Atomic layer deposition of aluminum sulfide thin films using trimethylaluminum and hydrogen sulfide
Source abstract
Abstract
Sequential exposures of trimethylaluminum and hydrogen sulfide are used to deposit aluminum sulfide thin films by atomic layer deposition (ALD) in the temperature ranging from 100 to 200 °C. Growth rate of 1.3 Å per ALD cycle is achieved by in-situ quartz crystal microbalance measurements. It is found that the growth rate per ALD cycle is highly dependent on the purging time between the two precursors. Increased purge time results in higher growth rate. Surface limited chemistry during each ALD half cycle is studied by in-situ Fourier transformed infrared vibration spectroscopy. Time of flight secondary ion-mass spectroscopy measurement is used to confirm elemental composition of the deposited films.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Electronic and Structural Properties of Oxides · ZnO doping and properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Indian Institute of Technology Bombay Department of Energy Science and Engineering, , Powai, Mumbai 400076, India
Indian Institute of Technology Bombay Centre for Research in Nanotechnology and Science, , Powai, Mumbai 400076, India
References (23)
Show source-provided references
1. J. Appl. Phys. · 2004 · 95 · 18410.1063/1.1630372 ↗
2. J. Phys. D: Appl. Phys. · 2008 · 41 · 18530410.1088/0022-3727/41/18/185304 ↗
3. Solid State Sci. · 2009 · 11 · 22410.1016/j.solidstatesciences.2008.04.020 ↗
4. J. Cryst. Growth · 1986 · 77 · 48510.1016/0022-0248(86)90341-6 ↗
5. J. Cryst. Growth · 1988 · 86 · 25210.1016/0022-0248(90)90725-Z ↗
6. J. Am. Chem. Soc. · 1997 · 119 · 956610.1021/ja972111c ↗
7. J. Appl. Phys. · 2005 · 98 · 04351210.1063/1.2012515 ↗
8. J. Electron. Spectrosc. Relat. Phenom. · 2005 · 148 · 9110.1016/j.elspec.2005.04.001 ↗
9. W. Rachmady, M. Radosavljevic, G. Dewey, and R. S. Chau, U.S. patent 8,344,418 B2 (1 January 2013).
10. Appl. Surf. Sci. · 2004 · 229 · 10510.1016/j.apsusc.2004.01.050 ↗
11. Z. Phys. · 1959 · 155 · 20610.1007/BF01337937 ↗
12. Thin Solid Films · 2009 · 517 · 565810.1016/j.tsf.2009.02.050 ↗
13. Chem. Mater. · 2004 · 16 · 63910.1021/cm0304546 ↗
14. Rev. Sci. Instrum. · 2002 · 73 · 298110.1063/1.1490410 ↗
15. Chem. Mater. · 2002 · 14 · 435010.1021/cm020357x ↗
16. Thin Solid Films · 2012 · 520 · 275010.1016/j.tsf.2011.11.081 ↗
17. Chem. Rev. · 2010 · 110 · 11110.1021/cr900056b ↗
18. J. Phys. Chem. C · 2011 · 115 · 1538410.1021/jp2024389 ↗
19. Thin Solid Films · 1997 · 292 · 13510.1016/S0040-6090(96)08934-1 ↗
20. Surf. Sci. · 1995 · 322 · 23010.1016/0039-6028(95)90033-0 ↗
21. J. Vac. Sci. Technol., A · 2005 · 23 · 11810.1116/1.1821585 ↗
22. J. Phys. Chem. C · 2008 · 112 · 1953010.1021/jp804296a ↗
23. J. Phys. Chem. C · 2010 · 114 · 803210.1021/jp9086943 ↗