Effect of methane addition on ultrananocrystalline diamond formation: Morphology changes and induced stress
Source abstract
Abstract
The morphology and structure of ultrananocrystalline diamond grown on Si substrate by chemical vapor deposition are systematically studied by varying the methane concentration in the Ar/H2/CH4 precursor mixture. The films, analyzed by field-emission-gun scanning electron microscopy (FEG-SEM), showed a nanocrystallite cluster morphology that decreased its grain size (L) as a function of the CH4 addition in the gas phase. From Raman spectra, the induced stress of nanodiamond films was analyzed by the G peak shift associated with the defect incorporation and sp2 bond enhancement. The compressive stress increased as a function of CH4 addition, which also promoted the broadening of the transpolyacetylene peak as indicative of film amorphitization. The nanodiamond crystallinity was confirmed from high-resolution x-ray diffractograms, where Scherrer’s equation was applied to (111) and (200) x-ray peaks resulting in grain- size values ranging from 8.5 to 4.0 nm as the methane concentration increased, also corroborated by FEG-SEM images.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics · High-pressure geophysics and materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Instituto Nacional de Pesquisas Espaciais Laboratório Associado de Sensores e Materiais, , Av. dos Astronautas 1758, Jd. Granja, S.J. Campos, Sao Paulo 12245-970, Brazil
References (28)
Show source-provided references
1. Annu. Rev. Mater. Sci. · 1999 · 29 · 21110.1146/annurev.matsci.29.1.211 ↗
2. Phys. Rev. B · 1997 · 56 · 597810.1103/PhysRevB.56.5978 ↗
3. Electroanalysis · 2000 · 12 · 710.1002/(SICI)1521-4109(20000101)12:1<7::AID-ELAN7>3.0.CO;2-# ↗
4. Semicond. Sci. Technol. · 2007 · 22 · 12810.1088/0268-1242/22/2/022 ↗
5. Diamond Relat. Mater. · 2008 · 17 · 45110.1016/j.diamond.2007.10.004 ↗
6. J. Appl. Phys. · 2001 · 89 · 576910.1063/1.1367313 ↗
7. Phys. Rev. B · 1995 · 51 · 1230310.1103/PhysRevB.51.12303 ↗
8. Surf. Coat. Technol. · 2007 · 202 · 111310.1016/j.surfcoat.2007.07.050 ↗
9. Diamond Relat. Mater. · 2009 · 18 · 74510.1016/j.diamond.2009.01.005 ↗
10. Diamond Relat. Mater. · 2005 · 14 · 189710.1016/j.diamond.2005.09.010 ↗
11. Surf. Coat. Technol. · 2002 · 151–152 · 26310.1016/S0257-8972(01)01566-3 ↗
12. Mater. Chem. Phys. · 2006 · 96 · 25310.1016/j.matchemphys.2005.07.048 ↗
13. Appl. Phys. Lett. · 1995 · 67 · 69410.1063/1.115206 ↗
14. Surf. Coat. Technol. · 2008 · 202 · 226310.1016/j.surfcoat.2007.08.050 ↗
15. J. Phys.: Condens. Matter · 2007 · 19 · 38621510.1088/0953-8984/19/38/386215 ↗
16. Revista Brasileirade Aplicações de Vácuo · 2006 · 25 · 161
17. J. Appl. Phys. · 2007 · 101 · 110.1063/1.2696363 ↗
18. J. Appl. Phys. · 2006 · 100 · 02430110.1063/1.2214304 ↗
19. Diamond Relat. Mater. · 1995 · 4 · 46410.1016/0925-9635(94)05260-3 ↗
20. Int. J. Refract. Met. Hard Mater. · 2002 · 20 · 9310.1016/S0263-4368(02)00006-9 ↗
21. Phys. Solid State · 2004 · 46 · 72010.1134/1.1711458 ↗
22. Diamond Relat. Mater. · 2005 · 14 · 39810.1016/j.diamond.2004.11.019 ↗
23. Diamond Relat. Mater · 2007 · 16 · 73010.1016/j.diamond.2007.01.033 ↗
24. Phys. Rev. B · 2001 · 63 · 12140510.1103/PhysRevB.63.121405 ↗
25. Appl. Phys. Lett. · 2001 · 78 · 63110.1063/1.1343840 ↗
26. Diamond Relat. Mater. · 2008 · 17 · 10510.1016/j.diamond.2007.11.005 ↗
27. Chem. Phys. Lett. · 2007 · 446 · 10310.1016/j.cplett.2007.08.018 ↗
28. Diamond Relat. Mater. · 2002 · 11 · 60110.1016/S0925-9635(01)00631-8 ↗