Abstract
The evolution of the surface roughness during the atomic-layer deposition (ALD) of Al2O3, NiO, and HfO2 was studied by atomic-force microscopy and nonspecular x-ray reflectance. The results indicate that the crystallinity of the films played a crucial role in the roughness evolution during ALD. While the ALD of amorphous oxide films showed replication of the initial starting surface with no roughness build-up, the ALD of polycrystalline oxide films led to a strong anomalous dependence of the roughness on the film thickness. This behavior is explained within a model taking into account spatial variations of the adsorption site density.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Electronic and Structural Properties of Oxides · ZnO doping and properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Imec , B-3001 Leuven, Belgium
References (47)
Show source-provided references
1. Chem. Rev. · 2010 · 110 · 11110.1021/cr900056b ↗
2. J. Appl. Phys. · 2005 · 97 · 12130110.1063/1.1940727 ↗
3. Science · 2000 · 288 · 31910.1126/science.288.5464.319 ↗
4. Nature Mater. · 2003 · 2 · 74910.1038/nmat1000 ↗
5. Nature Mater. · 2007 · 6 · 81010.1038/nmat2014 ↗
6. Nature Nanotechnol. · 2010 · 5 · 14810.1038/nnano.2009.456 ↗
7. Nature Mater. · 2002 · 1 · 24110.1038/nmat769 ↗
8. Sol. Energy Mater. Sol. Cells · 2006 · 90 · 343810.1016/j.solmat.2006.04.014 ↗
9. Appl. Phys. Lett. · 2007 · 91 · 11210710.1063/1.2784168 ↗
10. Nature Nanotechnol. · 2009 · 4 · 29210.1038/nnano.2009.37 ↗
11. Nature Mater. · 2011 · 10 · 45610.1038/nmat3017 ↗
12. Nature Mater. · 2011 · 10 · 53910.1038/nmat3047 ↗
13. Adv. Mater. · 2010 · 22 · 217210.1002/adma.200903951 ↗
14. Thin Solid Films · 2002 · 414 · 4310.1016/S0040-6090(02)00427-3 ↗
15. Thin Solid Films · 1993 · 228 · 3210.1016/0040-6090(93)90557-6 ↗
16. J. Phys. Chem. · 1996 · 100 · 1312110.1021/jp9536763 ↗
17. Appl. Phys. Lett. · 2003 · 82 · 475810.1063/1.1585129 ↗
18. J. Appl. Phys. · 2002 · 92 · 716810.1063/1.1522811 ↗
19. J. Appl. Phys. · 2004 · 96 · 768610.1063/1.1810193 ↗
20. J. Appl. Phys. · 2007 · 102 · 02490610.1063/1.2756514 ↗
21. 1995
22. 2008
23. Adv. Phys. · 1997 · 46 · 13910.1080/00018739700101498 ↗
24. Phys. Rev. Lett. · 1993 · 70 · 290010.1103/PhysRevLett.70.2900 ↗
25. Phys. Rev. Lett. · 1996 · 76 · 377410.1103/PhysRevLett.76.3774 ↗
26. Phys. Rev. B. · 2006 · 74 · 12542010.1103/PhysRevB.74.125420 ↗
27. Phys. Rev. Lett. · 2000 · 84 · 312510.1103/PhysRevLett.84.3125 ↗
28. Phys. Rev. B · 2007 · 76 · 07531410.1103/PhysRevB.76.075314 ↗
29. Chem. Vap. Depos. · 2004 · 10 · 15910.1002/cvde.v10:3 ↗
30. J. Mater. Sci. Technol. · 2010 · 26 · 37110.1016/S1005-0302(10)60061-8 ↗
31. Phys. Rev. Lett. · 1992 · 69 · 376210.1103/PhysRevLett.69.3762 ↗
32. Chem. Vap. Depos. · 2012 · 18 · 6110.1002/cvde.201106949 ↗
33. Phys. Rev. B · 1988 · 38 · 229710.1103/PhysRevB.38.2297 ↗
34. Centr. Eur. J. Phys. · 2012 · 10 · 18110.2478/s11534-011-0096-2 ↗
35. See supplementary material at http://dx.doi.org/10.1116/1.4812707 for AFM micrographs and NS-XRR pattern including best fits to the data.
36. Thin Solid Films · 1994 · 250 · 7210.1016/0040-6090(94)90168-6 ↗
37. Chem. Mater · 2002 · 14 · 227610.1021/cm011587z ↗
38. Appl. Phys. Lett · 2009 · 95 · 09191110.1063/1.3223616 ↗
39. Phys. Rev. B · 1994 · 49 · 1066810.1103/PhysRevB.49.10668 ↗
40. Daillant · 2010 · 235
41. Appl. Phys. Lett. · 2006 · 88 · 01311610.1063/1.2161117 ↗
42. Rev. Mod. Phys. · 1993 · 65 · 128110.1103/RevModPhys.65.1281 ↗
43. Phys. Rev. Lett. · 1991 · 66 · 210410.1103/PhysRevLett.66.2104 ↗
44. Solid State Phenom. · 2003 · 93 · 41110.4028/www.scientific.net/SSP.93.411 ↗
45. J. Cryst. Growth · 2006 · 289 · 38710.1016/j.jcrysgro.2005.11.089 ↗
46. Surf. Coat. Technol. · 2004 · 180–181 · 14010.1016/j.surfcoat.2003.10.054 ↗
47. Phys. Rev. Lett. · 1990 · 64 · 77210.1103/PhysRevLett.64.772 ↗