Nb-B-C thin films for electrical contact applications deposited by magnetron sputtering
Source abstract
Abstract
The high wear resistance, high chemical inertness, and high electrical conductivity of magnetron-sputtered transition metal diborides make them a candidate material for sliding electrical contacts. However, their high hardness makes it difficult to penetrate surface oxides, resulting in a high electrical contact resistance. In this study, the authors have investigated how the contact resistance can be improved by the formation of softer Nb-B-C films. The Nb-B-C films were deposited by magnetron sputtering and shown to exhibit a nanocomposite microstructure consisting of nanocrystalline NbB2−x grains with a solid solution of C separated by an amorphous BCx phase. The formation of the BCx phase reduces the hardness from 41 GPa for the NbB2−x film to 19 GPa at 36 at. % C. As a consequence the contact resistance is drastically reduced and the lowest contact resistance of 35 mΩ (contact force 5 N) is achieved for a film containing 30 at. % C. However, crack formation and subsequent delamination and fragmentation is observed for the C-containing Nb-B-C films in tribology tests resulting in high friction values for these films.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
The Ångström Laboratory, Uppsala University Department of Chemistry, , SE-751 21 Uppsala, Sweden
Linköping University Thin Film Physics Division, Department of Physics, Chemistry, and Biology (IFM), , SE-581 83 Linköping, Sweden
References (26)
Show source-provided references
1. Surf. Coat. Technol. · 1998 · 98 · 148310.1016/S0257-8972(97)00397-6 ↗
2. Appl. Phys. Lett. · 2005 · 86 · 13190910.1063/1.1887824 ↗
3. J. Phys. D: Appl. Phys. · 2011 · 44 · 38540210.1088/0022-3727/44/38/385402 ↗
4. Thin Solid Films · 2001 · 401 · 17910.1016/S0040-6090(01)01481-X ↗
5. Surf. Coat. Technol. · 2000 · 124 · 25310.1016/S0257-8972(99)00638-6 ↗
6. Surf. Coat. Technol. · 2005 · 200 · 141810.1016/j.surfcoat.2005.08.078 ↗
7. N. Nedfors, O. Tengstrand, J. Lu, P. O. A. Persson, P. Eklund, L. Hultman, and U. Jansson, “Synthesis and characterization of multifunctional carbide- and boride-based thin films,” Ph.D. dissertation (Acta Universitatis Upsaliensis, 2014).
8. J. Appl. Phys. · 2006 · 100 · 05430310.1063/1.2336302 ↗
9. Surf. Coat. Technol. · 2011 · 206 · 35410.1016/j.surfcoat.2011.07.021 ↗
10. Z. Metallk. · 1963 · 54 · 345
11. J. Mater. Res. · 1992 · 7 · 156410.1557/JMR.1992.1564 ↗
12. Thin Solid Films · 2009 · 517 · 185810.1016/j.tsf.2008.07.014 ↗
13. Acta Mater. · 2005 · 53 · 367910.1016/j.actamat.2005.04.020 ↗
14. Inorg. Mater. · 1984 · 20 · 1580
15. Thin Solid Films · 2010 · 518 · 260710.1016/j.tsf.2009.07.195 ↗
16. Surf. Coat. Technol. · 1990 · 43–44 · 10710.1016/0257-8972(90)90065-K ↗
17. Surf. Coat. Technol. · 2007 · 201 · 610510.1016/j.surfcoat.2006.08.118 ↗
18. Phys. Rev. B · 2005 · 71 · 16540510.1103/PhysRevB.71.165405 ↗
19. Appl. Surf. Sci. · 2012 · 258 · 990710.1016/j.apsusc.2012.06.049 ↗
20. Surf. Sci. · 2004 · 572 · 41810.1016/j.susc.2004.09.020 ↗
21. Surf. Coat. Technol. · 1998 · 105 · 4510.1016/S0257-8972(98)00445-9 ↗
22. Thin Solid Films · 2010 · 518 · 554610.1016/j.tsf.2010.04.038 ↗
23. Nature · 1998 · 391 · 56110.1038/35328 ↗
24. Science · 2004 · 305 · 65410.1126/science.1098741 ↗
25. N. Nedfors, O. Tengstrand, A. Flink, A. M. Andersson, P. Eklund, L. Hultman, and U. Jansson, “Synthesis and characterization of multifunctional carbide- and boride-based thin films,” Ph.D. dissertation (Acta Universitatis Upsaliensis, 2014).