · 2007 · 55 · 144110.1016/j.actamat.2006.09.045 ↗
46. Scr. Mater. · 2009 · 61 · 72510.1016/j.scriptamat.2009.06.015 ↗
47. Surf. Coat. Technol. · 2014 · 257 · 7810.1016/j.surfcoat.2014.02.067 ↗
48. Phys. Rev. B · 1993 · 47 · 430710.1103/PhysRevB.47.4307 ↗
49. J. Appl. Phys. · 1993 · 73 · 819810.1063/1.353435 ↗
50. J. Alloys Compd. · 2010 · 502 · 48010.1016/j.jallcom.2010.04.202 ↗
51. Wear · 1998 · 218 · 8410.1016/S0043-1648(98)00181-1 ↗
52. J. Phys. Condens. Matter · 2010 · 22 · 29220310.1088/0953-8984/22/29/292203 ↗
53. Surf. Coat. Technol. · 1995 · 76–77 · 49910.1016/0257-8972(95)02566-9 ↗
54. Surf. Coat. Technol. · 2015 · 266 · 110.1016/j.surfcoat.2015.01.042 ↗