Vanadium dioxide film protected with an atomic-layer-deposited Al2O3 thin film
Source abstract
Abstract
A VO2 film exposed to ambient air is prone to oxidation, which will degrade its thermochromic properties. In this work, the authors deposited an ultrathin Al2O3 film with atomic layer deposition (ALD) to protect the underlying VO2 film from degradation, and then studied the morphology and crystalline structure of the films. To assess the protectiveness of the Al2O3 capping layer, the authors performed a heating test and a damp heating test. An ultrathin 5-nm-thick ALD Al2O3 film was sufficient to protect the underlying VO2 film heated at 350 °C. However, in a humid environment at prolonged durations, a thicker ALD Al2O3 film (15 nm) was required to protect the VO2. The authors also deposited and studied a TiO2/Al2O3 bilayer, which significantly improved the protectiveness of the Al2O3 film in a humid environment.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Transition Metal Oxide Nanomaterials · Semiconductor materials and devices · Ga2O3 and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Chinese Academy of Sciences Key Laboratory of Inorganic Coating Materials, Shanghai Institute of Ceramics, , 588 Heshuo Road, Shanghai 201800, China
References (28)
Show source-provided references
1. J. Vac. Sci. Technol. A · 2011 · 29 · 06150410.1116/1.3636372 ↗
2. J. Appl. Phys. · 2007 · 102 · 11371510.1063/1.2817818 ↗
3. Surf. Coat. Technol. · 2012 · 206 · 292210.1016/j.surfcoat.2011.12.022 ↗
4. J. Mater. Sci. · 2004 · 39 · 48910.1023/B:JMSC.0000011503.22893.f4 ↗
5. J. Phys. Chem. Solids · 2002 · 63 · 96510.1016/S0022-3697(02)00098-7 ↗
6. J. Mater. Sci.-Mater. Electron. · 1998 · 9 · 18710.1023/A:1008822023407 ↗
7. Langmuir · 2010 · 26 · 1073810.1021/la100515k ↗
8. Opt. Eng. · 1993 · 32 · 209210.1117/12.143951 ↗
9. Sol. Energy Mater. Sol. Cells · 2013 · 117 · 49410.1016/j.solmat.2013.07.023 ↗
10. Energy Environ. Sci. · 2012 · 5 · 610410.1039/c2ee02803d ↗
11. Thin Solid Films · 2004 · 449 · 16610.1016/j.tsf.2003.10.013 ↗
12. Thin Solid Films · 2014 · 562 · 56810.1016/j.tsf.2014.03.043 ↗
13. Opt. Mater. · 2007 · 30 · 40710.1016/j.optmat.2006.11.067 ↗
14. J. Phys. Chem. C · 2013 · 117 · 2030810.1021/jp406738h ↗
15. Thin Solid Films · 2002 · 413 · 18610.1016/S0040-6090(02)00438-8 ↗
16. Surf. Coat. Technol. · 1996 · 78 · 110.1016/0257-8972(95)02420-4 ↗
17. Chem. Rev. · 2010 · 110 · 11110.1021/cr900056b ↗
18. Thin Solid Films · 2008 · 516 · 403610.1016/j.tsf.2007.07.150 ↗
19. J. Appl. Phys. · 2009 · 106 · 02353310.1063/1.3159639 ↗
20. J. Coat. Technol. Res. · 2011 · 8 · 65510.1007/s11998-011-9327-0 ↗
21. Thin Solid Films. · 2012 · 522 · 28310.1016/j.tsf.2012.08.023 ↗
22. ACS Appl. Mater. Interfaces · 2011 · 3 · 459310.1021/am2009579 ↗
23. Sputtering deposition of VO2 film using plasma emission monitor as reactive gas flow rate feedback control
24. Surf. Sci. · 1995 · 322 · 23010.1016/0039-6028(95)90033-0 ↗
25. Thin Solid Films · 1997 · 292 · 13510.1016/S0040-6090(96)08934-1 ↗
26. Appl. Surf. Sci. · 2004 · 226 · 39310.1016/j.apsusc.2003.10.053 ↗
27. J. Phys. Chem. C · 2008 · 112 · 457310.1021/jp076866+ ↗
28. J. Vac. Sci. Technol. A · 2012 · 30 · 04151510.1116/1.4729447 ↗